1
-
-
0032523649
-
The tribochemical behavior of TiN-coatings during fretting wear
-
F. de Wit, B. Blampain, L. Froyen, J.P. Celis, The tribochemical behavior of TiN-coatings during fretting wear, Wear 217 (1998) 215-224.
-
(1998)
Wear
, vol.217
, pp. 215-224
-
-
De Wit, F.1
Blampain, B.2
Froyen, L.3
Celis, J.P.4
-
2
-
-
0034187703
-
Microhardness and structural analysis of (Ti, Al)N, (Ti, Cr)N, (Ti, Zr)N and (Ti, V)N films
-
H. Hasegawa, A. Kimura, T. Suzuki, Microhardness and structural analysis of (Ti, Al)N, (Ti, Cr)N, (Ti, Zr)N and (Ti, V)N films, J. Vac. Sci. Technol. A 18 (3) (2000) 1038-1040.
-
(2000)
J. Vac. Sci. Technol. A
, vol.18
, Issue.3
, pp. 1038-1040
-
-
Hasegawa, H.1
Kimura, A.2
Suzuki, T.3
-
3
-
-
0034228389
-
Structural determination of wear debris generated from sliding wear tests on ceramic coatings using Raman microscopy
-
C.P. Constable, J. Yarwood, P. Hovsepian, L.A. Donohue, D.B. Lewis, W.D. Munz, Structural determination of wear debris generated from sliding wear tests on ceramic coatings using Raman microscopy, J. Vac. Sci. Technol. A 18 (4) (2000) 1681-1689.
-
(2000)
J. Vac. Sci. Technol. A
, vol.18
, Issue.4
, pp. 1681-1689
-
-
Constable, C.P.1
Yarwood, J.2
Hovsepian, P.3
Donohue, L.A.4
Lewis, D.B.5
Munz, W.D.6
-
4
-
-
0036956589
-
Investigation of wear processes on worn tools using Raman microscopy
-
C.P. Constable, J. Yarwood, G. Robinson, Q. Luo, D.B. Lewis, W.D. Munz, Investigation of wear processes on worn tools using Raman microscopy, Surf. Eng. 18 (2) (2002) 127-132.
-
(2002)
Surf. Eng.
, vol.18
, Issue.2
, pp. 127-132
-
-
Constable, C.P.1
Yarwood, J.2
Robinson, G.3
Luo, Q.4
Lewis, D.B.5
Munz, W.D.6
-
5
-
-
0026223437
-
Friction and wear behavior of TiN in air: The chemistry of transfer films and debris formation
-
I.L. Singer, S. Fayeulle, P.D. Ehni, Friction and wear behavior of TiN in air: the chemistry of transfer films and debris formation, Wear 149 (1991) 375-394.
-
(1991)
Wear
, vol.149
, pp. 375-394
-
-
Singer, I.L.1
Fayeulle, S.2
Ehni, P.D.3
-
6
-
-
0036503606
-
Expressing wear rate in sliding contacts based on dissipated energy
-
M.Z. Huq, J.P. Cells, Expressing wear rate in sliding contacts based on dissipated energy, Wear 252 (2002) 375-383.
-
(2002)
Wear
, vol.252
, pp. 375-383
-
-
Huq, M.Z.1
Cells, J.P.2
-
7
-
-
0029361018
-
Oxidational wear of TiN coatings on tool steel and nitrided tool steel in unlubricated fretting
-
H. Mohrbacher, B. Blanpain, J.P. Celis, J.R. Roos, L. Stals, M. Van Stappen, Oxidational wear of TiN coatings on tool steel and nitrided tool steel in unlubricated fretting, Wear 188 (1995) 130-137.
-
(1995)
Wear
, vol.188
, pp. 130-137
-
-
Mohrbacher, H.1
Blanpain, B.2
Celis, J.P.3
Roos, J.R.4
Stals, L.5
Van Stappen, M.6
-
8
-
-
0037124998
-
High temperature fretting behavior of plasma vapor deposition TiN coating
-
A. Ramalho, J.P. Celis, High temperature fretting behavior of plasma vapor deposition TiN coating, Surf. Coat. Technol. 155 (2002) 169-175.
-
(2002)
Surf. Coat. Technol.
, vol.155
, pp. 169-175
-
-
Ramalho, A.1
Celis, J.P.2
-
9
-
-
0032193189
-
The crystallization of amorphous debris on titanium nitride coatings influenced by sliding wear conditions
-
E. de Wit, L. Froyen, J.P. Celis, The crystallization of amorphous debris on titanium nitride coatings influenced by sliding wear conditions, Wear 221 (1998) 124-133.
-
(1998)
Wear
, vol.221
, pp. 124-133
-
-
De Wit, E.1
Froyen, L.2
Celis, J.P.3
-
10
-
-
0028419608
-
Tribo-oxidation of a TiN coating sliding against corundum
-
E. Vancoille, B. Blanpain, X. Ye, J.P. Cells, J.R. Roos, Tribo-oxidation of a TiN coating sliding against corundum, J. Mater. Res. 9 (4) (1994) 992-998.
-
(1994)
J. Mater. Res.
, vol.9
, Issue.4
, pp. 992-998
-
-
Vancoille, E.1
Blanpain, B.2
Ye, X.3
Cells, J.P.4
Roos, J.R.5
-
11
-
-
0036847567
-
The role of atmosphere and lubricants in the oxidational wear of metals
-
H.S. Hong, The role of atmosphere and lubricants in the oxidational wear of metals, Tribol. Int. 35 (2002) 725-729.
-
(2002)
Tribol. Int.
, vol.35
, pp. 725-729
-
-
Hong, H.S.1
-
12
-
-
0027590258
-
Dry sliding wear of TiN-based ternary PVD coatings
-
E. Vancoille, J.P. Celis, J.R. Roos, Dry sliding wear of TiN-based ternary PVD coatings, Wear 165 (1993) 41-49.
-
(1993)
Wear
, vol.165
, pp. 41-49
-
-
Vancoille, E.1
Celis, J.P.2
Roos, J.R.3
-
13
-
-
0029253161
-
Fretting of titanium nitride and diamond-like carbon coatings at high frequencies and low amplitude
-
K. Schouterden, B. Blanpain, J.P. Celis, O. Vingsbo, Fretting of titanium nitride and diamond-like carbon coatings at high frequencies and low amplitude, Wear 181-183 (1995) 86-93.
-
(1995)
Wear
, vol.181-183
, pp. 86-93
-
-
Schouterden, K.1
Blanpain, B.2
Celis, J.P.3
Vingsbo, O.4
-
14
-
-
0033508849
-
Fretting wear of multilayered (Ti, Al)N/TiN coatings in air of different relative humidity
-
M.Z. Huq, J.P. Celis, Fretting wear of multilayered (Ti, Al)N/TiN coatings in air of different relative humidity, Wear 225-229 (1999) 53-64.
-
(1999)
Wear
, vol.225-229
, pp. 53-64
-
-
Huq, M.Z.1
Celis, J.P.2
-
15
-
-
0035354201
-
2O composite coating at elevated temperature
-
2O composite coating at elevated temperature, Wear 249 (2001) 440-451.
-
(2001)
Wear
, vol.249
, pp. 440-451
-
-
Ouyang, J.H.1
Sasaki, S.2
Umeda, K.3
-
16
-
-
0035309480
-
Wear behavior of a REFEL SiC containing fluorides up to 900°C
-
M. Shuaib, T.J. Davies, Wear behavior of a REFEL SiC containing fluorides up to 900°C, Wear 249 (2001) 20-30.
-
(2001)
Wear
, vol.249
, pp. 20-30
-
-
Shuaib, M.1
Davies, T.J.2
-
17
-
-
0022489379
-
Material selection for hard coatings
-
H. Holleck, Material selection for hard coatings, J. Vac. Sci. Technol. 4 (6) (1986) 2661-2669.
-
(1986)
J. Vac. Sci. Technol.
, vol.4
, Issue.6
, pp. 2661-2669
-
-
Holleck, H.1
|