Effects of composition on crystallization behaviour and mechanical properties of bioactive glass-ceramics in the MgO-CaO-SiO2-P2O5 system

Author keywords

[No Author keywords available]

Indexed keywords

COMPOSITION EFFECTS; COMPRESSIVE STRENGTH; CRYSTALLIZATION; ENERGY DISPERSIVE SPECTROSCOPY; FOURIER TRANSFORM INFRARED SPECTROSCOPY; FRACTURE TOUGHNESS; GLASS; LIME; MAGNESIA; PHOSPHATES; SCANNING ELECTRON MICROSCOPY; SILICA;

EID: 0343789628     PISSN: 02728842     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0272-8842(99)00072-3     Document Type: Article
Times cited : (48)

References (19)
  • 1
    • 0000591909 scopus 로고
    • Apatite and wollastonite containing glass-ceramics for prosthetic application
    • Kokubo T., Shigematsu M., Nagashima Y.et al. Apatite and wollastonite containing glass-ceramics for prosthetic application. Bull. Inst. Chem. Res. Kyoto Univ. 60:1982;260-268.
    • (1982) Bull. Inst. Chem. Res. Kyoto Univ. , vol.60 , pp. 260-268
    • Kokubo, T.1    Shigematsu, M.2    Nagashima, Y.3
  • 3
    • 0022075275 scopus 로고
    • Mechanical properties of a new type of apatite containing glass-ceramic for prosthetic application
    • Kokubo T., Ito S., Shigematsu M., Sakka S., Yamamuro T. Mechanical properties of a new type of apatite containing glass-ceramic for prosthetic application. J. Mater. Sci. 20:1985;2001-2004.
    • (1985) J. Mater. Sci , vol.20 , pp. 2001-2004
    • Kokubo, T.1    Ito, S.2    Shigematsu, M.3    Sakka, S.4    Yamamuro, T.5
  • 4
    • 84935306536 scopus 로고
    • New type of apatite containing glass-ceramics for prosthetic application
    • Kokubo T., Ito S., Shigemetsu M.et al. New type of apatite containing glass-ceramics for prosthetic application. Glastechn. Ber. 56k:1983;695-700.
    • (1983) Glastechn. Ber. , vol.56 , pp. 695-700
    • Kokubo, T.1    Ito, S.2    Shigemetsu, M.3
  • 5
    • 0022093658 scopus 로고
    • A new glass-ceramic for bone replacement: Evaluation of its bonding to bone tissue
    • Nakamura T., Yamamuro T., Higashi S.et al. A new glass-ceramic for bone replacement: evaluation of its bonding to bone tissue. J. Biomed. Mater. Res. 19:1985;685-698.
    • (1985) J. Biomed. Mater. Res. , vol.19 , pp. 685-698
    • Nakamura, T.1    Yamamuro, T.2    Higashi, S.3
  • 6
    • 0023436650 scopus 로고
    • Compositional dependence of formation of an apatite layar on glass-ceramic in simulated physiological solution
    • Kasuga T., Nakagawa K., Yoshida M., Miyade E. Compositional dependence of formation of an apatite layar on glass-ceramic in simulated physiological solution. J. Mater. Sci. 22:1987;3721-3724.
    • (1987) J. Mater. Sci. , vol.22 , pp. 3721-3724
    • Kasuga, T.1    Nakagawa, K.2    Yoshida, M.3    Miyade, E.4
  • 9
    • 0025486655 scopus 로고
    • Diametral compression tests of silicon carbide fiber reinforced glass
    • Okada A. Diametral compression tests of silicon carbide fiber reinforced glass. J. Mater. Sci. 25:1990;3901-3905.
    • (1990) J. Mater. Sci. , vol.25 , pp. 3901-3905
    • Okada, A.1
  • 10
    • 0000738741 scopus 로고
    • Fracture toughness determinations by indentation
    • Evans A.G., Charles E.A. Fracture toughness determinations by indentation. J. Am. Ceram. Soc. 59:1976;371-372.
    • (1976) J. Am. Ceram. Soc. , vol.59 , pp. 371-372
    • Evans, A.G.1    Charles, E.A.2
  • 12
    • 84987335986 scopus 로고
    • A critical evaluation of indentation techniques for measuring fracture toughness: 1. Direct crack measurements
    • Anstis G.R., Chantikul P., Lawn B.R., Marshall D.B. A critical evaluation of indentation techniques for measuring fracture toughness: 1. Direct crack measurements. J. Am. Ceram. Soc. 64:1981;533-538.
    • (1981) J. Am. Ceram. Soc. , vol.64 , pp. 533-538
    • Anstis, G.R.1    Chantikul, P.2    Lawn, B.R.3    Marshall, D.B.4
  • 13
    • 0016953209 scopus 로고
    • Strength degradation of brittle surfaces: sharp indenters
    • B.R. Lawn, E.R. Fuller, S.M. Wiederhorn, Strength degradation of brittle surfaces: sharp indenters, J. Am. Ceram. Soc. 59, 1976, 193-197.
    • (1976) J. Am. Ceram. Soc. , vol.59 , pp. 193-197
    • Lawn, B.R.1    Fuller, E.R.2    Wiederhorn, S.M.3
  • 14
    • 84987368857 scopus 로고
    • A critical evaluation of indentation techniques for measuring fracture toughness: II. Strength method
    • Chantikul P., Anstis G.R., Lawn B.R., Marshall D.B. A critical evaluation of indentation techniques for measuring fracture toughness: II. Strength method. J. Am. Ceram. Soc. 64:1981;539-543.
    • (1981) J. Am. Ceram. Soc. , vol.64 , pp. 539-543
    • Chantikul, P.1    Anstis, G.R.2    Lawn, B.R.3    Marshall, D.B.4
  • 15
    • 84914801099 scopus 로고
    • Compressive measurement of indentation fracture toughness with Berkovich and Vickers indenters
    • Dukino R.D., Swain M.V. Compressive measurement of indentation fracture toughness with Berkovich and Vickers indenters. J. Am. Ceram. Soc. 75:1992;3299-3304.
    • (1992) J. Am. Ceram. Soc. , vol.75 , pp. 3299-3304
    • Dukino, R.D.1    Swain, M.V.2
  • 16
    • 34249836589 scopus 로고
    • Chemical reaction of bioactive glass and glass-ceramic with a simulated body fluid
    • Kokubo T., Kushitani H., Ohtsuki G.et al. Chemical reaction of bioactive glass and glass-ceramic with a simulated body fluid. J. Mater. Sci. in Medicine. 3:1992;79-83.
    • (1992) J. Mater. Sci. in Medicine , vol.3 , pp. 79-83
    • Kokubo, T.1    Kushitani, H.2    Ohtsuki, G.3
  • 17
    • 0025418004 scopus 로고
    • Surface chemistry of bioactive glass-ceramics
    • Kokubo T. Surface chemistry of bioactive glass-ceramics. J. Non-Cryst. Solids. 120:1990;138-151.
    • (1990) J. Non-Cryst. Solids , vol.120 , pp. 138-151
    • Kokubo, T.1
  • 18
    • 0002873956 scopus 로고
    • Surface structure of load bearable glass-ceramic A-W
    • P. Vincenzini. Amsterdam: Elsevier
    • Kokubo T., Hayashi S., Sakka S.et al. Surface structure of load bearable glass-ceramic A-W. Vincenzini P. High Tech Ceramics. 1987;75-185 Elsevier, Amsterdam.
    • (1987) High Tech Ceramics , pp. 75-185
    • Kokubo, T.1    Hayashi, S.2    Sakka, S.3
  • 19
    • 0028441727 scopus 로고
    • Bone-like hydroxyapatite induction by a gel-derived titania on a titanium substrate
    • Panjian L., Kangasnieme L., Ikka G., Kokuba T. Bone-like hydroxyapatite induction by a gel-derived titania on a titanium substrate. J. Am. Ceram. Soc. 77:1994;1307-1312.
    • (1994) J. Am. Ceram. Soc. , vol.77 , pp. 1307-1312
    • Panjian, L.1    Kangasnieme, L.2    Ikka, G.3    Kokuba, T.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.