Volumn 256, Issue 5, 2004, Pages 469-479

The corrosion-wear behaviour of thermally oxidised CP-Ti and Ti-6Al-4V

Author keywords

Bio implants; Corrosion wear; Thermal oxidation; Titanium; Wear

Indexed keywords

ABRASION; CORROSION; DEGRADATION; DIFFUSION; HARDNESS; OXIDATION; SHEAR STRENGTH; SURFACE CHEMISTRY; TITANIUM DIOXIDE;

EID: 1642332462     PISSN: 00431648     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0043-1648(03)00557-X     Document Type: Article
Times cited : (176)

References (11)
  • 1
    • 0032605637 scopus 로고    scopus 로고
    • A review of metallic ceramic and surface treated metals used for bearing surfaces in human joint replacements
    • Dearnley P.A.A review of metallic ceramic and surface treated metals used for bearing surfaces in human joint replacements Proc. Inst. Mech. Eng., Part H 213 1999 107-135
    • (1999) Proc. Inst. Mech. Eng. , vol.213 , Issue.PART H , pp. 107-135
    • Dearnley, P.A.1
  • 3
    • 0031444302 scopus 로고    scopus 로고
    • Wear analysis of a retrieved hip implant with a titanium nitride coating
    • Harman M.K.Banks S.A.Hodge W.A.Wear analysis of a retrieved hip implant with a titanium nitride coating J. Arthroplasty 128 1997 838-945
    • (1997) J. Arthroplasty , vol.128 , pp. 838-945
    • Harman, M.K.1    Banks, S.A.2    Hodge, W.A.3
  • 4
    • 0006537783 scopus 로고    scopus 로고
    • Fifteen years experience with Ti-6Al-7Nb alloy for joint replacements
    • P.A. Blenkinsop, W.J. Evans (Eds.), The Institute of Materials, London
    • M. Semlitsch, H. Weber, R. Steger, Fifteen years experience with Ti-6Al-7Nb alloy for joint replacements, in: P.A. Blenkinsop, W.J. Evans (Eds.), Proceedings of the Titanium'95 Conference on Science and Technology, vol. II, The Institute of Materials, London, 1996, pp. 1742-1759.
    • (1996) Proceedings of the Titanium'95 Conference on Science and Technology , vol.2 , pp. 1742-1759
    • Semlitsch, M.1    Weber, H.2    Steger, R.3
  • 5
    • 0033626715 scopus 로고    scopus 로고
    • Enhanced wear resistance of titanium surfaces by a new thermal oxidation treatment
    • Dong H.Bell T.Enhanced wear resistance of titanium surfaces by a new thermal oxidation treatment Wear 238 2000 131-137
    • (2000) Wear , vol.238 , pp. 131-137
    • Dong, H.1    Bell, T.2
  • 6
    • 0034001282 scopus 로고    scopus 로고
    • Oxygen boost diffusion for the deep-case hardening of titanium alloys
    • Dong H.Li X.Oxygen boost diffusion for the deep-case hardening of titanium alloys Mater. Sci. Eng. A 280 2 2000 303-310
    • (2000) Mater. Sci. Eng. A , vol.280 , Issue.2 , pp. 303-310
    • Dong, H.1    Li, X.2
  • 7
    • 0035482879 scopus 로고    scopus 로고
    • Corrosion response of surface engineered titanium alloys damaged by prior abrasion
    • Komotori J.Lee B.J.Dong H.Dearnley P.A.Corrosion response of surface engineered titanium alloys damaged by prior abrasion Wear 251 2001 1239-1249
    • (2001) Wear , vol.251 , pp. 1239-1249
    • Komotori, J.1    Lee, B.J.2    Dong, H.3    Dearnley, P.A.4
  • 8
    • 0034960852 scopus 로고    scopus 로고
    • The electrochemical oxide growth behaviour on titanium in acid and alkaline electrolytes
    • Sul Y.-T.Johansson C.B.Jeong Y.Albrektsson T.The electrochemical oxide growth behaviour on titanium in acid and alkaline electrolytes Med. Eng. Phys. 23 2001 329-346
    • (2001) Med. Eng. Phys. , vol.23 , pp. 329-346
    • Sul, Y.-T.1    Johansson, C.B.2    Jeong, Y.3    Albrektsson, T.4
  • 10
    • 1542377292 scopus 로고    scopus 로고
    • Corrosion-wear mechanisms of hard coated austenitic 316L stainless steels
    • P.A. Dearnley, G. Aldrich-Smith, Corrosion-wear mechanisms of hard coated austenitic 316L stainless steels, Wear 256 (5) (2004) 491-499.
    • (2004) Wear , vol.256 , Issue.5 , pp. 491-499
    • Dearnley, P.A.1    Aldrich-Smith, G.2
  • 11
    • 0000833831 scopus 로고
    • Generation and relief of stress in ceramic films
    • Institute of Materials, London
    • A. Atkinson, Generation and relief of stress in ceramic films, in: Ceramic Films and Coatings, Institute of Materials, London, 1995, pp. 317-331.
    • (1995) Ceramic Films and Coatings , pp. 317-331
    • Atkinson, A.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.