Volumn 34 A, Issue 3, 2003, Pages 553-566
|
Hydride embrittlement and irradiation effects on the hoop mechanical properties of pressurized water reactor (PWR) and boiling-water reactor (BWR) ZIRCALOY cladding tubes: Part I. Hydride embrittlement in stress-relieved, annealed, and recrystallized ZIRCALOY at 20°C and 300°C
|
Author keywords
[No Author keywords available]
|
Indexed keywords
ANNEALING;
BOILING WATER REACTORS;
EMBRITTLEMENT;
FRACTURE MECHANICS;
IRRADIATION;
MECHANICAL PROPERTIES;
PRESSURIZED WATER REACTORS;
RECRYSTALLIZATION (METALLURGY);
SCANNING ELECTRON MICROSCOPY;
STRESSES;
TRANSMISSION ELECTRON MICROSCOPY;
X RAY DIFFRACTION ANALYSIS;
GAUGE LENGTH;
HYDRIDE EMBRITTLEMENT;
MECHANICAL MODELING;
ZIRCONIUM ALLOYS;
|
EID: 0037353796
PISSN: 10735623
EISSN: None
Source Type: Journal
DOI: 10.1007/s11661-003-0091-3 Document Type: Article |
Times cited : (58)
|
References (20)
|