1
-
-
0019073337
-
Abrasive wear of white cast irons
-
K.H. Zum Gahr and G.T. Eldis, Abrasive wear of white cast irons [J], Wear, 64(1980), p. 175.
-
(1980)
Wear
, vol.64
, pp. 175
-
-
Gahr, K.H.Z.1
Eldis, G.T.2
-
2
-
-
51249166054
-
Effect of heat treatment on the gouging abrasion resistance of alloy white cast irons
-
I.R. Sare and B.K. Armold, Effect of heat treatment on the gouging abrasion resistance of alloy white cast irons [J], Metall. Mater. Trans. A, 26A(1995), p. 1785.
-
(1995)
Metall. Mater. Trans. A
, vol.26 A
, pp. 1785
-
-
Sare, I.R.1
Armold, B.K.2
-
3
-
-
0030385627
-
Microstructure-property relationships in high chromium white iron alloys
-
C.P. Tabrett, I.R. Sare, and M.R. Ghomashchi, Microstructure-property relationships in high chromium white iron alloys [J], Int. Mater. Rev., 41(1996), No. 2, p. 59.
-
(1996)
Int. Mater. Rev.
, vol.41
, Issue.2
, pp. 59
-
-
Tabrett, C.P.1
Sare, I.R.2
Ghomashchi, M.R.3
-
4
-
-
0020709105
-
Effect of carbide volume fraction on the low stress abrasion resistance of high Cr-Mo white irons
-
J.K. Fulcher, T.H. Kosel, and N.P. Fiore, Effect of carbide volume fraction on the low stress abrasion resistance of high Cr-Mo white irons [J], Wear, 84(1983), p. 313.
-
(1983)
Wear
, vol.84
, pp. 313
-
-
Fulcher, J.K.1
Kosel, T.H.2
Fiore, N.P.3
-
5
-
-
0019172549
-
Abrasive wear of white cast irons
-
J.D. Watson, P.J. Mutton, and I.R. Sare, Abrasive wear of white cast irons [J], Met. Forum, 1980, No. 3, p. 74.
-
(1980)
Met. Forum
, Issue.3
, pp. 74
-
-
Watson, J.D.1
Mutton, P.J.2
Sare, I.R.3
-
6
-
-
0017905174
-
Influence of abrasive hardness on the wear resistance of high chromium irons
-
R.B. Gundlach and J.L. Parks, Influence of abrasive hardness on the wear resistance of high chromium irons [J], Wear, 46(1978), p. 97.
-
(1978)
Wear
, vol.46
, pp. 97
-
-
Gundlach, R.B.1
Parks, J.L.2
-
7
-
-
0018547030
-
Abrasion resistance and fracture toughness of white cast irons
-
I.R. Sare, Abrasion resistance and fracture toughness of white cast irons [J], Met. Technol., 1979, No. 6, p. 412.
-
(1979)
Met. Technol.
, Issue.6
, pp. 412
-
-
Sare, I.R.1
-
8
-
-
0019008881
-
Optimizing fracture toughness and abrasion resistance in white cast irons
-
K.H. Zum Gahr and D.V. Doane, Optimizing fracture toughness and abrasion resistance in white cast irons [J], Metall. Trans., 11A(1980), p. 613.
-
(1980)
Metall. Trans.
, vol.11 A
, pp. 613
-
-
Gahr, K.H.Z.1
Doane, D.V.2
-
9
-
-
0027574834
-
Abrasive wear study of selected white cast irons as liner materials for the mining industry
-
L. Xu, C. Vose, and D. St John, Abrasive wear study of selected white cast irons as liner materials for the mining industry [J], Wear, 162-164 (1993), p. 820.
-
(1993)
Wear
, vol.162-164
, pp. 820
-
-
Xu, L.1
Vose, C.2
St. John, D.3
-
10
-
-
0021862906
-
Laboratory tests of spalling, breaking and abrasion of wear-resistance alloys used in mining and mineral processing
-
R. Blickensderfer and J.H. Tylczak, Laboratory Tests of Spalling, Breaking and Abrasion of Wear-resistance Alloys Used in Mining and Mineral Processing [R], Bureau of Mines, United States, 1985, p. 17.
-
(1985)
Bureau of Mines, United States
, pp. 17
-
-
Blickensderfer, R.1
Tylczak, J.H.2
-
11
-
-
0016377563
-
Optimizing abrasion resistance and toughness in steels and irons for the mining industry
-
Climax Molybdenum Co.
-
D.E. Diesburg and F. Borik, Optimizing abrasion resistance and toughness in steels and irons for the mining industry, [in] Bundesministerium fuer Forschung und Technologie, Forschungsbericht, Technologische Forschung und Entwicklung [C], Climax Molybdenum Co., 1974, p. 15.
-
(1974)
Bundesministerium fuer Forschung und Technologie, Forschungsbericht, Technologische Forschung und Entwicklung
, pp. 15
-
-
Diesburg, D.E.1
Borik, F.2
-
12
-
-
17444445734
-
Effect of heat treatment on the abrasion resistance of alloy white irons
-
C.P. Tabrett and LR. Sare, Effect of heat treatment on the abrasion resistance of alloy white irons [J], Wear, 203-204(1997), p. 206.
-
(1997)
Wear
, vol.203-204
, pp. 206
-
-
Tabrett, C.P.1
Sare, I.R.2
-
13
-
-
0015564303
-
Some metallurgical factors controlling the adhesive and abrasive wear resistance of steels
-
P.L. Hurricks, Some metallurgical factors controlling the adhesive and abrasive wear resistance of steels [J], Wear, 26(1973), p. 285.
-
(1973)
Wear
, vol.26
, pp. 285
-
-
Hurricks, P.L.1
-
14
-
-
0024859435
-
Study of high chromium cast iron on abrasion resistance and impact fatigue resistance
-
X. Fan, L. Lie, and Q. Zhou, Study of high chromium cast iron on abrasion resistance and impact fatigue resistance, [in] International Conference on Wear of Materials [C], 1989, p. 57.
-
(1989)
International Conference on Wear of Materials
, pp. 57
-
-
Fan, X.1
Lie, L.2
Zhou, Q.3
-
16
-
-
0018926872
-
Abrasive wear of brittle solids
-
M.A. Moore and F.S. King, Abrasive wear of brittle solids [J], Wear, 60(1979), p. 123.
-
(1979)
Wear
, vol.60
, pp. 123
-
-
Moore, M.A.1
King, F.S.2
-
18
-
-
0028436675
-
Three-body abrasive wear of ceramic materials
-
T. Yamamoto, M. Olsson, and S. Hogmark, Three-body abrasive wear of ceramic materials [J], Wear, 174(1994), p. 21.
-
(1994)
Wear
, vol.174
, pp. 21
-
-
Yamamoto, T.1
Olsson, M.2
Hogmark, S.3
-
19
-
-
0242371843
-
Effect of subcritical treatment on microstructure and wear resistance of a high chrome white cast iron
-
Chinese source
-
Z.P. Sun, B.L. Shen, S.J. Gao, et al., Effect of subcritical treatment on microstructure and wear resistance of a high chrome white cast iron [J], Trans. Met. Heat Treat. (in Chinese), 24(2003), No. 3, p. 54.
-
(2003)
Trans. Met. Heat Treat.
, vol.24
, Issue.3
, pp. 54
-
-
Sun, Z.P.1
Shen, B.L.2
Gao, S.J.3
-
20
-
-
12144278396
-
Investigation on effect of retained austenite in high chromium cast iron under different wear conditions
-
J.M. Tong and W.L. Zhang, Investigation on effect of retained austenite in high chromium cast iron under different wear conditions [J], Trans. Met. Heat Treat. (in Chinese), 14(1993), No. 2, p. 1.
-
(1993)
Trans. Met. Heat Treat.
, vol.14
, Issue.2
, pp. 1
-
-
Tong, J.M.1
Zhang, W.L.2
|