Volumn 25, Issue 1-3, 2004, Pages 80-83

NMR relaxometry study of cement hydration in the presence of different oxidic fine fraction materials

Author keywords

[No Author keywords available]

Indexed keywords

ACTINIDES; FILLERS; HYDRATION; IONS; LEAD COMPOUNDS; OXIDATION; PARAMAGNETIC MATERIALS; PORTLAND CEMENT; POWDERS; REACTION KINETICS; SOLIDIFICATION;

EID: 0347354815     PISSN: 09262040     EISSN: None     Source Type: Journal    
DOI: 10.1016/j.ssnmr.2003.05.003     Document Type: Article
Times cited : (27)

References (8)
  • 3
    • 0347566284 scopus 로고    scopus 로고
    • Stabilization and Solidification of Hazardous, Radioactive and Mixed Wastes, 3rd Edition
    • T.M. Gilliam, C.C. Wiles (Eds.), American Society for Testing and Materials, Philadelphia PA
    • T.M. Gilliam, C.C. Wiles, in: T.M. Gilliam, C.C. Wiles (Eds.), Stabilization and Solidification of Hazardous, Radioactive and Mixed Wastes, 3rd Edition, ASTM STP 1240, American Society for Testing and Materials, Philadelphia PA, 1996.
    • (1996) ASTM STP , vol.1240
    • Gilliam, T.M.1    Wiles, C.C.2
  • 4
    • 0035421673 scopus 로고    scopus 로고
    • Influence of lead, zinc, iron (III) and chromium (III) oxides on the setting time and strength development of Portland cement
    • Fernández Olmo I., Chacon E., Irabien A. Influence of lead, zinc, iron (III) and chromium (III) oxides on the setting time and strength development of Portland cement. Cem. Concr. Res. 31:2001;1213-1219.
    • (2001) Cem. Concr. Res. , vol.31 , pp. 1213-1219
    • Fernández Olmo, I.1    Chacon, E.2    Irabien, A.3
  • 5
    • 0036628837 scopus 로고    scopus 로고
    • Aqueous solubility diagrams for cementitious waste stabilitation systems 3. Mechanism of zinc immobilization by calcium silicate hydrate
    • Tommaseo C.E., Kersten M. Aqueous solubility diagrams for cementitious waste stabilitation systems 3. Mechanism of zinc immobilization by calcium silicate hydrate. Environ. Sci. Technol. 36:2002;2919-2925.
    • (2002) Environ. Sci. Technol. , vol.36 , pp. 2919-2925
    • Tommaseo, C.E.1    Kersten, M.2
  • 6
    • 0001290830 scopus 로고    scopus 로고
    • Blastfurnace slag cements - A construction material with very unusual nuclear spin relaxation behavior during hardening
    • Nestle N., Dakkouri M., Geier O., Freude D., Kärger J. Blastfurnace slag cements - a construction material with very unusual nuclear spin relaxation behavior during hardening. J. Appl. Phys. 88:2000;4269-4273.
    • (2000) J. Appl. Phys. , vol.88 , pp. 4269-4273
    • Nestle, N.1    Dakkouri, M.2    Geier, O.3    Freude, D.4    Kärger, J.5
  • 7
    • 0037148263 scopus 로고    scopus 로고
    • Transient high concentrations of chain anions in hydrating cement - Indications from proton spin relaxation measurements
    • Nestle N., Zimmermann C., Dakkouri M., Kärger J. Transient high concentrations of chain anions in hydrating cement - indications from proton spin relaxation measurements. J. Phys. D. 35:2002;166-171.
    • (2002) J. Phys. D , vol.35 , pp. 166-171
    • Nestle, N.1    Zimmermann, C.2    Dakkouri, M.3    Kärger, J.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.