메뉴 건너뛰기




Volumn 13, Issue 1, 2004, Pages 99-102

Effect of Be on Aging Behavior of an Al-Si-Cu-Mg Cast Alloy

Author keywords

Aging behavior; Aluminum alloy; Effect of Be; Nucleation density; Precipitates

Indexed keywords

AGE HARDENING; BERYLLIUM; BINDING ENERGY; CASTING; DIFFERENTIAL SCANNING CALORIMETRY; DISSOLUTION; MICROHARDNESS; NUCLEATION; PRECIPITATION (CHEMICAL); TRANSMISSION ELECTRON MICROSCOPY;

EID: 1342308848     PISSN: 10599495     EISSN: None     Source Type: Journal    
DOI: 10.1361/10599490417605     Document Type: Article
Times cited : (9)

References (17)
  • 1
    • 0001306248 scopus 로고
    • Aging Behavior in Cast Al-Si-Mg Alloys
    • S. Shivkumar, C. Keller, and D. Apelian: "Aging Behavior in Cast Al-Si-Mg Alloys," AFS Trans., 1990, 98, pp. 905-11.
    • (1990) AFS Trans. , vol.98 , pp. 905-911
    • Shivkumar, S.1    Keller, C.2    Apelian, D.3
  • 2
    • 0142113249 scopus 로고    scopus 로고
    • Age-Hardening Characteristics of Al-Si-Cu-Base Cast Alloys
    • H.G. Kang, M. Kida, H. Miyahara, and K. Ogi: "Age-Hardening Characteristics of Al-Si-Cu-Base Cast Alloys," AFS Trans., 1999, 107, pp. 507-15.
    • (1999) AFS Trans. , vol.107 , pp. 507-515
    • Kang, H.G.1    Kida, M.2    Miyahara, H.3    Ogi, K.4
  • 3
    • 0012834454 scopus 로고
    • Solution Treatment Effects in Cast Al-Si-Cu Alloys
    • N. Crowell and S. Shivkumar: "Solution Treatment Effects in Cast Al-Si-Cu Alloys," AFS Trans., 1995, 103, pp. 721-26.
    • (1995) AFS Trans. , vol.103 , pp. 721-726
    • Crowell, N.1    Shivkumar, S.2
  • 4
    • 0012973019 scopus 로고    scopus 로고
    • Solidification Conditions, Heat Treatment and Tensile Ductility of Al-7Si-0.4Mg Casting Alloys
    • C.H. Caceres and Q.G. Wang: "Solidification Conditions, Heat Treatment and Tensile Ductility of Al-7Si-0.4Mg Casting Alloys," AFS Trans., 1996, 104, pp. 1039-43.
    • (1996) AFS Trans. , vol.104 , pp. 1039-1043
    • Caceres, C.H.1    Wang, Q.G.2
  • 5
    • 0033204382 scopus 로고    scopus 로고
    • Effect of Mg on the Ageing Behavior of Al-Si-Cu 319 Type Aluminum Casting Alloys
    • P. Ouellet and F.H. Samuel: "Effect of Mg on the Ageing Behavior of Al-Si-Cu 319 Type Aluminum Casting Alloys," J. Mater. Sci., 1999, 34(19), pp. 4671-97.
    • (1999) J. Mater. Sci. , vol.34 , Issue.19 , pp. 4671-4697
    • Ouellet, P.1    Samuel, F.H.2
  • 6
    • 0142017927 scopus 로고
    • Effect of Iron Impurity and a Cd Trace Addition on the Delayed Ageing of Al-7Si-0.3Mg Casting Alloy
    • S. Murali, K.S. Raman, and K.S.S. Murthy: "Effect of Iron Impurity and a Cd Trace Addition on the Delayed Ageing of Al-7Si-0.3Mg Casting Alloy," Cast Metals, 1991, 2(1), pp. 31-36.
    • (1991) Cast Metals , vol.2 , Issue.1 , pp. 31-36
    • Murali, S.1    Raman, K.S.2    Murthy, K.S.S.3
  • 7
    • 23044531210 scopus 로고    scopus 로고
    • Effect of Mg and Cu Additions on the Microstructural Characteristics and Tensile Properties of Sr-Modified Al-Si Eutectics Alloys
    • M.A. Moustafa, F.H. Samuel, H.W. Doty, and S. Valtierra: "Effect of Mg and Cu Additions on the Microstructural Characteristics and Tensile Properties of Sr-Modified Al-Si Eutectics Alloys," Int. J. Cast Metals Res., 2002, 14, pp. 235-53.
    • (2002) Int. J. Cast Metals Res. , vol.14 , pp. 235-253
    • Moustafa, M.A.1    Samuel, F.H.2    Doty, H.W.3    Valtierra, S.4
  • 8
    • 0024754686 scopus 로고
    • Effect of Beryllium and Calcium on Aging Behavior of Al-0.75Mg-0.5Si Alloy
    • T. Xiao and W.V. Youdelis: "Effect of Beryllium and Calcium on Aging Behavior of Al-0.75Mg-0.5Si Alloy," Mater. Sci. Technol, 1989, 5(11), pp. 991-94.
    • (1989) Mater. Sci. Technol , vol.5 , Issue.11 , pp. 991-994
    • Xiao, T.1    Youdelis, W.V.2
  • 9
    • 0011701322 scopus 로고
    • Effect of Beryllium on Age Hardening, Defect Structure, and S′ Formation in Al-2.5Cu-1.2 Mg Alloy
    • W.V. Youdellis and W. Fang: "Effect of Beryllium on Age Hardening, Defect Structure, and S′ Formation in Al-2.5Cu-1.2 Mg Alloy," Mater. Sci. Technol, 1994, 10(12), pp. 1031-41.
    • (1994) Mater. Sci. Technol , vol.10 , Issue.12 , pp. 1031-1041
    • Youdellis, W.V.1    Fang, W.2
  • 10
    • 0003869258 scopus 로고
    • Translated by Z. WANG, ZHANG Zhenlu, and X. Zheng, Metallurgical industry Press, Beijing
    • L.F. Mondolfo, Aluminum Alloys: Structure and Property (in Chinese), Translated by Z. WANG, ZHANG Zhenlu, and X. Zheng, Metallurgical industry Press, Beijing, 1988, pp. 203-204, 239-240, 586-93.
    • (1988) Aluminum Alloys: Structure and Property (in Chinese) , pp. 203-204
    • Mondolfo, L.F.1
  • 11
    • 0032098892 scopus 로고    scopus 로고
    • Effects of Be Addition on Microstructures and Mechanical Properties of B319.0 Alloys
    • P.S. Warng, Y.J. Liauh, S.L. Lee, and J.C. Lin: "Effects of Be Addition on Microstructures and Mechanical Properties of B319.0 Alloys," Mater. Chem. Phys., 1998, 53, pp. 195-202.
    • (1998) Mater. Chem. Phys. , vol.53 , pp. 195-202
    • Warng, P.S.1    Liauh, Y.J.2    Lee, S.L.3    Lin, J.C.4
  • 13
    • 0032683183 scopus 로고    scopus 로고
    • Mechanical Properties of Al-11% Si Casting Alloys Containing Trace Be and Sr
    • S-N. Yie, S-L. Lee, Y-H. Lin, and J-C. Lin: "Mechanical Properties of Al-11% Si Casting Alloys Containing Trace Be and Sr," Material Trans., JIM, 1999, 40(4), pp. 294-300.
    • (1999) Material Trans., JIM , vol.40 , Issue.4 , pp. 294-300
    • Yie, S.-N.1    Lee, S.-L.2    Lin, Y.-H.3    Lin, J.-C.4
  • 14
    • 0001067184 scopus 로고
    • Suppression of θ″ Formation in the SiC Whisker-Reinforced Al-4wt% Cu Composites
    • T.S. Kim, T.H. Kim, K.H. Oh, and H.I. Lee: "Suppression of θ" Formation in the SiC Whisker-Reinforced Al-4wt% Cu Composites," J. Mater. Sci., 1992, 27, pp. 2599-605.
    • (1992) J. Mater. Sci. , vol.27 , pp. 2599-2605
    • Kim, T.S.1    Kim, T.H.2    Oh, K.H.3    Lee, H.I.4
  • 15
    • 0032154061 scopus 로고    scopus 로고
    • Precipitation Kinetics in Al6061 and in an Al6061-Alumina Particle Composite
    • S.P. Chen, K.M. Mussert, and S. van der Zwaag: "Precipitation Kinetics in Al6061 and in an Al6061-Alumina Particle Composite," J. Mater. Sci., 1998, 33, pp. 4477-83.
    • (1998) J. Mater. Sci. , vol.33 , pp. 4477-4483
    • Chen, S.P.1    Mussert, K.M.2    Van der Zwaag, S.3
  • 16
    • 0032295311 scopus 로고    scopus 로고
    • DSC Analysis of the Precipitation Behavior of Two Al-Mg-Si Alloys Naturally Aged for Different Times
    • L. Zhen and S.B. Kang: "DSC Analysis of the Precipitation Behavior of Two Al-Mg-Si Alloys Naturally Aged for Different Times," Mater. Lett., 1998, 37(1), pp. 349-53.
    • (1998) Mater. Lett. , vol.37 , Issue.1 , pp. 349-353
    • Zhen, L.1    Kang, S.B.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.