메뉴 건너뛰기




Volumn 20, Issue 4, 2004, Pages 364-369

Depth of cure and surface microhardness of composite resin cured with blue LED curing lights

Author keywords

Composite resin; Depth of cure; Light emitting diode; Microhardness; Photopolymerization

Indexed keywords

COMPOSITE MATERIALS; CURING; LIGHT EMITTING DIODES; MICROHARDNESS; PARAMETER ESTIMATION; QUARTZ; STANDARDS; VICKERS HARDNESS TESTING;

EID: 1342264216     PISSN: 01095641     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0109-5641(03)00130-1     Document Type: Article
Times cited : (82)

References (20)
  • 1
    • 0040024969 scopus 로고    scopus 로고
    • High intensity vs multi-mode intensity
    • High intensity vs multi-mode intensity. CRA Newsl. 22:(12):1998;2-3.
    • (1998) CRA Newsl , vol.22 , Issue.12 , pp. 2-3
  • 4
    • 0032085067 scopus 로고    scopus 로고
    • The effect of the photopolymerization method on the quality of composite resin samples
    • Tarle Z., Meniga A., Ristic M., Sutalo J., Pichler G., Davidson C.L. The effect of the photopolymerization method on the quality of composite resin samples. J Oral Rehabil. 25:1998;436-442.
    • (1998) J Oral Rehabil , vol.25 , pp. 436-442
    • Tarle, Z.1    Meniga, A.2    Ristic, M.3    Sutalo, J.4    Pichler, G.5    Davidson, C.L.6
  • 5
    • 0032062492 scopus 로고    scopus 로고
    • Curing depth of four composite veneering materials polymerised with different laboratory photo-curing units
    • Tanoue N., Koishi Y., Matsumura H., Atsuta M. Curing depth of four composite veneering materials polymerised with different laboratory photo-curing units. J Oral Rehabil. 25:1998;348-352.
    • (1998) J Oral Rehabil , vol.25 , pp. 348-352
    • Tanoue, N.1    Koishi, Y.2    Matsumura, H.3    Atsuta, M.4
  • 6
    • 0032059294 scopus 로고    scopus 로고
    • Properties of four composite veneering materials polymerized with different laboratory photo-curing units
    • Tanoue N., Matsumura H., Atsuta M. Properties of four composite veneering materials polymerized with different laboratory photo-curing units. J Oral Rehabil. 25:1998;358-364.
    • (1998) J Oral Rehabil , vol.25 , pp. 358-364
    • Tanoue, N.1    Matsumura, H.2    Atsuta, M.3
  • 7
    • 0008998168 scopus 로고    scopus 로고
    • Newly developed curing unit using blue light-emitting diodes
    • Fujibayashi K., Ishimaru K., Takahashi N., Kohno A. Newly developed curing unit using blue light-emitting diodes. Dent Jpn. 34:1998;49-53.
    • (1998) Dent Jpn , vol.34 , pp. 49-53
    • Fujibayashi, K.1    Ishimaru, K.2    Takahashi, N.3    Kohno, A.4
  • 8
    • 0034013693 scopus 로고    scopus 로고
    • Light-emitting diode (LED) polymerization of dental composites: Flexural properties and polymerization potential
    • Stahl F., Ashworth S.H., Jandt K.D., Mills R.W. Light-emitting diode (LED) polymerization of dental composites: flexural properties and polymerization potential. Biomaterials. 21:2000;1379-1385.
    • (2000) Biomaterials , vol.21 , pp. 1379-1385
    • Stahl, F.1    Ashworth, S.H.2    Jandt, K.D.3    Mills, R.W.4
  • 10
    • 1342338919 scopus 로고    scopus 로고
    • Resin curing lights, LED
    • Resin curing lights, LED. CRA Newsl. 25:(10):2001;1-2.
    • (2001) CRA Newsl , vol.25 , Issue.10 , pp. 1-2
  • 11
    • 0031152066 scopus 로고    scopus 로고
    • Effect of light wavelength on polymerization of light-cured resins
    • Nomoto R. Effect of light wavelength on polymerization of light-cured resins. Dent Mater. 16:1997;60-73.
    • (1997) Dent Mater , vol.16 , pp. 60-73
    • Nomoto, R.1
  • 12
    • 0033599665 scopus 로고    scopus 로고
    • Dental composite depth of cure with halogen and blue light emitting diode technology
    • Mills R.W., Jandt K.D., Ashworth S.H. Dental composite depth of cure with halogen and blue light emitting diode technology. Br Dent J. 186:1999;388-391.
    • (1999) Br Dent J , vol.186 , pp. 388-391
    • Mills, R.W.1    Jandt, K.D.2    Ashworth, S.H.3
  • 13
    • 1342296414 scopus 로고
    • Incandescent lamps
    • Lighting Association Tokyo: Ohmu-sha. in Japanese
    • Honda K. Incandescent lamps. Lighting Association. The lighting handbook. 1994;129-134 Ohmu-sha, Tokyo. in Japanese.
    • (1994) The Lighting Handbook , pp. 129-134
    • Honda, K.1
  • 14
    • 0032019772 scopus 로고    scopus 로고
    • Curing depth of composite veneering materials polymerised with seven laboratory photo-curing units
    • Tanoue N., Matsumura H., Atsuta M. Curing depth of composite veneering materials polymerised with seven laboratory photo-curing units. J Oral Rehabil. 25:1998;199-203.
    • (1998) J Oral Rehabil , vol.25 , pp. 199-203
    • Tanoue, N.1    Matsumura, H.2    Atsuta, M.3
  • 15
    • 0035378990 scopus 로고    scopus 로고
    • Degree of conversion and temperature rise during polymerization of composite resin samples with blue diodes
    • Knezevic A., Tarle Z., Meniga A., Sutalo J., Pichler G., Ristic M. Degree of conversion and temperature rise during polymerization of composite resin samples with blue diodes. J Oral Rehabil. 28:2001;586-591.
    • (2001) J Oral Rehabil , vol.28 , pp. 586-591
    • Knezevic, A.1    Tarle, Z.2    Meniga, A.3    Sutalo, J.4    Pichler, G.5    Ristic, M.6
  • 16
    • 0031150940 scopus 로고    scopus 로고
    • Depth of cure of light-cured composite resin with light-curing units of different intensity
    • Marais J.T., Dannheimer M.F., Germishuys P.J., Borman J.W. Depth of cure of light-cured composite resin with light-curing units of different intensity. J Dent Assoc S Afr. 52:1997;403-407.
    • (1997) J Dent Assoc S Afr , vol.52 , pp. 403-407
    • Marais, J.T.1    Dannheimer, M.F.2    Germishuys, P.J.3    Borman, J.W.4
  • 17
    • 0030112056 scopus 로고    scopus 로고
    • Surface hardness of light-cured composite resin cured directly or through a transparent matrix using three different light guides
    • Dannheimer M.F., Marais J.T., Borman J., Germishuys P.J., Nel J.C. Surface hardness of light-cured composite resin cured directly or through a transparent matrix using three different light guides. J Dent Assoc S Afr. 51:1996;193-195.
    • (1996) J Dent Assoc S Afr , vol.51 , pp. 193-195
    • Dannheimer, M.F.1    Marais, J.T.2    Borman, J.3    Germishuys, P.J.4    Nel, J.C.5
  • 18
    • 0023663248 scopus 로고
    • Variations in the performances of curing light units by determination of composite setting time
    • Strang R., Macdonald I., O'Hagan S., Murray J., Stephen K.W. Variations in the performances of curing light units by determination of composite setting time. Br Dent J. 162:1987;63-65.
    • (1987) Br Dent J , vol.162 , pp. 63-65
    • Strang, R.1    Macdonald, I.2    O'hagan, S.3    Murray, J.4    Stephen, K.W.5
  • 19
    • 0025289870 scopus 로고
    • An investigation into the microhardness of a light cured composite when cured through varying thicknesses of porcelain
    • Warren K. An investigation into the microhardness of a light cured composite when cured through varying thicknesses of porcelain. J Oral Rehabil. 17:1990;327-334.
    • (1990) J Oral Rehabil , vol.17 , pp. 327-334
    • Warren, K.1
  • 20
    • 0023969675 scopus 로고
    • Effect of exposure time on the depth of polymerization of a visible light-cured composite resin
    • Baharav H., Abraham D., Cardash H.S., Helft M. Effect of exposure time on the depth of polymerization of a visible light-cured composite resin. J Oral Rehabil. 15:1988;167-172.
    • (1988) J Oral Rehabil , vol.15 , pp. 167-172
    • Baharav, H.1    Abraham, D.2    Cardash, H.S.3    Helft, M.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.