메뉴 건너뛰기




Volumn 125, Issue 9, 2003, Pages 2597-2609

Formation and structure of self-assembled monolayers of alkanethiolates on palladium

Author keywords

[No Author keywords available]

Indexed keywords

CHEMICAL BONDS; CONFORMATIONS; ELLIPSOMETRY; LIGHT ABSORPTION; LIGHT REFLECTION; PALLADIUM; POLYCRYSTALLINE MATERIALS; THIN FILMS; X RAY PHOTOELECTRON SPECTROSCOPY;

EID: 0242417588     PISSN: 00027863     EISSN: None     Source Type: Journal    
DOI: 10.1021/ja028692+     Document Type: Article
Times cited : (318)

References (60)
  • 6
    • 0031632795 scopus 로고    scopus 로고
    • Xia, Y.; Whitesides, G. M. Annu. Rev. Mater. Sci. 1998, 28, 153-184. Xia, Y.; Zhao, X.-M.; Kim, E.; Whitesides, G. M. Chem. Mater. 1995, 7, 2332-2337. Xia, Y.; Rogers, J. A.; Paul, K. E.; Whitesides, G. M. Chem. Rev. 1999, 99, 1823-1848. Rogers, J. A.; Bao, Z.; Baldwin, K.; Dodabalapur, A.; Crone, B.; Raju, V. R.; Kuck, V.; Katz, H.; Amundson, K.; Ewing, J.; Drzaic, P. Proc. Natl. Acad. Sci. U.S.A. 2001, 98, 4835-4840. Michel, B.; Bernard, A.; Bietsch, A.; Delamarche, E.; Geissler, M.; Juncker, D.; Kind, H.; Renault, J. P.; Rothuizen, H.; Schmid, H.; Schmidt-Winkel, P.; Stutz, R.; Wolf, H. IBM J. Res. Dev. 2001, 45, 697-719. There is also a number of patents describing SAMs of alkanethiolates on palladium; these patents are listed in the Supporting Information.
    • (1998) Annu. Rev. Mater. Sci. , vol.28 , pp. 153-184
    • Xia, Y.1    Whitesides, G.M.2
  • 7
    • 33751154943 scopus 로고
    • Xia, Y.; Whitesides, G. M. Annu. Rev. Mater. Sci. 1998, 28, 153-184. Xia, Y.; Zhao, X.-M.; Kim, E.; Whitesides, G. M. Chem. Mater. 1995, 7, 2332-2337. Xia, Y.; Rogers, J. A.; Paul, K. E.; Whitesides, G. M. Chem. Rev. 1999, 99, 1823-1848. Rogers, J. A.; Bao, Z.; Baldwin, K.; Dodabalapur, A.; Crone, B.; Raju, V. R.; Kuck, V.; Katz, H.; Amundson, K.; Ewing, J.; Drzaic, P. Proc. Natl. Acad. Sci. U.S.A. 2001, 98, 4835-4840. Michel, B.; Bernard, A.; Bietsch, A.; Delamarche, E.; Geissler, M.; Juncker, D.; Kind, H.; Renault, J. P.; Rothuizen, H.; Schmid, H.; Schmidt-Winkel, P.; Stutz, R.; Wolf, H. IBM J. Res. Dev. 2001, 45, 697-719. There is also a number of patents describing SAMs of alkanethiolates on palladium; these patents are listed in the Supporting Information.
    • (1995) Chem. Mater. , vol.7 , pp. 2332-2337
    • Xia, Y.1    Zhao, X.-M.2    Kim, E.3    Whitesides, G.M.4
  • 8
    • 0346704264 scopus 로고    scopus 로고
    • Xia, Y.; Whitesides, G. M. Annu. Rev. Mater. Sci. 1998, 28, 153-184. Xia, Y.; Zhao, X.-M.; Kim, E.; Whitesides, G. M. Chem. Mater. 1995, 7, 2332-2337. Xia, Y.; Rogers, J. A.; Paul, K. E.; Whitesides, G. M. Chem. Rev. 1999, 99, 1823-1848. Rogers, J. A.; Bao, Z.; Baldwin, K.; Dodabalapur, A.; Crone, B.; Raju, V. R.; Kuck, V.; Katz, H.; Amundson, K.; Ewing, J.; Drzaic, P. Proc. Natl. Acad. Sci. U.S.A. 2001, 98, 4835-4840. Michel, B.; Bernard, A.; Bietsch, A.; Delamarche, E.; Geissler, M.; Juncker, D.; Kind, H.; Renault, J. P.; Rothuizen, H.; Schmid, H.; Schmidt-Winkel, P.; Stutz, R.; Wolf, H. IBM J. Res. Dev. 2001, 45, 697-719. There is also a number of patents describing SAMs of alkanethiolates on palladium; these patents are listed in the Supporting Information.
    • (1999) Chem. Rev. , vol.99 , pp. 1823-1848
    • Xia, Y.1    Rogers, J.A.2    Paul, K.E.3    Whitesides, G.M.4
  • 9
    • 0035942286 scopus 로고    scopus 로고
    • Xia, Y.; Whitesides, G. M. Annu. Rev. Mater. Sci. 1998, 28, 153-184. Xia, Y.; Zhao, X.-M.; Kim, E.; Whitesides, G. M. Chem. Mater. 1995, 7, 2332-2337. Xia, Y.; Rogers, J. A.; Paul, K. E.; Whitesides, G. M. Chem. Rev. 1999, 99, 1823-1848. Rogers, J. A.; Bao, Z.; Baldwin, K.; Dodabalapur, A.; Crone, B.; Raju, V. R.; Kuck, V.; Katz, H.; Amundson, K.; Ewing, J.; Drzaic, P. Proc. Natl. Acad. Sci. U.S.A. 2001, 98, 4835-4840. Michel, B.; Bernard, A.; Bietsch, A.; Delamarche, E.; Geissler, M.; Juncker, D.; Kind, H.; Renault, J. P.; Rothuizen, H.; Schmid, H.; Schmidt-Winkel, P.; Stutz, R.; Wolf, H. IBM J. Res. Dev. 2001, 45, 697-719. There is also a number of patents describing SAMs of alkanethiolates on palladium; these patents are listed in the Supporting Information.
    • (2001) Proc. Natl. Acad. Sci. U.S.A. , vol.98 , pp. 4835-4840
    • Rogers, J.A.1    Bao, Z.2    Baldwin, K.3    Dodabalapur, A.4    Crone, B.5    Raju, V.R.6    Kuck, V.7    Katz, H.8    Amundson, K.9    Ewing, J.10    Drzaic, P.11
  • 10
    • 0035465563 scopus 로고    scopus 로고
    • Xia, Y.; Whitesides, G. M. Annu. Rev. Mater. Sci. 1998, 28, 153-184. Xia, Y.; Zhao, X.-M.; Kim, E.; Whitesides, G. M. Chem. Mater. 1995, 7, 2332-2337. Xia, Y.; Rogers, J. A.; Paul, K. E.; Whitesides, G. M. Chem. Rev. 1999, 99, 1823-1848. Rogers, J. A.; Bao, Z.; Baldwin, K.; Dodabalapur, A.; Crone, B.; Raju, V. R.; Kuck, V.; Katz, H.; Amundson, K.; Ewing, J.; Drzaic, P. Proc. Natl. Acad. Sci. U.S.A. 2001, 98, 4835-4840. Michel, B.; Bernard, A.; Bietsch, A.; Delamarche, E.; Geissler, M.; Juncker, D.; Kind, H.; Renault, J. P.; Rothuizen, H.; Schmid, H.; Schmidt-Winkel, P.; Stutz, R.; Wolf, H. IBM J. Res. Dev. 2001, 45, 697-719. There is also a number of patents describing SAMs of alkanethiolates on palladium; these patents are listed in the Supporting Information.
    • (2001) IBM J. Res. Dev. , vol.45 , pp. 697-719
    • Michel, B.1    Bernard, A.2    Bietsch, A.3    Delamarche, E.4    Geissler, M.5    Juncker, D.6    Kind, H.7    Renault, J.P.8    Rothuizen, H.9    Schmid, H.10    Schmidt-Winkel, P.11    Stutz, R.12    Wolf, H.13
  • 12
    • 0004202943 scopus 로고
    • American Technical Publishers, Homewood
    • Moniz, B. J. Metallurgy, 2nd ed.; American Technical Publishers: Homewood, 1994.
    • (1994) Metallurgy, 2nd Ed.
    • Moniz, B.J.1
  • 15
    • 0242613199 scopus 로고    scopus 로고
    • Two-step upgrading of olefinic sulfur-rich cracked naphtha by hydrodesulfurization and treatment over metal-containing MCM-22 zeolites, PCT Int. Appl. 0208360, 2002
    • Walsh, D. E. Two-step upgrading of olefinic sulfur-rich cracked naphtha by hydrodesulfurization and treatment over metal-containing MCM-22 zeolites, PCT Int. Appl. 0208360, 2002; Qian, W.; Yoda, Y.; Hirai, Y.; Ishihara, A.; Kabe, T. Applied Catalysis, A: General 1999, 184, 81-88. Shirai, M.; Pu, Y.; Arai, M.; Nishiyama, Y. Appl. Surf. Sci. 1998, 126, 99-106. Sugioka, M.; Sado, F.; Matsumoto, Y.; Maesaki, N. Catal. Today 1996, 29, 255-259.
    • Walsh, D.E.1
  • 16
    • 0002222797 scopus 로고    scopus 로고
    • Walsh, D. E. Two-step upgrading of olefinic sulfur-rich cracked naphtha by hydrodesulfurization and treatment over metal-containing MCM-22 zeolites, PCT Int. Appl. 0208360, 2002; Qian, W.; Yoda, Y.; Hirai, Y.; Ishihara, A.; Kabe, T. Applied Catalysis, A: General 1999, 184, 81-88. Shirai, M.; Pu, Y.; Arai, M.; Nishiyama, Y. Appl. Surf. Sci. 1998, 126, 99-106. Sugioka, M.; Sado, F.; Matsumoto, Y.; Maesaki, N. Catal. Today 1996, 29, 255-259.
    • (1999) Applied Catalysis, A: General , vol.184 , pp. 81-88
    • Qian, W.1    Yoda, Y.2    Hirai, Y.3    Ishihara, A.4    Kabe, T.5
  • 17
    • 0032048740 scopus 로고    scopus 로고
    • Walsh, D. E. Two-step upgrading of olefinic sulfur-rich cracked naphtha by hydrodesulfurization and treatment over metal-containing MCM-22 zeolites, PCT Int. Appl. 0208360, 2002; Qian, W.; Yoda, Y.; Hirai, Y.; Ishihara, A.; Kabe, T. Applied Catalysis, A: General 1999, 184, 81-88. Shirai, M.; Pu, Y.; Arai, M.; Nishiyama, Y. Appl. Surf. Sci. 1998, 126, 99-106. Sugioka, M.; Sado, F.; Matsumoto, Y.; Maesaki, N. Catal. Today 1996, 29, 255-259.
    • (1998) Appl. Surf. Sci. , vol.126 , pp. 99-106
    • Shirai, M.1    Pu, Y.2    Arai, M.3    Nishiyama, Y.4
  • 18
    • 0000439241 scopus 로고    scopus 로고
    • Walsh, D. E. Two-step upgrading of olefinic sulfur-rich cracked naphtha by hydrodesulfurization and treatment over metal-containing MCM-22 zeolites, PCT Int. Appl. 0208360, 2002; Qian, W.; Yoda, Y.; Hirai, Y.; Ishihara, A.; Kabe, T. Applied Catalysis, A: General 1999, 184, 81-88. Shirai, M.; Pu, Y.; Arai, M.; Nishiyama, Y. Appl. Surf. Sci. 1998, 126, 99-106. Sugioka, M.; Sado, F.; Matsumoto, Y.; Maesaki, N. Catal. Today 1996, 29, 255-259.
    • (1996) Catal. Today , vol.29 , pp. 255-259
    • Sugioka, M.1    Sado, F.2    Matsumoto, Y.3    Maesaki, N.4
  • 19
    • 0034248008 scopus 로고    scopus 로고
    • Kind, H.; Gieissler, M.; Schmid, H.; Michel, B.; Kern, K.; Delamarche, E. Langmuir 2000, 16, 6367-6373. Brandow, S. L.; Chen, M.; Wang, T.; Dulcey, C. S.; Calver, J. M.; Bohland, J. F.; Calabrese, G. S.; Dressick, W. J. J. Electrochem. Soc. 1997, 144, 3425-3434.
    • (2000) Langmuir , vol.16 , pp. 6367-6373
    • Kind, H.1    Gieissler, M.2    Schmid, H.3    Michel, B.4    Kern, K.5    Delamarche, E.6
  • 22
    • 33845184543 scopus 로고
    • Bain, C. D.; Evall, J.; Whitesides, G. M. J. Am. Chem. Soc. 1989, 111, 7155-7164. Bain, C. D.; Whitesides, G. M. J. Am. Chem. Soc. 1989, 111, 7164-7175. Haag, R.; Rampi, M. A.; Holmlin, R. E.; Whitesides, G. M. J. Am. Chem. Soc. 1999, 121, 7895-7906.
    • (1989) J. Am. Chem. Soc. , vol.111 , pp. 7155-7164
    • Bain, C.D.1    Evall, J.2    Whitesides, G.M.3
  • 23
    • 33845185565 scopus 로고
    • Bain, C. D.; Evall, J.; Whitesides, G. M. J. Am. Chem. Soc. 1989, 111, 7155-7164. Bain, C. D.; Whitesides, G. M. J. Am. Chem. Soc. 1989, 111, 7164-7175. Haag, R.; Rampi, M. A.; Holmlin, R. E.; Whitesides, G. M. J. Am. Chem. Soc. 1999, 121, 7895-7906.
    • (1989) J. Am. Chem. Soc. , vol.111 , pp. 7164-7175
    • Bain, C.D.1    Whitesides, G.M.2
  • 24
    • 0033200218 scopus 로고    scopus 로고
    • Bain, C. D.; Evall, J.; Whitesides, G. M. J. Am. Chem. Soc. 1989, 111, 7155-7164. Bain, C. D.; Whitesides, G. M. J. Am. Chem. Soc. 1989, 111, 7164-7175. Haag, R.; Rampi, M. A.; Holmlin, R. E.; Whitesides, G. M. J. Am. Chem. Soc. 1999, 121, 7895-7906.
    • (1999) J. Am. Chem. Soc. , vol.121 , pp. 7895-7906
    • Haag, R.1    Rampi, M.A.2    Holmlin, R.E.3    Whitesides, G.M.4
  • 26
    • 0242697362 scopus 로고    scopus 로고
    • note
    • While the surface will chemisorb oxygen readily, palladium resists oxidation in bulk up to 400 °C. See ref 9.
  • 28
    • 31544435825 scopus 로고
    • Adamson, A. W.; Gast, A. P. Physical Chemistry of Surfaces, 6th ed.; John Wiley & Sons: New York, 1997. Bain, C. D.; Whitesides, G. M. J. Am. Chem. Soc. 1988, 110, 3665-3666.
    • (1988) J. Am. Chem. Soc. , vol.110 , pp. 3665-3666
    • Bain, C.D.1    Whitesides, G.M.2
  • 30
    • 0001296191 scopus 로고
    • Biebuyck, H. A.; Bain, C. D.; Whitesides, G. M. Langmuir 1994, 10, 1825-1831; Bain, C. D.; Biebuyck, H. A.; Whitesides, G. M. Langmuir 1989, 5, 723-727.
    • (1994) Langmuir , vol.10 , pp. 1825-1831
    • Biebuyck, H.A.1    Bain, C.D.2    Whitesides, G.M.3
  • 31
  • 33
    • 0028422095 scopus 로고
    • Bucher, J. P.; Santesson, L.; Kem, K. Langmuir 1994, 10, 979-983. McCarley, R. L.; Dunaway, D. J.; Willicut, R. J. Langmuir 1993, 9, 2775-2777. Yamada, R.; Wano, H.; Uosaki, K. Langmuir 2000, 16, 5523-5525.
    • (1994) Langmuir , vol.10 , pp. 979-983
    • Bucher, J.P.1    Santesson, L.2    Kem, K.3
  • 34
    • 0000608369 scopus 로고
    • Bucher, J. P.; Santesson, L.; Kem, K. Langmuir 1994, 10, 979-983. McCarley, R. L.; Dunaway, D. J.; Willicut, R. J. Langmuir 1993, 9, 2775-2777. Yamada, R.; Wano, H.; Uosaki, K. Langmuir 2000, 16, 5523-5525.
    • (1993) Langmuir , vol.9 , pp. 2775-2777
    • McCarley, R.L.1    Dunaway, D.J.2    Willicut, R.J.3
  • 35
    • 0034205216 scopus 로고    scopus 로고
    • Bucher, J. P.; Santesson, L.; Kem, K. Langmuir 1994, 10, 979-983. McCarley, R. L.; Dunaway, D. J.; Willicut, R. J. Langmuir 1993, 9, 2775-2777. Yamada, R.; Wano, H.; Uosaki, K. Langmuir 2000, 16, 5523-5525.
    • (2000) Langmuir , vol.16 , pp. 5523-5525
    • Yamada, R.1    Wano, H.2    Uosaki, K.3
  • 38
    • 0003998388 scopus 로고
    • The refractive index selected is an average value of the refractive indices of hydrocarbons and thiols. The refractive indices for hexadecane (1.4345), decanethiol (1.4509), dodecanethiol (1.4589), and octadecanethiol (1.4645) are reported in the CRC Handbook of Chemistry and Physics, 75th ed.; 1994.
    • (1994) CRC Handbook of Chemistry and Physics, 75th Ed.
  • 39
    • 0021788046 scopus 로고
    • Allara, D. L.; Nuzzo, R. G. Langmuir 1985, 1, 52-66; Allara, D. L.; A., B.; C. A., P. Macromolecules 1978, 11, 1215-1220.
    • (1985) Langmuir , vol.1 , pp. 52-66
    • Allara, D.L.1    Nuzzo, R.G.2
  • 40
    • 33947092525 scopus 로고
    • Allara, D. L.; Nuzzo, R. G. Langmuir 1985, 1, 52-66; Allara, D. L.; A., B.; C. A., P. Macromolecules 1978, 11, 1215-1220.
    • (1978) Macromolecules , vol.11 , pp. 1215-1220
    • Allara, D.L.1
  • 48
    • 0242444964 scopus 로고    scopus 로고
    • note
    • We note that, in pattern transfer experiments, the regions functionalized by μCP do dissolve in the etchant when exposed for times longer than the time required to etch the unpatterned regions. We have not determined whether this observation is a result of dissolution of the palladium-sulfide layer or is a result of etching at defect sites and subsequent dissolution of the underlying palladium.
  • 49
    • 0345979435 scopus 로고    scopus 로고
    • Ulman, A. Chem. Rev. 1996, 96, 1533-1554.
    • (1996) Chem. Rev. , vol.96 , pp. 1533-1554
    • Ulman, A.1
  • 52
    • 25744449978 scopus 로고
    • Strong, L.; Whitesides, G. M. Langmuir 1988, 4, 546-558. Dubois, L. H.; Zegarski, B. R.; Nuzzo, R. G. J. Chem. Phys. 1993, 98, 678-688.
    • (1988) Langmuir , vol.4 , pp. 546-558
    • Strong, L.1    Whitesides, G.M.2
  • 55
    • 13544254996 scopus 로고    scopus 로고
    • Bomermann, J.; Huck, M.; Kuntze, J.; Rauch, T.; Speller, S.; Helland, W. Surf. Sci. 1996, 358, 849-854. Liu, W.; Mitchell, K. A. R.; Bemdt, W. Surf. Sci. 1997, 393, L119-L125. Speller, S.; Rauch, T.; Bomermann, J.; Borrmann, P.; Heiland, W. Surf. Sci. 1999, 441, 107-116.
    • (1996) Surf. Sci. , vol.358 , pp. 849-854
    • Bomermann, J.1    Huck, M.2    Kuntze, J.3    Rauch, T.4    Speller, S.5    Helland, W.6
  • 56
    • 0039973999 scopus 로고    scopus 로고
    • Bomermann, J.; Huck, M.; Kuntze, J.; Rauch, T.; Speller, S.; Helland, W. Surf. Sci. 1996, 358, 849-854. Liu, W.; Mitchell, K. A. R.; Bemdt, W. Surf. Sci. 1997, 393, L119-L125. Speller, S.; Rauch, T.; Bomermann, J.; Borrmann, P.; Heiland, W. Surf. Sci. 1999, 441, 107-116.
    • (1997) Surf. Sci. , vol.393
    • Liu, W.1    Mitchell, K.A.R.2    Bemdt, W.3
  • 57
    • 0033359825 scopus 로고    scopus 로고
    • Bomermann, J.; Huck, M.; Kuntze, J.; Rauch, T.; Speller, S.; Helland, W. Surf. Sci. 1996, 358, 849-854. Liu, W.; Mitchell, K. A. R.; Bemdt, W. Surf. Sci. 1997, 393, L119-L125. Speller, S.; Rauch, T.; Bomermann, J.; Borrmann, P.; Heiland, W. Surf. Sci. 1999, 441, 107-116.
    • (1999) Surf. Sci. , vol.441 , pp. 107-116
    • Speller, S.1    Rauch, T.2    Bomermann, J.3    Borrmann, P.4    Heiland, W.5
  • 58
    • 0003406742 scopus 로고    scopus 로고
    • John Wiley & Sons: New York
    • The nearest-neighbor distance between palladium atoms in the (111) plane is 2.75 Å. Kittel, C. Introduction to Solid State Physics, 7th ed.; John Wiley & Sons: New York, 1996.
    • (1996) Introduction to Solid State Physics, 7th Ed.
    • Kittel, C.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.