메뉴 건너뛰기




Volumn 82, Issue 2, 2003, Pages 211-219

Hydrolytic stability of phenolic antioxidants and its effect on their performance in high-density polyethylene

Author keywords

HPLC ESI MS; Hydrolysis; Pipes; Polyethylene; Stabilizer

Indexed keywords

EXTRUSION; HYDROLYSIS; PHENOLS; POLYETHYLENES;

EID: 0141921690     PISSN: 01413910     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0141-3910(03)00209-X     Document Type: Conference Paper
Times cited : (25)

References (30)
  • 1
    • 0028174013 scopus 로고
    • Polyethylene Pipe in the British Gas Distribution System
    • Greig J.M. Polyethylene pipe in the British gas distribution system. Plast Rubber Compos Process Appl. 21:1994;133-140.
    • (1994) Plast Rubber Compos Process Appl , vol.21 , pp. 133-140
    • Greig, J.M.1
  • 2
    • 0347256390 scopus 로고
    • Thermoplastics pipes for the transport of fluids - Methods of extrapolation of hydrostatic stress rupture data to determine the long-term hydrostatic strength of thermoplastics pipe materials
    • Technical Report ISO/TR 9080. Thermoplastics pipes for the transport of fluids - methods of extrapolation of hydrostatic stress rupture data to determine the long-term hydrostatic strength of thermoplastics pipe materials. 1992.
    • (1992) Technical Report , vol.ISO-TR 9080
  • 3
    • 0025388386 scopus 로고
    • Molecular structure and morphology of crosslinked polyethylene in an aged hot-water pipe
    • Gedde U.W., Ifwarson M. Molecular structure and morphology of crosslinked polyethylene in an aged hot-water pipe. Polym Eng Sci. 30(4):1990;202-210.
    • (1990) Polym Eng Sci. , vol.30 , Issue.4 , pp. 202-210
    • Gedde, U.W.1    Ifwarson, M.2
  • 5
    • 0141931685 scopus 로고    scopus 로고
    • Long term durability of cross-linked polyethylene tubing used in chlorinated hot water systems
    • Plast Pipeline Syst Millennium, Conf. Pap. 68FFA2
    • Gill TS, Knapp RJ, Bradley SW, Bradley WL. Long term durability of cross-linked polyethylene tubing used in chlorinated hot water systems. In: Proceedings Plast Pipes X., Plast Pipeline Syst Millennium, Conf. Pap. 68FFA2. 1998. p. 641-50.
    • (1998) Proceedings Plast Pipes X , pp. 641-650
    • Gill, T.S.1    Knapp, R.J.2    Bradley, S.W.3    Bradley, W.L.4
  • 6
    • 0032131610 scopus 로고    scopus 로고
    • Assessment of lifetime of hot-water polyethylene pipes based on oxidation induction time data
    • Viebke J., Gedde U.W. Assessment of lifetime of hot-water polyethylene pipes based on oxidation induction time data. Polym Eng Sci. 38(8):1998;1244-1250.
    • (1998) Polym Eng Sci. , vol.38 , Issue.8 , pp. 1244-1250
    • Viebke, J.1    Gedde, U.W.2
  • 7
    • 0141931686 scopus 로고
    • Oxidation induction time (OIT) - A tool to characterize the thermo-oxidative degradation of PE-MD pipe resin?
    • Edinburgh, Scotland, UK, 18-21 September
    • Schmutz Th, Kramer E, Zweifel H. Oxidation induction time (OIT) - a tool to characterize the thermo-oxidative degradation of PE-MD pipe resin? In: Proceedings Plastics Pipes IX, Institute of Materials, Edinburgh, Scotland, UK, 18-21 September 1995.
    • (1995) Proceedings Plastics Pipes IX, Institute of Materials
    • Schmutz, Th.1    Kramer, E.2    Zweifel, H.3
  • 8
    • 11744281051 scopus 로고    scopus 로고
    • Lifetime prediction for PE-MD pipes. Influence of additives on thermo-oxidative stability
    • Hilton Head Island, South Carolina, USA, 14 May
    • Schmutz Th, Zweifel H, Kramer E, Dörner G. Lifetime prediction for PE-MD pipes. Influence of additives on thermo-oxidative stability. In: Proceedings Ann. Meeting of The Plastics Pipe Institute, Hilton Head Island, South Carolina, USA, 14 May 1996.
    • (1996) Proceedings Ann. Meeting of The Plastics Pipe Institute
    • Schmutz, Th.1    Zweifel, H.2    Kramer, E.3    Dörner, G.4
  • 9
    • 0027569489 scopus 로고
    • Molecular structure, morphology, and antioxidant consumption in polybutene-1 pipes in hot-water applications
    • Karlsson K., Eriksson P.-A., Hedenqvist M., Ifwarson M., Smith G.D., Gedde U.W. Molecular structure, morphology, and antioxidant consumption in polybutene-1 pipes in hot-water applications. Polym Eng Sci. 33(5):1993;303-310.
    • (1993) Polym Eng Sci. , vol.33 , Issue.5 , pp. 303-310
    • Karlsson, K.1    Eriksson, P.-A.2    Hedenqvist, M.3    Ifwarson, M.4    Smith, G.D.5    Gedde, U.W.6
  • 10
    • 84989029849 scopus 로고
    • Modeling of antioxidant loss from polyolefins in hot-water applications. I.: Model and application of medium density polyethylene pipes
    • Smith G.D., Karlsson K., Gedde U.W. Modeling of antioxidant loss from polyolefins in hot-water applications. I.: Model and application of medium density polyethylene pipes. Polym Eng Sci. 32(10):1992;658-667.
    • (1992) Polym Eng Sci. , vol.32 , Issue.10 , pp. 658-667
    • Smith, G.D.1    Karlsson, K.2    Gedde, U.W.3
  • 11
    • 0031143544 scopus 로고    scopus 로고
    • Antioxidant diffusion in polyethylene hot-water pipes
    • Viebke J., Gedde U.W. Antioxidant diffusion in polyethylene hot-water pipes. Polym Eng Sci. 37(5):1997;896-911.
    • (1997) Polym Eng Sci. , vol.37 , Issue.5 , pp. 896-911
    • Viebke, J.1    Gedde, U.W.2
  • 12
    • 0030399080 scopus 로고    scopus 로고
    • Antioxidant efficiency loss by precipitation and diffusion to surrounding media in polyethylene hot-water pipes
    • Viebke J., Hedenquist M., Gedde U.W. Antioxidant efficiency loss by precipitation and diffusion to surrounding media in polyethylene hot-water pipes. Polym Eng Sci. 36(24):1996;2896-2904.
    • (1996) Polym Eng Sci. , vol.36 , Issue.24 , pp. 2896-2904
    • Viebke, J.1    Hedenquist, M.2    Gedde, U.W.3
  • 13
    • 0021840199 scopus 로고
    • Radiometrische untersuchungen zur migration mehrkerniger phenolisher antioxidantien aus polypropylenprüfkörpern in lebensmittel
    • Lötzsch K., Eckert H.G., Kellner H.-M., Pfahler G. Radiometrische untersuchungen zur migration mehrkerniger phenolisher antioxidantien aus polypropylenprüfkörpern in lebensmittel. Fette, Seifen, Anstrichmittel. 87:1985;544-550.
    • (1985) Fette, Seifen, Anstrichmittel , vol.87 , pp. 544-550
    • Lötzsch, K.1    Eckert, H.G.2    Kellner, H.-M.3    Pfahler, G.4
  • 14
    • 0023965571 scopus 로고
    • Stabilization of polyolefins for applications in extractive media
    • Pfahler G., Lötzsch K. Stabilization of polyolefins for applications in extractive media. Kunststoffe. 78(2):1988;142-148.
    • (1988) Kunststoffe , vol.78 , Issue.2 , pp. 142-148
    • Pfahler, G.1    Lötzsch, K.2
  • 15
    • 84989040033 scopus 로고
    • Molecular structure, morphology, and antioxidant consumption in medium density polyethylene pipes in hot-water applications
    • Karlsson K., Smith G.D., Gedde U.W. Molecular structure, morphology, and antioxidant consumption in medium density polyethylene pipes in hot-water applications. Polym Eng Sci. 32(10):1992;649-657.
    • (1992) Polym Eng Sci. , vol.32 , Issue.10 , pp. 649-657
    • Karlsson, K.1    Smith, G.D.2    Gedde, U.W.3
  • 16
    • 0032303397 scopus 로고    scopus 로고
    • Influence of various stabilizer systems on the ageing behavior of PE-MD-II. Ageing of pipe specimens in air and water at elevated temperatures
    • Dörner G., Lang R.W. Influence of various stabilizer systems on the ageing behavior of PE-MD-II. Ageing of pipe specimens in air and water at elevated temperatures. Polym Degrad Stab. 62:1998;431-440.
    • (1998) Polym Degrad Stab , vol.62 , pp. 431-440
    • Dörner, G.1    Lang, R.W.2
  • 17
    • 0018491736 scopus 로고
    • Los of additives from polymers: A theoretical model
    • Calvert P.D., Billingham N.C. Los of additives from polymers. a theoretical model J Appl Polym Sci. 24:1979;357-370.
    • (1979) J Appl Polym Sci. , vol.24 , pp. 357-370
    • Calvert, P.D.1    Billingham, N.C.2
  • 18
    • 0032304697 scopus 로고    scopus 로고
    • Influence of various stabilizer systems on the ageing behavior of PE-MD-I. Hot-water ageing of compression molded plaques
    • Dörner G., Lang R.W. Influence of various stabilizer systems on the ageing behavior of PE-MD-I. Hot-water ageing of compression molded plaques. Polym Degrad Stab. 62:1998;421-430.
    • (1998) Polym Degrad Stab , vol.62 , pp. 421-430
    • Dörner, G.1    Lang, R.W.2
  • 19
    • 0141931682 scopus 로고    scopus 로고
    • Advanced extraction resistant long-term thermal stabilizers for polyolefin pipes
    • Houston, Texas, USA, February
    • Schmutz Th, Kramer E, Zweifel H, Dörner G. Advanced extraction resistant long-term thermal stabilizers for polyolefin pipes. In: Proceedings Polyolefins X Conference, Houston, Texas, USA, February. 1997. p. 371-89.
    • (1997) Proceedings Polyolefins X Conference , pp. 371-389
    • Schmutz, Th.1    Kramer, E.2    Zweifel, H.3    Dörner, G.4
  • 20
    • 0030085809 scopus 로고    scopus 로고
    • Degradation of polyolefin pipes in hot water applications: Simulation of the degradation process
    • Viebke J., Elble E., Gedde U.W. Degradation of polyolefin pipes in hot water applications. simulation of the degradation process Polym Eng Sci. 36(4):1996;458-466.
    • (1996) Polym Eng Sci. , vol.36 , Issue.4 , pp. 458-466
    • Viebke, J.1    Elble, E.2    Gedde, U.W.3
  • 21
    • 0024862094 scopus 로고
    • Degradation and stabilization of HDPE during multiple extrusions
    • Moss S., Zweifel H. Degradation and stabilization of HDPE during multiple extrusions. Polym Degrad Stab. 25:1989;217-245.
    • (1989) Polym Degrad Stab , vol.25 , pp. 217-245
    • Moss, S.1    Zweifel, H.2
  • 24
    • 0033098568 scopus 로고    scopus 로고
    • Chemical reactions during the processing of stabilized PE: 2. Structure/property correlations
    • Epacher E., Fekete E., Gahleitner M., Pukánszky B. Chemical reactions during the processing of stabilized PE: 2. Structure/property correlations. Polym Degrad Stab. 63:1999;499-507.
    • (1999) Polym Degrad Stab , vol.63 , pp. 499-507
    • Epacher, E.1    Fekete, E.2    Gahleitner, M.3    Pukánszky, B.4
  • 25
    • 0033342145 scopus 로고    scopus 로고
    • Two-step degradation of high-density polyethylene during multiple extrusion
    • Epacher E., Tolvéth J., Stoll K., Pukánszky B. Two-step degradation of high-density polyethylene during multiple extrusion. J Appl Polym Sci. 74:1999;1596-1605.
    • (1999) J Appl Polym Sci. , vol.74 , pp. 1596-1605
    • Epacher, E.1    Tolvéth, J.2    Stoll, K.3    Pukánszky, B.4
  • 27
    • 0019280903 scopus 로고
    • Transformations of phenolic antioxidants and the role of their products in the long-term properties of polyolefins
    • Pospisil J. Transformations of phenolic antioxidants and the role of their products in the long-term properties of polyolefins. Adv. Polym. Sci. 36:1980;69-133.
    • (1980) Adv. Polym. Sci. , vol.36 , pp. 69-133
    • Pospisil, J.1
  • 28
    • 0008480924 scopus 로고
    • Thermal degradation of polyethylene in a nitrogen atmosphere of low oxygen content IV. Structural changes occuring in different types of HDPE
    • Holmström A., Sörvik E.M. Thermal degradation of polyethylene in a nitrogen atmosphere of low oxygen content IV. Structural changes occuring in different types of HDPE. J Appl Polym Sci: Symp. 57:1976;33-53.
    • (1976) J Appl Polym Sci: Symp , vol.57 , pp. 33-53
    • Holmström, A.1    Sörvik, E.M.2
  • 29
    • 0027148715 scopus 로고
    • The thermal stability of HDPE blends during heat-processing and short-term photooxidation
    • Yongcheng Y. The thermal stability of HDPE blends during heat-processing and short-term photooxidation. Polym Degrad Stab. 39:1993;193-198.
    • (1993) Polym Degrad Stab , vol.39 , pp. 193-198
    • Yongcheng, Y.1
  • 30
    • 0343953456 scopus 로고    scopus 로고
    • Processing stability of high density polyethylene; Effect of adsorbed and dissolved oxygen
    • Epacher E., Tolvéth J., Kröhnke C., Pukánszky B. Processing stability of high density polyethylene; effect of adsorbed and dissolved oxygen. Polymer. 41:2000;8401-8408.
    • (2000) Polymer , vol.41 , pp. 8401-8408
    • Epacher, E.1    Tolvéth, J.2    Kröhnke, C.3    Pukánszky, B.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.