Volumn 18, Issue 5, 2003, Pages 385-394

Chemical alteration of tephra in the depositional environment: Theoretical stability modelling

Author keywords

Chemical stability; Durability; Gibbs free energy of hydration; Glass; Leaching; NBO; Non bridging oxygen; O ratio; Si; Tephra; Tephrochronology

Indexed keywords

CHEMICAL ALTERATION; DEPOSITIONAL ENVIRONMENT; DURABILITY; LEACHING; QUATERNARY; TEPHRA; TEPHROCHRONOLOGY;

EID: 0043270544     PISSN: 02678179     EISSN: None     Source Type: Journal    
DOI: 10.1002/jqs.760     Document Type: Article
Times cited : (58)

References (24)
  • 1
    • 0043154867 scopus 로고    scopus 로고
    • Obsidian hydration dating
    • Brothwell DR, Pollard AM (eds). Wiley: Chichester
    • Ambrose WR. 2001. Obsidian hydration dating. In Handbook of Archaeological Sciences, Brothwell DR, Pollard AM (eds). Wiley: Chichester; 81-92.
    • (2001) Handbook of Archaeological Sciences , pp. 81-92
    • Ambrose, W.R.1
  • 2
    • 0030176845 scopus 로고    scopus 로고
    • The aqueous corrosion of potash-lime-silica glass in the range 10-250°C
    • Cooper GI, Cox GA. 1996. The aqueous corrosion of potash-lime-silica glass in the range 10-250°C. Applied Geochemistry 11: 511-521.
    • (1996) Applied Geochemistry , vol.11 , pp. 511-521
    • Cooper, G.I.1    Cox, G.A.2
  • 4
    • 0027038252 scopus 로고
    • Geochemical stability of fine-grained silicic Holocene tephra in Iceland and Scotland
    • Dugmore AJ, Newton AJ, Sugden DE, Larsen G. 1992. Geochemical stability of fine-grained silicic Holocene tephra in Iceland and Scotland. Journal of Quaternary Science 7: 173-183.
    • (1992) Journal of Quaternary Science , vol.7 , pp. 173-183
    • Dugmore, A.J.1    Newton, A.J.2    Sugden, D.E.3    Larsen, G.4
  • 6
    • 0034017644 scopus 로고    scopus 로고
    • The tephrochronology of Iceland and the North Atlantic region during the Middle and Late Quaternary: A review
    • Haflidason H, Eiriksson J, van Kreveld S. 2000. The tephrochronology of Iceland and the North Atlantic region during the Middle and Late Quaternary: a review. Journal of Quaternary Science 15: 3-22.
    • (2000) Journal of Quaternary Science , vol.15 , pp. 3-22
    • Haflidason, H.1    Eiriksson, J.2    van Kreveld, S.3
  • 7
    • 84975636416 scopus 로고
    • Calculation of density and optical constants of a glass from its composition in weight percentage
    • Huggins ML, Sun K-H. 1943. Calculation of density and optical constants of a glass from its composition in weight percentage. Journal of the American Ceramic Society 26: 4-11.
    • (1943) Journal of the American Ceramic Society , vol.26 , pp. 4-11
    • Huggins, M.L.1    Sun, K.-H.2
  • 8
    • 84986407401 scopus 로고
    • Nuclear waste glass durability. 1. Predicting environmental response from thermodynamic (Pourbaix) diagrams
    • Jantzen CM. 1992. Nuclear waste glass durability. 1. Predicting environmental response from thermodynamic (Pourbaix) diagrams. Journal of the American Ceramic Society 75: 2435-2448.
    • (1992) Journal of the American Ceramic Society , vol.75 , pp. 2435-2448
    • Jantzen, C.M.1
  • 10
    • 0035448887 scopus 로고    scopus 로고
    • The effect of clay on the dissolution of nuclear waste glass
    • Lemmens K. 2001. The effect of clay on the dissolution of nuclear waste glass. Journal of Nuclear Materials 298: 11-18.
    • (2001) Journal of Nuclear Materials , vol.298 , pp. 11-18
    • Lemmens, K.1
  • 11
  • 12
    • 0034973661 scopus 로고    scopus 로고
    • Inter-regional correlation of palaeoclimatic records for the last Glacial-Interglacial transition: A protocol for improved precision recommended by the INTIMATE project group
    • Intimate Group
    • Lowe JJ, Hoek WZ, INTIMATE Group. 2001. Inter-regional correlation of palaeoclimatic records for the last Glacial-Interglacial transition: a protocol for improved precision recommended by the INTIMATE project group. Quaternary Science Reviews 20: 1175-1187.
    • (2001) Quaternary Science Reviews , vol.20 , pp. 1175-1187
    • Lowe, J.J.1    Hoek, W.Z.2
  • 14
    • 0022009338 scopus 로고
    • The durability of glass - A review
    • Newton RG. 1985. The durability of glass-a review. Glass Technology 26: 21-38.
    • (1985) Glass Technology , vol.26 , pp. 21-38
    • Newton, R.G.1
  • 15
    • 0035197743 scopus 로고    scopus 로고
    • The mechanism, rates and consequences of basaltic glass dissolution: 1. An experimental study of the dissolution rates of basaltic glass as a function of aqueous AI, Si and oxalic acid concentration at 25°C and pH = 3 and 11
    • Oelkers EH, Gislason SR. 2001. The mechanism, rates and consequences of basaltic glass dissolution: 1. An experimental study of the dissolution rates of basaltic glass as a function of aqueous AI, Si and oxalic acid concentration at 25°C and pH = 3 and 11. Geochimica et Cosmochimica Acta 65: 3671-3681.
    • (2001) Geochimica et Cosmochimica Acta , vol.65 , pp. 3671-3681
    • Oelkers, E.H.1    Gislason, S.R.2
  • 16
    • 0017559946 scopus 로고
    • Chemical durability of glasses; a thermodynamic approach
    • Paul A. 1977. Chemical durability of glasses; a thermodynamic approach. Journal of Materials Science 12: 2246-2268.
    • (1977) Journal of Materials Science , vol.12 , pp. 2246-2268
    • Paul, A.1
  • 21
    • 0041652026 scopus 로고
    • New light on the structure of glass
    • Stevels JM. 1960-61. New light on the structure of glass. Philips Technical Review 22: 300-311.
    • (1960) Philips Technical Review , vol.22 , pp. 300-311
    • Stevels, J.M.1
  • 22
    • 0034975594 scopus 로고    scopus 로고
    • Dissolution kinetics of basaltic glasses: Control by solution chemistry and protective effect of the alteration film
    • Techer I, Advocat T, Lancelot J, Liotard J-M. 2001. Dissolution kinetics of basaltic glasses: control by solution chemistry and protective effect of the alteration film. Chemical Geology 176: 235-263.
    • (2001) Chemical Geology , vol.176 , pp. 235-263
    • Techer, I.1    Advocat, T.2    Lancelot, J.3    Liotard, J.-M.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.