2
-
-
0022080223
-
Transformation-toughened zirconia ceramics
-
E. P. Butler, "Transformation-Toughened Zirconia Ceramics," Mater. Sci. Technol., 1, 417 (1985).
-
(1985)
Mater. Sci. Technol.
, vol.1
, pp. 417
-
-
Butler, E.P.1
-
3
-
-
0022755218
-
Strength limitations of transformation-toughened zirconia alloys
-
M. V. Swain and L. R. F. Rose, "Strength Limitations of Transformation-Toughened Zirconia Alloys," J. Am. Ceram. Soc., 69 [7] 511-18 (1986).
-
(1986)
J. Am. Ceram. Soc.
, vol.69
, Issue.7
, pp. 511-518
-
-
Swain, M.V.1
Rose, L.R.F.2
-
4
-
-
0022768179
-
3 ceramics
-
3 Ceramics," J. Am. Ceram. Soc., 69 [8] 638-40 (1986).
-
(1986)
J. Am. Ceram. Soc.
, vol.69
, Issue.8
, pp. 638-640
-
-
Masaki, T.1
-
5
-
-
84985154160
-
Grain-size-dependent transformation behavior in polycrystalline tetragonal zirconia
-
P. F. Becher and M. V. Swain, "Grain-Size-Dependent Transformation Behavior in Polycrystalline Tetragonal Zirconia," J. Am. Ceram. Soc., 75 [3] 493-502 (1992).
-
(1992)
J. Am. Ceram. Soc.
, vol.75
, Issue.3
, pp. 493-502
-
-
Becher, P.F.1
Swain, M.V.2
-
7
-
-
0033313270
-
The effect of copper oxide on sintering, microstructure, mechanical properties and hydrothermal ageing of coated 2.5Y-TZP ceramics
-
S. Ramesh, C. Gill, and S. Lawson, "The Effect of Copper Oxide on Sintering, Microstructure, Mechanical Properties and Hydrothermal Ageing of Coated 2.5Y-TZP Ceramics," J. Mater. Sci., 34, 5457-67 (1999).
-
(1999)
J. Mater. Sci.
, vol.34
, pp. 5457-5467
-
-
Ramesh, S.1
Gill, C.2
Lawson, S.3
-
9
-
-
0024016154
-
Evaluation of fracture toughness for ceramic materials by a single-edge-precracked-beam method
-
T. Nose and T. Fujii, "Evaluation of Fracture Toughness for Ceramic Materials by a Single-Edge-Precracked-Beam Method," J. Am. Ceram. Soc., 71 [5] 328-33 (1988).
-
(1988)
J. Am. Ceram. Soc.
, vol.71
, Issue.5
, pp. 328-333
-
-
Nose, T.1
Fujii, T.2
-
10
-
-
0020141691
-
Measurement of the crystallographically transformed zone produced by fracture in ceramics containing tetragonal zirconia
-
D. R. Clarke and F. Adar, "Measurement of the Crystallographically Transformed Zone Produced by Fracture in Ceramics Containing Tetragonal Zirconia," J. Am. Ceram. Soc., 65 [6] 284-88 (1982).
-
(1982)
J. Am. Ceram. Soc.
, vol.65
, Issue.6
, pp. 284-288
-
-
Clarke, D.R.1
Adar, F.2
-
13
-
-
0024866786
-
Evaluation of fracture toughness and R-curve behavior of Y-TZP ceramics
-
T. R. Lai, C. L. Hogg, and M. V. Swai, "Evaluation of Fracture Toughness and R-Curve Behavior of Y-TZP Ceramics," ISIJ Int., 29 [3] 240-45 (1989).
-
(1989)
ISIJ Int.
, vol.29
, Issue.3
, pp. 240-245
-
-
Lai, T.R.1
Hogg, C.L.2
Swai, M.V.3
-
14
-
-
0021636354
-
3-stabilized tetragonal zirconia polycrystals
-
Edited by N. Clausen, M. Ruhle, and A. H. Heuer. The American Ceramic Society, Westerville, OH
-
3-Stabilized Tetragonal Zirconia Polycrystals"; pp. 382-90 in Advances in Ceramics, Vol. 12, Science and Technology of Zirconia III. Edited by N. Clausen, M. Ruhle, and A. H. Heuer. The American Ceramic Society, Westerville, OH, 1984.
-
(1984)
Advances in Ceramics, Vol. 12, Science and Technology of Zirconia III
, pp. 382-390
-
-
Tsukuma, K.1
Kubota, Y.2
Tsukidate, T.3
-
15
-
-
0028194740
-
2: Implications to solid electrolytes and cermets
-
2: Implications to Solid Electrolytes and Cermets," Mater. Sci. Eng. B, B22, 247-255 (1994).
-
(1994)
Mater. Sci. Eng. B
, vol.B22
, pp. 247-255
-
-
Chen, S.1
Deng, W.2
Shen, P.3
-
16
-
-
84944648082
-
Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenides
-
R. D. Shannon, "Revised Effective Ionic Radii and Systematic Studies of Interatomic Distances in Halides and Chalcogenides," Acta Crystallogr., Sect. A, A32, 751 (1976).
-
(1976)
Acta Crystallogr., Sect. A
, vol.A32
, pp. 751
-
-
Shannon, R.D.1
-
17
-
-
0022145432
-
2 containing ceramics and ferrous alloys
-
2 Containing Ceramics and Ferrous Alloys," Acta Metall., 33, 1827-45, (1995).
-
(1985)
Acta Metall.
, vol.33
, pp. 1827-1845
-
-
Chen, I.W.1
Chiao, Y.-H.2
|