Friction and wear of titanium alloys sliding against metal, polymer, and ceramic counterfaces

Author keywords

Ceramics; Material transfer; Titanium; Tribochemical reaction

Indexed keywords

ALUMINA; BRAKES; CERAMIC MATERIALS; ENERGY DISPERSIVE SPECTROSCOPY; ENGINES; FRACTURE TOUGHNESS; FRICTION; POLYMERS; POLYTETRAFLUOROETHYLENES; SILICON NITRIDE; STAINLESS STEEL; TITANIUM; TRIBOLOGY; WEAR OF MATERIALS; X RAY DIFFRACTION ANALYSIS;

EID: 13844274898     PISSN: 00431648     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.wear.2004.09.062     Document Type: Article
Times cited : (256)

References (15)
  • 2
    • 0021851059 scopus 로고
    • The effect of ion implantation on the fretting wear of four titanium alloys at temperatures up to 600°C
    • ASME, New York
    • R.B. Waterhouse, A. Iwabuchi, The effect of ion implantation on the fretting wear of four titanium alloys at temperatures up to 600°C, in: Proceedings of the International Conference on Wear of Materials, ASME, New York, 1985, pp. 471-484.
    • (1985) Proceedings of the International Conference on Wear of Materials , pp. 471-484
    • Waterhouse, R.B.1    Iwabuchi, A.2
  • 3
    • 0026360706 scopus 로고
    • Tribological properties of titanium alloys
    • K.G. Budinski, Tribological properties of titanium alloys, Wear 151 (1991) 203-217.
    • (1991) Wear , vol.151 , pp. 203-217
    • Budinski, K.G.1
  • 4
    • 0031194193 scopus 로고    scopus 로고
    • Dry sliding wear mechanisms of the Ti6Al4V alloy
    • A. Molinari, T.B. Straffelini, T. Bacci, Dry sliding wear mechanisms of the Ti6Al4V alloy, Wear 208 (1997) 105-112.
    • (1997) Wear , vol.208 , pp. 105-112
    • Molinari, A.1    Straffelini, T.B.2    Bacci, T.3
  • 5
    • 0033492058 scopus 로고    scopus 로고
    • Tribological behavior of alumina sliding against Ti6Al4V in unlubricated contact
    • H. Dong, T. Bell, Tribological behavior of alumina sliding against Ti6Al4V in unlubricated contact, Wear 225-229 (1999) 874-884.
    • (1999) Wear , vol.225-229 , pp. 874-884
    • Dong, H.1    Bell, T.2
  • 6
    • 13844257832 scopus 로고    scopus 로고
    • Opportunities for low cost titanium in reduced fuel consumption, improved emissions, and enhanced durability heavy-duty vehicles
    • Oak Ridge, Tennessee
    • EHKT Technologies, Opportunities for low cost titanium in reduced fuel consumption, improved emissions, and enhanced durability heavy-duty vehicles, Oak Ridge National Laboratory Report, ORNL/Sub/4000013062/1, Oak Ridge, Tennessee, 2002, p. 59.
    • (2002) Oak Ridge National Laboratory Report , vol.ORNL-SUB-4000013062-1 , pp. 59
  • 7
    • 13844303955 scopus 로고    scopus 로고
    • Literature, Red Devil Brakes, Inc., Mt. Pleasant, Pennsylvania, not dated
    • Ultra-Lite Brakes and Components, Literature, Red Devil Brakes, Inc., Mt. Pleasant, Pennsylvania, not dated.
    • Ultra-lite Brakes and Components
  • 8
    • 13844303954 scopus 로고    scopus 로고
    • Fatigue and fracture properties of stainless steel
    • S.R. Lampman (Ed.), ASM International
    • S. Lampman, Fatigue and fracture properties of stainless steel, in: S.R. Lampman (Ed.), ASM Handbook, Fatigue and Fracture, 19, ASM International, 1996, pp. 712-732.
    • (1996) ASM Handbook, Fatigue and Fracture , vol.19 , pp. 712-732
    • Lampman, S.1
  • 9
    • 0014746014 scopus 로고
    • IC and Charpy V-notch test results in the transition temperature range
    • ASTM, Philadelphia
    • IC and Charpy V-notch test results in the transition temperature range, in: Impact Testing of Materials STP 466, ASTM, Philadelphia, 1979, pp. 281-302.
    • (1979) Impact Testing of Materials STP , vol.466 , pp. 281-302
    • Barsom, J.M.1    Rolfe, S.T.2
  • 11
    • 0025431574 scopus 로고
    • Friction and wear of ceramics
    • T.E. Fischer, Friction and wear of ceramics, Scripta Metall. Mater. 24 (1990) 833-838.
    • (1990) Scripta Metall. Mater. , vol.24 , pp. 833-838
    • Fischer, T.E.1
  • 12
    • 0018694220 scopus 로고
    • The role of microstructure in the impact wear of two aluminum alloys
    • S.L. Rice, The role of microstructure in the impact wear of two aluminum alloys, ASME Proc. Wear Mater. (1979) 27-34.
    • (1979) ASME Proc. Wear Mater. , pp. 27-34
    • Rice, S.L.1
  • 13
    • 0019481909 scopus 로고
    • Characteristics of metallic subsurface zones in sliding and impact wear
    • S.L. Rice, H. Nowotny, S.F. Wayne, Characteristics of metallic subsurface zones in sliding and impact wear, ASME Proc. Wear Mater. (1981) 47-52.
    • (1981) ASME Proc. Wear Mater. , pp. 47-52
    • Rice, S.L.1    Nowotny, H.2    Wayne, S.F.3
  • 14
    • 85040803656 scopus 로고
    • Carl Hanser Verlag Munchen Wien, Berlin
    • G. Heinicke, Tribochemistry, Carl Hanser Verlag Munchen Wien, Berlin, 1984.
    • (1984) Tribochemistry
    • Heinicke, G.1
  • 15
    • 0002135518 scopus 로고
    • X-ray diffraction system PTS for powder, texture and stress analysis
    • H.J. Bunge (Ed.), DGM Informationsgesellschaft, Verlag
    • H. Krause, A. Haase, X-Ray Diffraction System PTS for Powder, Texture and Stress Analysis, in: H.J. Bunge (Ed.), Experimental Techniques of Texture Analysis, vol. 405-408, DGM Informationsgesellschaft, Verlag, 1986.
    • (1986) Experimental Techniques of Texture Analysis , vol.405-408
    • Krause, H.1    Haase, A.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.