Volumn 155-156, Issue 1-3, 2004, Pages 1256-1260

Effect of substrate crystallographic orientation on wettability and adhesion in several representative systems

Author keywords

Adhesion; Contact angle; Crystallographic orientation; Wetting

Indexed keywords

ADHESION; CHEMICAL BONDS; CONTACT ANGLE; CRYSTALLOGRAPHY; SUBSTRATES; WETTING; MOLTEN MATERIALS;

EID: 10044269565     PISSN: 09240136     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.jmatprotec.2004.04.212     Document Type: Article
Times cited : (19)

References (18)
  • 1
    • 0001216544 scopus 로고
    • Interfece and capillary phenomena in crystal growth and melting processes
    • Yu.V. Naidich, N.F. Grigorenko, V.M. Perevertailo, Interfece and capillary phenomena in crystal growth and melting processes, J. Cryst. Growth 53 (1981) 261-272.
    • (1981) J. Cryst. Growth , vol.53 , pp. 261-272
    • Naidich, Yu.V.1    Grigorenko, N.F.2    Perevertailo, V.M.3
  • 4
    • 0032640067 scopus 로고    scopus 로고
    • The role of van der Waals inter-actions on wetting and adhesion in metal/carbon systems
    • O. Dezellus, N. Eustathopoulos, The role of van der Waals inter-actions on wetting and adhesion in metal/carbon systems, Scripta Mater. 40 (1999) 1283-1288.
    • (1999) Scripta Mater. , vol.40 , pp. 1283-1288
    • Dezellus, O.1    Eustathopoulos, N.2
  • 5
    • 0032036145 scopus 로고    scopus 로고
    • Wettability of diamond by liquid pure tin
    • K. Nogi, M. Nishikawa, H. Fujii, S. Hara, Wettability of diamond by liquid pure tin, Acta Mater. 46 (1998) 2305-2311.
    • (1998) Acta Mater. , vol.46 , pp. 2305-2311
    • Nogi, K.1    Nishikawa, M.2    Fujii, H.3    Hara, S.4
  • 6
    • 0026866882 scopus 로고
    • Wettability of MgO single crystal by liquid pure Pb, Sn and Bi
    • K. Nogi, M. Tsujimoto, K. Ogino, N. Iwamoto, Wettability of MgO single crystal by liquid pure Pb, Sn and Bi, Acta Metall. Mater. 40 (1992) 1045-1050.
    • (1992) Acta Metall. Mater. , vol.40 , pp. 1045-1050
    • Nogi, K.1    Tsujimoto, M.2    Ogino, K.3    Iwamoto, N.4
  • 7
    • 0028460528 scopus 로고
    • Surface observation of MgO single crystal with atomic force microscope and crystal-lographic orientation dependence of Wettability of MgO by liquid metals
    • H. Takeda, M. Takeda, K. Nogi, K. Ogino, Surface observation of MgO single crystal with atomic force microscope and crystal-lographic orientation dependence of Wettability of MgO by liquid metals, Mater. Trans. JIM 35 (1994) 466-472.
    • (1994) Mater. Trans. JIM , vol.35 , pp. 466-472
    • Takeda, H.1    Takeda, M.2    Nogi, K.3    Ogino, K.4
  • 10
    • 0043011233 scopus 로고    scopus 로고
    • The influence of surface structure on wetting of α-alumina by Al in a reduced atmosphere
    • P. Shen, H. Fujii, T. Matsumoto, K. Nogi, The influence of surface structure on wetting of α-alumina by Al in a reduced atmosphere, Acta Mater. 51 (2003) 4897-4906.
    • (2003) Acta Mater. , vol.51 , pp. 4897-4906
    • Shen, P.1    Fujii, H.2    Matsumoto, T.3    Nogi, K.4
  • 11
    • 0037092753 scopus 로고    scopus 로고
    • 3 (0 0 0 1) surface from low-energy electron diffraction: Al termination and evidence for anomalously large thermal vibrations
    • 3 (0 0 0 1) surface from low-energy electron diffraction: Al termination and evidence for anomalously large thermal vibrations, Phys. Rev. B 65 (2002) 195405.
    • (2002) Phys. Rev. B , vol.65 , pp. 195405
    • Scares, E.A.1    Van Hove, M.A.2    Walters, C.F.3    McCarty, K.F.4
  • 13
    • 0001542390 scopus 로고
    • Electronic structure and energetics of sapphire (0 0 0 1) and (1 1̄ 0 2) surface
    • J. Guo, D.E. Ellis, D.J. Lam, Electronic structure and energetics of sapphire (0 0 0 1) and (1 1̄ 0 2) surface, Phys. Rev. B 45 (1992) 13647-13656.
    • (1992) Phys. Rev. B , vol.45 , pp. 13647-13656
    • Guo, J.1    Ellis, D.E.2    Lam, D.J.3
  • 14
    • 0028383033 scopus 로고
    • 3 (0 0 0 1) surface: Atomic and electronic structure
    • 3 (0 0 0 1) surface: atomic and electronic structure, J. Am. Ceram. Soc. 77 (1994) 323-334.
    • (1994) J. Am. Ceram. Soc. , vol.77 , pp. 323-334
    • Gautier, M.1
  • 17
    • 0021727167 scopus 로고
    • Surface of magnesia and alumina
    • W.D. Kingry (Ed.), The American Ceramic Society
    • 3 Ceramics, The American Ceramic Society, 1984, pp. 176-189.
    • (1984) 3 Ceramics , pp. 176-189
    • Tasker, P.W.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.