6
-
-
0026413564
-
Relaxation in liquids, polymers and plastic crystals-strong/fragile patterns and problems
-
Angell C.A. Relaxation in liquids, polymers and plastic crystals-strong/fragile patterns and problems J. Non-Cryst. Solids 131-133 1991 13-31
-
(1991)
J. Non-Cryst. Solids
, vol.131-133
, pp. 13-31
-
-
Angell, C.A.1
-
9
-
-
0033716541
-
Indentation of glass as a function of temperature
-
Le Bourhis E. Metayer D. Indentation of glass as a function of temperature J. Non-Cryst. Solids 272 2000 34-38
-
(2000)
J. Non-Cryst. Solids
, vol.272
, pp. 34-38
-
-
Le Bourhis, E.1
Metayer, D.2
-
10
-
-
0033687580
-
The brittle to ductile transition in a soda-lime-silica glass
-
Rouxel T. Sanglebœf J.C. The brittle to ductile transition in a soda-lime-silica glass J. Non-Cryst. Solids 271 2000 224-235
-
(2000)
J. Non-Cryst. Solids
, vol.271
, pp. 224-235
-
-
Rouxel, T.1
Sanglebœf, J.C.2
-
11
-
-
0035399101
-
Change in Vickers hardness at the glass transition region for fragile and strong glasses
-
Watanabe T. Benino Y. Komatsu T. Change in Vickers hardness at the glass transition region for fragile and strong glasses J. Non-Cryst. Solids 286 2001 141-145
-
(2001)
J. Non-Cryst. Solids
, vol.286
, pp. 141-145
-
-
Watanabe, T.1
Benino, Y.2
Komatsu, T.3
-
12
-
-
0038016844
-
Vitrification of lead-rich solid ashes from incineration of hazardous industrial wastes
-
Kavouras P. Kaimakamis G. Ioannidis Th. A. Kehagias Th. Komninou Ph. Kokkou S. Pavlidou E. Antonopoulos J. Sofoniou M. Zouboulis A. Hadjiantoniou C.P. Prakouras A. Karakostas Th. Vitrification of lead-rich solid ashes from incineration of hazardous industrial wastes Waste Manag. 23 2003 361-371
-
(2003)
Waste Manag.
, vol.23
, pp. 361-371
-
-
Kavouras, P.1
Kaimakamis, G.2
Ioannidis Th., A.3
Kehagias, Th.4
Komninou, Ph.5
Kokkou, S.6
Pavlidou, E.7
Antonopoulos, J.8
Sofoniou, M.9
Zouboulis, A.10
Hadjiantoniou, C.P.11
Prakouras, A.12
Karakostas, Th.13
-
13
-
-
0034325740
-
The crystallization kinetics of iron rich glass in different atmospheres
-
Karamanov A. Pisciella P. Pelino M. The crystallization kinetics of iron rich glass in different atmospheres J. Europ. Cer. Soc. 20 2000 2233-2237
-
(2000)
J. Europ. Cer. Soc.
, vol.20
, pp. 2233-2237
-
-
Karamanov, A.1
Pisciella, P.2
Pelino, M.3
-
14
-
-
0033226191
-
Iron-rich sintered glass-ceramics from industrial wastes
-
Karamanov A. Taglieri G. Pelino M. Iron-rich sintered glass-ceramics from industrial wastes J. Am. Ceram. Soc. 82 1999 3012-3016
-
(1999)
J. Am. Ceram. Soc.
, vol.82
, pp. 3012-3016
-
-
Karamanov, A.1
Taglieri, G.2
Pelino, M.3
-
15
-
-
0001234017
-
Structural role of lead in lead silicate glasses derived from XPS spectra
-
Wang P.W. Zhang L. Structural role of lead in lead silicate glasses derived from XPS spectra J. Non-Cryst. Solids 194 1996 129-134
-
(1996)
J. Non-Cryst. Solids
, vol.194
, pp. 129-134
-
-
Wang, P.W.1
Zhang, L.2
-
17
-
-
0342954983
-
Changes of the mechanical properties during the crystallization of bio-active glass-ceramics
-
Unyi T. Juhász A. Tasnádi P. Lendvai J. Changes of the mechanical properties during the crystallization of bio-active glass-ceramics J. Mater. Sci. 35 2000 3059-3068
-
(2000)
J. Mater. Sci.
, vol.35
, pp. 3059-3068
-
-
Unyi, T.1
Juhász, A.2
Tasnádi, P.3
Lendvai, J.4
-
21
-
-
0035219436
-
Chemical durability of glasses obtained by vitrification of industrial wastes
-
Pisciella P. Crisucci S. Karamanov A. Pelino M. Chemical durability of glasses obtained by vitrification of industrial wastes Waste Manag 21 2001 1-9
-
(2001)
Waste Manag
, vol.21
, pp. 1-9
-
-
Pisciella, P.1
Crisucci, S.2
Karamanov, A.3
Pelino, M.4
-
22
-
-
0024908225
-
Interpretation of the indentation size effect in Vickers microhardness measurements-absolute hardness of materials
-
Farges G. Degout D. Interpretation of the indentation size effect in Vickers microhardness measurements-absolute hardness of materials Thin Solid Films 181 1989 365-374
-
(1989)
Thin Solid Films
, vol.181
, pp. 365-374
-
-
Farges, G.1
Degout, D.2
-
23
-
-
0024681283
-
An explanation of the indentation size effect in ceramics
-
Bull S.J. Page T.F. Yoffe E.H. An explanation of the indentation size effect in ceramics Phil. Mag. Let 59 1989 281-288
-
(1989)
Phil. Mag. Let
, vol.59
, pp. 281-288
-
-
Bull, S.J.1
Page, T.F.2
Yoffe, E.H.3
-
24
-
-
84987335986
-
A critical evaluation of indentation techniques for determining fracture toughness: I, direct crack measurements
-
Antsis G.R. Chantikul P. Lawn B.R. Marshall D.B. A critical evaluation of indentation techniques for determining fracture toughness: I, direct crack measurements J. Am. Ceram. Soc. 64 1981 533-538
-
(1981)
J. Am. Ceram. Soc.
, vol.64
, pp. 533-538
-
-
Antsis, G.R.1
Chantikul, P.2
Lawn, B.R.3
Marshall, D.B.4
-
26
-
-
84987306805
-
A simple method for determining elastic-modulus-to-hardness ratios using Knoop indentation measurements
-
Marshall D.B. Noma T. Evans A.G. A simple method for determining elastic-modulus-to-hardness ratios using Knoop indentation measurements J. Am. Ceram. Soc. 65 1982 C175-C176
-
(1982)
J. Am. Ceram. Soc.
, vol.65
-
-
Marshall, D.B.1
Noma, T.2
Evans, A.G.3
-
29
-
-
0030085165
-
The effect of indentation-induced cracking on the apparent microhardness
-
Li H. Bradt R.C. The effect of indentation-induced cracking on the apparent microhardness J. Mater. Sci. 31 1996 1065-1070
-
(1996)
J. Mater. Sci.
, vol.31
, pp. 1065-1070
-
-
Li, H.1
Bradt, R.C.2
-
32
-
-
0029519930
-
Indentation deformation and fracture toughness of densified silicate glass
-
Zhang Z. Soga N. Hirao K. Indentation deformation and fracture toughness of densified silicate glass J. Mater. Sci. 30 1995 6359-6362
-
(1995)
J. Mater. Sci.
, vol.30
, pp. 6359-6362
-
-
Zhang, Z.1
Soga, N.2
Hirao, K.3
-
34
-
-
0022162022
-
Effect of contact residual stress relaxation on fracture strength of indented soda-lime glass
-
Roach D.H. Cooper A.R. Effect of contact residual stress relaxation on fracture strength of indented soda-lime glass J. Am. Ceram. Soc. 68 1985 632-636
-
(1985)
J. Am. Ceram. Soc.
, vol.68
, pp. 632-636
-
-
Roach, D.H.1
Cooper, A.R.2
-
35
-
-
0019058721
-
Flaw characteristics in dynamic fatigue: The influence of residual contact stresses
-
Marshall D.B. Lawn B.R. Flaw characteristics in dynamic fatigue: the influence of residual contact stresses J. Am. Ceram. Soc. 63 1980 532-536
-
(1980)
J. Am. Ceram. Soc.
, vol.63
, pp. 532-536
-
-
Marshall, D.B.1
Lawn, B.R.2
-
36
-
-
0020751114
-
Theory of fatigue for brittle flaws originating from residual stress concentrations
-
Fuller E.R. Lawn B.R. Cook R.F. Theory of fatigue for brittle flaws originating from residual stress concentrations J. Am. Ceram. Soc. 66 1983 314-321
-
(1983)
J. Am. Ceram. Soc.
, vol.66
, pp. 314-321
-
-
Fuller, E.R.1
Lawn, B.R.2
Cook, R.F.3
-
37
-
-
84986413041
-
Fracture toughness measurement of glass and ceramic materials using chevron-notched specimens
-
Reddy K.P.R. Fontana E.H. Helfinstine J.D. Fracture toughness measurement of glass and ceramic materials using chevron-notched specimens J. Am. Ceram. Soc. 71 1988 C310-C313
-
(1988)
J. Am. Ceram. Soc.
, vol.71
-
-
Reddy, K.P.R.1
Fontana, E.H.2
Helfinstine, J.D.3
-
38
-
-
0037466570
-
Reliability of the chevron-notch technique for fracture toughness determination in glass
-
Boccaccini A.R. Rawlings R.D. Dlouhý I. Reliability of the chevron-notch technique for fracture toughness determination in glass Mater. Sci. Eng. A. Struct. 347 2003 102-108
-
(2003)
Mater. Sci. Eng. A. Struct.
, vol.347
, pp. 102-108
-
-
Boccaccini, A.R.1
Rawlings, R.D.2
Dlouhý, I.3
|