Volumn 4948, Issue , 2002, Pages 539-547

Visualization of low-velocity dynamic indentation cracking of an epoxy and polymethylmethacrylate

Author keywords

Conical; Elastic plastic indentation; High speed photography; Radial and median and cracking; Stone tools

Indexed keywords

CRACKING (CHEMICAL); ELASTOPLASTICITY; EPOXY RESINS; POLYMETHYL METHACRYLATES; VISUALIZATION;

EID: 0344551224     PISSN: 0277786X     EISSN: None     Source Type: Conference Proceeding    
DOI: 10.1117/12.516948     Document Type: Conference Paper
Times cited : (2)

References (13)
  • 1
    • 0014496330 scopus 로고
    • The influence of sample preparation on Palmqvist's method for toughness testing of cemented carbides
    • H. E. Exner, "The influence of sample preparation on Palmqvist's method for toughness testing of cemented carbides," Trans. Metallurgical Soc. AIME, 245, pp. 677-683, 1969.
    • (1969) Trans. Metallurgical Soc. AIME , vol.245 , pp. 677-683
    • Exner, H.E.1
  • 2
    • 0000333650 scopus 로고
    • Micomechanics of crack nucleation during indentations
    • J. T. Hagan, "Micomechanics of crack nucleation during indentations," J. Mater. Sci., 14, pp. 2975-2980, 1979.
    • (1979) J. Mater. Sci. , vol.14 , pp. 2975-2980
    • Hagan, J.T.1
  • 3
    • 0025462680 scopus 로고
    • Quasi-static indentation cracking of thermally tempered soda-lime glass with spherical and Vickers indenters
    • M. M. Chaudhri and M. A. Phillips, "Quasi-static indentation cracking of thermally tempered soda-lime glass with spherical and Vickers indenters," Philos. Mag. A 62, 1-27, 1990.
    • (1990) Philos. Mag. , vol.A62 , pp. 1-27
    • Chaudhri, M.M.1    Phillips, M.A.2
  • 4
    • 21144484459 scopus 로고
    • Indentation cracking in soda-lime glass and Ni-Zn ferrite under Knoop and conical indenters and residual stress measurements
    • S. Chandrasekar and M. M. Chaudhri, "Indentation cracking in soda-lime glass and Ni-Zn ferrite under Knoop and conical indenters and residual stress measurements," Philos. Mag. A. 67, 1187-1218, 1993.
    • (1993) Philos. Mag. , vol.A67 , pp. 1187-1218
    • Chandrasekar, S.1    Chaudhri, M.M.2
  • 5
    • 0025418269 scopus 로고
    • Direct observation and analysis of indentation cracking in glasses and ceramics
    • R. F. Cook and G. M. Pharr, "Direct observation and analysis of indentation cracking in glasses and ceramics," J. Am. Ceram. Soc., 73, 787-817, 1990.
    • (1990) J. Am. Ceram. Soc. , vol.73 , pp. 787-817
    • Cook, R.F.1    Pharr, G.M.2
  • 6
    • 17644444347 scopus 로고    scopus 로고
    • In situ observations of indentation damage in single crystals of MgO
    • M. M. Chaudhri and Y. Enomoto, "In situ observations of indentation damage in single crystals of MgO," Wear, 233-235, 717-726, 1999.
    • (1999) Wear , vol.233-235 , pp. 717-726
    • Chaudhri, M.M.1    Enomoto, Y.2
  • 8
    • 0022184053 scopus 로고
    • Measurement of dislocation velocities in potassium chloride single crystals from dynamic localised loading experiments
    • (Strasbourg)
    • M. M. Chaudhri, "Measurement of dislocation velocities in potassium chloride single crystals from dynamic localised loading experiments," SPIE vol. 491 High Speed Photography (Strasbourg 1984) pp. 595 - 599.
    • (1984) SPIE Vol. 491 High Speed Photography , pp. 595-599
    • Chaudhri, M.M.1
  • 9
    • 0018985510 scopus 로고
    • Single particle impact damage of fused silica
    • M. M. Chaudhri and P. A. Brophy, "Single particle impact damage of fused silica," J. Mater. Sci., 15, 345-352, 1980.
    • (1980) J. Mater. Sci. , vol.15 , pp. 345-352
    • Chaudhri, M.M.1    Brophy, P.A.2
  • 10
    • 0030128567 scopus 로고    scopus 로고
    • Interpretation of river line patterns on indentation generated fracture surfaces with comments on the fractal characteristics described by Djordjevic et al
    • D. Hull, "Interpretation of river line patterns on indentation generated fracture surfaces with comments on the fractal characteristics described by Djordjevic et al.," J. Mater. Sci. Letters, 15, 651-653, 1996.
    • (1996) J. Mater. Sci. Letters , vol.15 , pp. 651-653
    • Hull, D.1
  • 11
    • 0029324178 scopus 로고
    • Fractal and topological characterization of branching patterns on the fracture surface of cross-linked dimethacrylate resins
    • Z. V. Djordjevic, X. F. Li, W. S. Shin, S. L. Wunder, and Baran, G. R., "Fractal and topological characterization of branching patterns on the fracture surface of cross-linked dimethacrylate resins," J. Mater. Sci., 30, 2968-2980, 1995.
    • (1995) J. Mater. Sci. , vol.30 , pp. 2968-2980
    • Djordjevic, Z.V.1    Li, X.F.2    Shin, W.S.3    Wunder, S.L.4    Baran, G.R.5
  • 13
    • 0006869931 scopus 로고
    • Stress fields round indentations in poly(methyl methacrylate)
    • K. E. Puttick, L. S. A. Smith, and L. E. Miller, "Stress fields round indentations in poly(methyl methacrylate)," J. Phys. D: appl. phys., 10, 617-631, 1977.
    • (1977) J. Phys. D: Appl. Phys. , vol.10 , pp. 617-631
    • Puttick, K.E.1    Smith, L.S.A.2    Miller, L.E.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.