메뉴 건너뛰기




Volumn 220, Issue 1-2, 1996, Pages 176-184

SiCf/O′-SiAlON composite: Properties and oxidation retained properties

Author keywords

Interface; Oxidation; O SiAlON; SiC fiber reinforcement; Strength; Toughness; Work of fracture

Indexed keywords

BENDING STRENGTH; BONDING; FIBER REINFORCED MATERIALS; FRACTURE; HEAT TREATMENT; HIGH TEMPERATURE EFFECTS; HOT PRESSING; INTERFACES (MATERIALS); OXIDATION; PRESSURE EFFECTS; SHEAR STRENGTH; SILICON CARBIDE;

EID: 0041713884     PISSN: 09215093     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0921-5093(96)10477-9     Document Type: Article
Times cited : (6)

References (20)
  • 2
    • 85047673403 scopus 로고
    • Review-sialons and related nitrogen ceramics
    • K.H. Jack, Review-sialons and related nitrogen ceramics, J. Mater. Sci., 11 (1976) 1135-1158.
    • (1976) J. Mater. Sci. , vol.11 , pp. 1135-1158
    • Jack, K.H.1
  • 3
    • 0001214651 scopus 로고
    • Microstructure and fracture toughness of hot-pressed zirconia-toughened sialon
    • M.G. Cain and M.H. Lewis, Microstructure and fracture toughness of hot-pressed zirconia-toughened sialon, J. Am. Ceram. Soc., 76 (6) (1993) 1401-1408.
    • (1993) J. Am. Ceram. Soc. , vol.76 , Issue.6 , pp. 1401-1408
    • Cain, M.G.1    Lewis, M.H.2
  • 4
    • 0009072416 scopus 로고
    • Mechanical properties and microstructure of β-SiAlON-β-SiC composites by pressureless sintering
    • C. Yamagishi, K. Tsukamoto, J. Hakoshima, H. Shimojima and Y. Akiyama, Mechanical properties and microstructure of β-SiAlON-β-SiC composites by pressureless sintering, J. Mater. Sci., 27 (1992) 1908-1912.
    • (1992) J. Mater. Sci. , vol.27 , pp. 1908-1912
    • Yamagishi, C.1    Tsukamoto, K.2    Hakoshima, J.3    Shimojima, H.4    Akiyama, Y.5
  • 5
    • 84986335246 scopus 로고
    • SiC Whisker-reinforced sialon composites: Effect of sintering aid content
    • T. Tiegs, SiC Whisker-reinforced sialon composites: effect of sintering aid content, Ceram. Eng. Sci. Proc., 10 (9-10) (1989) 1101-1107.
    • (1989) Ceram. Eng. Sci. Proc. , vol.10 , Issue.9-10 , pp. 1101-1107
    • Tiegs, T.1
  • 6
    • 0025464999 scopus 로고
    • High-temperature strength of SiC whisker-sialon composites
    • Y. Akimune, High-temperature strength of SiC whisker-sialon composites, J. Mater. Sci. Lett., 9 (1990) 816-817.
    • (1990) J. Mater. Sci. Lett. , vol.9 , pp. 816-817
    • Akimune, Y.1
  • 7
    • 0028550101 scopus 로고
    • Combustion-synthesized β′-SiAlON reinforced with SiC monofilaments
    • C.M. Huang, Y. Xu, D. Zhu and W.M. Kriven, Combustion-synthesized β′-SiAlON reinforced with SiC monofilaments, Mater. Sci. Eng., A188 (1994) 341-351.
    • (1994) Mater. Sci. Eng. , vol.A188 , pp. 341-351
    • Huang, C.M.1    Xu, Y.2    Zhu, D.3    Kriven, W.M.4
  • 8
    • 0041618717 scopus 로고
    • Silicon oxynitride and Si-Al-O-N ceramics from organosilicon polymers
    • J.D. Mackenzie and D.R. Ulrich (eds.), Wiley, New York
    • Y.F. Yu and T.I. Mah, Silicon oxynitride and Si-Al-O-N ceramics from organosilicon polymers, in J.D. Mackenzie and D.R. Ulrich (eds.), Ultrastructure Processing of Advanced Ceramics, Wiley, New York, 1988, p. 773-781.
    • (1988) Ultrastructure Processing of Advanced Ceramics , pp. 773-781
    • Yu, Y.F.1    Mah, T.I.2
  • 9
    • 0021610434 scopus 로고
    • An indentation method for measuring matrix-fiber frictional stress in ceramic composites
    • D.B. Marshall, An indentation method for measuring matrix-fiber frictional stress in ceramic composites, J. Am. Ceram. Soc., 67 (12) (1984) C-259-C-260.
    • (1984) J. Am. Ceram. Soc. , vol.67 , Issue.12
    • Marshall, D.B.1
  • 10
    • 0023399385 scopus 로고
    • Measurement of interfacial mechanical properties in fiber-reinforced ceramic composites
    • D.B. Marshall and W.C. Oliver, Measurement of interfacial mechanical properties in fiber-reinforced ceramic composites, J. Am. Ceram. Soc., 70 (8) (1987) 542-548.
    • (1987) J. Am. Ceram. Soc. , vol.70 , Issue.8 , pp. 542-548
    • Marshall, D.B.1    Oliver, W.C.2
  • 11
    • 0024754722 scopus 로고
    • Interfacial bonding and friction in SiC (filament)-reinforced ceramic-and glass-matrix composites
    • J.D. Bright, D.K. Shetty, C.W. Griffin and S.Y. Limaye, Interfacial bonding and friction in SiC (filament)-reinforced ceramic-and glass-matrix composites, J. Am. Ceram. Soc., 72 (10) (1989) 1891-1898.
    • (1989) J. Am. Ceram. Soc. , vol.72 , Issue.10 , pp. 1891-1898
    • Bright, J.D.1    Shetty, D.K.2    Griffin, C.W.3    Limaye, S.Y.4
  • 12
    • 0029386589 scopus 로고
    • Interfacial properties of SiC monofilament reinforced β′-SiAlON composites
    • C.M. Huang, D. Zhu, Y. Xu, T. Mackin and W.M. Kriven, Interfacial properties of SiC monofilament reinforced β′-SiAlON composites, Mater. Sci. Eng., A201 (1995) 159-168.
    • (1995) Mater. Sci. Eng. , vol.A201 , pp. 159-168
    • Huang, C.M.1    Zhu, D.2    Xu, Y.3    Mackin, T.4    Kriven, W.M.5
  • 14
    • 0026074509 scopus 로고
    • Effect of interfacial roughness on the frictional stress measured using pushout tests
    • P.D. Jero, R.J. Kerans and T.A. Parthasarathy, Effect of interfacial roughness on the frictional stress measured using pushout tests, J. Am. Ceram. Soc., 74 (11) (1991) 2793-2801.
    • (1991) J. Am. Ceram. Soc. , vol.74 , Issue.11 , pp. 2793-2801
    • Jero, P.D.1    Kerans, R.J.2    Parthasarathy, T.A.3
  • 15
    • 0026239620 scopus 로고
    • The microstructure of SCS-6 SiC fiber
    • X.J. Ning and P. Pirouz, The microstructure of SCS-6 SiC fiber, J. Mater. Res., 6 (10) (1991) 2234-2248.
    • (1991) J. Mater. Res. , vol.6 , Issue.10 , pp. 2234-2248
    • Ning, X.J.1    Pirouz, P.2
  • 16
    • 0042620701 scopus 로고
    • Chemical considerations in carbon-fiber/oxide-matrix composites
    • K.L. Luthra and H.D. Park, Chemical considerations in carbon-fiber/oxide-matrix composites, J. Am. Ceram. Soc., 75 (7) (1992) 1889-1898.
    • (1992) J. Am. Ceram. Soc. , vol.75 , Issue.7 , pp. 1889-1898
    • Luthra, K.L.1    Park, H.D.2
  • 17
    • 0022152449 scopus 로고
    • The mechanics of matrix cracking in brittle-matrix fiber composites
    • D.B. Marshall, B.N. Cox and A.G. Evans, The mechanics of matrix cracking in brittle-matrix fiber composites, Acta Metall., 33 (11) (1985) 2013-2021.
    • (1985) Acta Metall. , vol.33 , Issue.11 , pp. 2013-2021
    • Marshall, D.B.1    Cox, B.N.2    Evans, A.G.3
  • 19
    • 0043121511 scopus 로고
    • Effect of oxidation on single-fiber pullout interfacial shear stresses in a silicon carbide-borosilicate glass system
    • M. Barsoum and I.C. Tung, Effect of oxidation on single-fiber pullout interfacial shear stresses in a silicon carbide-borosilicate glass system, J. Am. Seram. Soc., 74 (10) (1991) 2693-2696.
    • (1991) J. Am. Seram. Soc. , vol.74 , Issue.10 , pp. 2693-2696
    • Barsoum, M.1    Tung, I.C.2
  • 20
    • 84985100207 scopus 로고
    • 4 matrix composite
    • 4 matrix composite, J. Am. Ceram. Soc., 75 (2) (1992) 406-412.
    • (1992) J. Am. Ceram. Soc. , vol.75 , Issue.2 , pp. 406-412
    • Bhatt, R.T.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.