Volumn 89, Issue 3, 2003, Pages 329-334

Suppression of secondary ferrite formation by boron addition in high carbon steel wires

Author keywords

Delamination; Drawing; Free boron; High carbon steel wire; Pearlite; Secondary ferrite

Indexed keywords

BORON; COOLING; DELAMINATION; FERRITE; HEAT TREATMENT; MICROSTRUCTURE; WIRE;