메뉴 건너뛰기




Volumn 24, Issue 8, 2004, Pages 2329-2338

Crack-healing and oxidation behavior of silicon nitride ceramics

Author keywords

Crack healing; Oxidation behavior; Si3N4; Strength

Indexed keywords

ACTIVATION ENERGY; BENDING (DEFORMATION); CERAMIC MATERIALS; CRACKS; OXIDATION;

EID: 1342310167     PISSN: 09552219     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0955-2219(03)00645-9     Document Type: Article
Times cited : (111)

References (27)
  • 1
    • 0026840695 scopus 로고
    • Crack-healing behavior of hot-pressed silicon nitride due to oxidation
    • Choi S.R. Tikara V. Crack-healing behavior of hot-pressed silicon nitride due to oxidation Scripta. Metall. Mater. 26 1992 1263-1268
    • (1992) Scripta. Metall. Mater. , vol.26 , pp. 1263-1268
    • Choi, S.R.1    Tikara, V.2
  • 2
    • 0028396285 scopus 로고
    • Thereshold stress intensity for oxidative crack healing in sintered silicon nitride
    • Ogasawara T. Hori T. Okada A. Thereshold stress intensity for oxidative crack healing in sintered silicon nitride J. Mat. Sci. Lett. 13 1994 404-406
    • (1994) J. Mat. Sci. Lett. , vol.13 , pp. 404-406
    • Ogasawara, T.1    Hori, T.2    Okada, A.3
  • 5
    • 0003157862 scopus 로고    scopus 로고
    • 4 ceramics and it's application to structural integrity
    • ECF-12 ed. M.W. Brown, E.R. de los Rios and K.J. Miller. Engineering Materials Advisory Services
    • 4 ceramics and it's application to structural integrity. In Fracture From Defects, ECF-12 ed. M.W. Brown, E.R. de los Rios and K.J. Miller. Engineering Materials Advisory Services, 1998, pp. 497-502.
    • (1998) Fracture From Defects , pp. 497-502
    • Ando, K.1    Sato, S.2    Kobayashi, Y.3    Chu, M.C.4
  • 6
    • 84875873679 scopus 로고    scopus 로고
    • The study on crack healing behaviour of silicon nitride ceramics
    • Ando K. Chu M.C. Sato S. Yao F. Kobayashi Y. The study on crack healing behaviour of silicon nitride ceramics Jpn. Soc. Mech. Eng. 64-623 1998 1936-1942
    • (1998) Jpn. Soc. Mech. Eng. , vol.64 , Issue.623 , pp. 1936-1942
    • Ando, K.1    Chu, M.C.2    Sato, S.3    Yao, F.4    Kobayashi, Y.5
  • 7
    • 0002251556 scopus 로고    scopus 로고
    • Crack Healing behaviour of silicon nitride ceramics (effect of sintering additives and sintering powder.)
    • Chu M.C. Ando K. Hirasawa T. Sato S. Kobayashi Y. Crack Healing behaviour of silicon nitride ceramics (effect of sintering additives and sintering powder.) High Pressure Institute of Japan 36-2 1998 82-89
    • (1998) High Pressure Institute of Japan , vol.36-42 , pp. 82-89
    • Chu, M.C.1    Ando, K.2    Hirasawa, T.3    Sato, S.4    Kobayashi, Y.5
  • 9
    • 0001195536 scopus 로고    scopus 로고
    • Crack healing behavior and high temperature strength of silicon nitride ceramics
    • Ando K. Chu M.C. Kobayashi Y. Yao F. Sato S. Crack healing behavior and high temperature strength of silicon nitride ceramics Jpn. Soc. Mech. Eng. 65-633 A 1999 1132-1139
    • (1999) Jpn. Soc. Mech. Eng. , vol.65 , Issue.633 A , pp. 1132-1139
    • Ando, K.1    Chu, M.C.2    Kobayashi, Y.3    Yao, F.4    Sato, S.5
  • 11
    • 0036629631 scopus 로고    scopus 로고
    • Self crack-healing behavior under stress of silicon nitride ceramics and resultant strength at the crack-healed temperature
    • Takahashi K. Kim B.S. Chu M.C. Saito S. Ando K. Self crack-healing behavior under stress of silicon nitride ceramics and resultant strength at the crack-healed temperature Jpn. Soc. Mech. Eng. 68-761 A 2002 1063-1070
    • (2002) Jpn. Soc. Mech. Eng. , vol.68 , Issue.761 A , pp. 1063-1070
    • Takahashi, K.1    Kim, B.S.2    Chu, M.C.3    Saito, S.4    Ando, K.5
  • 12
    • 0033688614 scopus 로고    scopus 로고
    • Crack-healing behavior, high-temperature and fatigue strength of SiC-reinforced silicon nitride composite
    • Yao F. Ando K. Chu M.C. Sato S. Crack-healing behavior, high-temperature and fatigue strength of SiC-reinforced silicon nitride composite J. Mat. Sci. Lett. 12 19 2000 1081-1084
    • (2000) J. Mat. Sci. Lett. , vol.12 , Issue.19 , pp. 1081-1084
    • Yao, F.1    Ando, K.2    Chu, M.C.3    Sato, S.4
  • 13
    • 1342300911 scopus 로고    scopus 로고
    • Improvement of the strength of silicon nitride by aging
    • ed. Bradt R.C. et al. Kluwer Academic/Plenum Publishers
    • Lube, T., Improvement of the strength of silicon nitride by aging. In Fracture Mechanics of Ceramics, ed. Bradt R.C. et al. Kluwer Academic/Plenum Publishers. Vol. 13, 2002, pp. 151-157.
    • (2002) Fracture Mechanics of Ceramics , vol.13 , pp. 151-157
    • Lube, T.1
  • 14
    • 0036132177 scopus 로고    scopus 로고
    • (Crack-healing+Proof test): A new methodology to guarantee the structural integrity of a ceramics component
    • Ando K. Shirai Y. Nakatani M. Kobayashi Y. Sato S. (Crack-healing+Proof test): a new methodology to guarantee the structural integrity of a ceramics component J. Eur. Ceram. Soc. 22 2002 121-128
    • (2002) J. Eur. Ceram. Soc. , vol.22 , pp. 121-128
    • Ando, K.1    Shirai, Y.2    Nakatani, M.3    Kobayashi, Y.4    Sato, S.5
  • 15
    • 0035470705 scopus 로고    scopus 로고
    • Crack-healing behavior under stress of mullite/SiC ceramics and resultant fatigue strength
    • Ando K. Furusawa K. Chu M.C. Hanagata T. Tsuji K. Sato S. Crack-healing behavior under stress of mullite/SiC ceramics and resultant fatigue strength J. Am. Ceram.Soc. 84 9 2001 2073-2078
    • (2001) J. Am. Ceram.Soc. , vol.84 , Issue.9 , pp. 2073-2078
    • Ando, K.1    Furusawa, K.2    Chu, M.C.3    Hanagata, T.4    Tsuji, K.5    Sato, S.6
  • 18
    • 0036740298 scopus 로고    scopus 로고
    • 4/SiC ceramics under cyclic stress and resultant fatigue strength at the healing temperature
    • 4/SiC ceramics under cyclic stress and resultant fatigue strength at the healing temperature J. Am. Ceram. Soc. 85 9 2002 2268-2272
    • (2002) J. Am. Ceram. Soc. , vol.85 , Issue.9 , pp. 2268-2272
    • Ando, K.1    Takahashi, K.2    Nakayama, S.3    Saito, S.4
  • 21
    • 0018503878 scopus 로고
    • Residual stress effects in sharp contact cracking
    • Marshall D.B. Lawn B.R. Residual stress effects in sharp contact cracking J. Material Science 14 1979 2001-2012
    • (1979) J. Material Science , vol.14 , pp. 2001-2012
    • Marshall, D.B.1    Lawn, B.R.2
  • 23
    • 0041888384 scopus 로고    scopus 로고
    • Crack-healing behavior of alumina and strength of crack-healed member
    • Kim B.S. Ando K. Chu M.C. Saito S. Crack-healing behavior of alumina and strength of crack-healed member Jpn. Soc. Mater. Sci. 52-6 2003 667-673
    • (2003) Jpn. Soc. Mater. Sci. , vol.52-56 , pp. 667-673
    • Kim, B.S.1    Ando, K.2    Chu, M.C.3    Saito, S.4
  • 24
    • 85030881940 scopus 로고    scopus 로고
    • In situ crack-healing behavior of mullite/SiC composite ceramics
    • accepted for publication (in Japanese)
    • Furusawa, K., Furumachi, N., Takahashi, K., Saito, S., and Ando, K., In situ crack-healing behavior of mullite/SiC composite ceramics. Jpn. Soc. Mater. Sci., accepted for publication (in Japanese).
    • Jpn. Soc. Mater. Sci.
    • Furusawa, K.1    Furumachi, N.2    Takahashi, K.3    Saito, S.4    Ando, K.5
  • 25
    • 0036680737 scopus 로고    scopus 로고
    • Crack healing behavior and high temperature strength of mullite/SiC composite ceramics
    • Ando K. Chu M.C. Tuji K. Hirasawa T. Kobayashi Y. Sato S. Crack healing behavior and high temperature strength of mullite/SiC composite ceramics J. Eur. Ceram. Soc. 22 2002 1313-1319
    • (2002) J. Eur. Ceram. Soc. , vol.22 , pp. 1313-1319
    • Ando, K.1    Chu, M.C.2    Tuji, K.3    Hirasawa, T.4    Kobayashi, Y.5    Sato, S.6
  • 26
    • 0036692888 scopus 로고    scopus 로고
    • Crack-healing behavior of structural ceramics under constant and cyclic stress at elevated temperature
    • Ando K. Furusawa K. Takahashi K. Chu M.C. Sato S. Crack-healing behavior of structural ceramics under constant and cyclic stress at elevated temperature J. Ceram. Soc. Jpn. 110 8 2002 741-747
    • (2002) J. Ceram. Soc. Jpn. , vol.110 , Issue.8 , pp. 741-747
    • Ando, K.1    Furusawa, K.2    Takahashi, K.3    Chu, M.C.4    Sato, S.5
  • 27
    • 1342322086 scopus 로고    scopus 로고
    • Effect of small amount of iron impurity on oxidation of powder SiC
    • Nanri H. Nagasoe A. Effect of small amount of iron impurity on oxidation of powder SiC Taikabustu 51 1999 650-655
    • (1999) Taikabustu , vol.51 , pp. 650-655
    • Nanri, H.1    Nagasoe, A.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.