Mechanical properties and microstructure changes after long-term aging at 700°C for a nickel-base superalloy

Author keywords

Mechanical property; Microstructure; Nickel base superalloy; Precipitate

Indexed keywords

AGE HARDENING; HEAT TREATMENT; MECHANICAL PROPERTIES; METALLOGRAPHIC MICROSTRUCTURE; NICKEL ALLOYS;

EID: 0347513612     PISSN: 10058850     EISSN: None     Source Type: Journal    
DOI: None     Document Type: Article
Times cited : (11)

References (10)
  • 1
    • 0347175803 scopus 로고    scopus 로고
    • Properties and long-term aging at different temperature for a new nickel base superalloy
    • Chinese source
    • S. Zhao and X. Xie, Properties and long-term aging at different temperature for a new nickel base superalloy [J], Acta Metall. Sin. (in Chinese), 39(2003), p.399.
    • (2003) Acta Metall. Sin. , vol.39 , pp. 399
    • Zhao, S.1    Xie, X.2
  • 2
    • 0346545489 scopus 로고    scopus 로고
    • The corrosion resistance of nickel-containing alloys in coal-fired boiler environments
    • NACE International, Houston
    • G.D. Smith, S.J. Patel, N.C. Farr, et al., The corrosion resistance of nickel-containing alloys in coal-fired boiler environments, [in] Corrosion 99 [C], NACE International, Houston, 1999, p.12.
    • (1999) Corrosion'99 , pp. 12
    • Smith, G.D.1    Patel, S.J.2    Farr, N.C.3
  • 3
    • 0346545488 scopus 로고    scopus 로고
    • Introduction of an advanced superheater alloy for coal-fired boilers
    • NACE International, Houston
    • G.D. Smith and H.W. Sizek, Introduction of an advanced superheater alloy for coal-fired boilers, [in] Corrosion 2000 [C], NACE International, Houston, 2000, p.00256.1.
    • (2000) Corrosion 2000
    • Smith, G.D.1    Sizek, H.W.2
  • 4
    • 0041114126 scopus 로고    scopus 로고
    • Laboratory-simulated fuel-ash corrosion of superheater tubes in coal-fired ultra-supercritical-boilers
    • P. Castello, V. Cuttmann, N. Farr, et al. Laboratory-simulated fuel-ash corrosion of superheater tubes in coal-fired ultra-supercritical-boilers [J], Mater. Corros., 51(2000), p.786.
    • (2000) Mater. Corros. , vol.51 , pp. 786
    • Castello, P.1    Cuttmann, V.2    Farr, N.3
  • 5
    • 0001340390 scopus 로고    scopus 로고
    • Phase precipitation and phase stability in Nimonic 263
    • J.-C. Zhao, V. ravikumar, and A.M. Beltran, Phase precipitation and phase stability in Nimonic 263 [J], Metall. Mater. Trans. A, 32A(2001), p.1271.
    • (2001) Metall. Mater. Trans. A , vol.32 A , pp. 1271
    • Zhao, J.-C.1    Ravikumar, V.2    Beltran, A.M.3
  • 6
    • 0004209969 scopus 로고
    • Ni-350, Orange. NJ: Alloy Digest, Inc.
    • Alloy Digest [M], Ni-350, Orange. NJ: Alloy Digest, Inc, 1987.
    • (1987) Alloy Digest
  • 9
    • 0027624170 scopus 로고
    • Numerical determination of the elastic driving force for directional coarsening in nickel-superalloys
    • S. Socrate and D.M. Parks, Numerical determination of the elastic driving force for directional coarsening in nickel-superalloys [J], Acta Metall. Mater., 41(1993), p.2185.
    • (1993) Acta Metall. Mater. , vol.41 , pp. 2185
    • Socrate, S.1    Parks, D.M.2
  • 10
    • 0036478362 scopus 로고    scopus 로고
    • Characteristics of microstructure and element distribution of nickel-base single crystal superalloy CMSX-2 after high temperature creep
    • Chinese source
    • Z. Peng, Y. Ren, Y. Luo, et al., Characteristics of microstructure and element distribution of nickel-base single crystal superalloy cmsx-2 after high temperature creep [J], Acta Metall. Sin. (in Chinese), 38(2002), p.135.
    • (2002) Acta Metall. Sin. , vol.38 , pp. 135
    • Peng, Z.1    Ren, Y.2    Luo, Y.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.