Mechanical, thermal and microstructure evaluation of HDPE after weathering in Rio de Janeiro City

Author keywords

High density polyethylene; Microstructure; Outdoor weathering; Oxidation; Thermal and mechanical properties

Indexed keywords

ADDITIVES; BAND STRUCTURE; FOURIER TRANSFORM INFRARED SPECTROSCOPY; MICROSTRUCTURE; OXIDATION; WEATHERING;

EID: 0037230819     PISSN: 01413910     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0141-3910(02)00337-3     Document Type: Article
Times cited : (81)

References (27)
  • 1
    • 0012552697 scopus 로고
    • Weathering
    • H.M. Mark, N.M. Bikales, C.G. Overberger, & G. Menges. New York: John Wiley
    • Searle N.D. Weathering. Mark H.M., Bikales N.M., Overberger C.G., Menges G. Encyclopedia of polymer science and engineering, vol.17. 1989;796-827 John Wiley, New York.
    • (1989) Encyclopedia of Polymer Science and Engineering , vol.17 , pp. 796-827
    • Searle, N.D.1
  • 6
    • 33845201198 scopus 로고    scopus 로고
    • Comparison of UV degradation of polyethylene in accelerated test and sunlight
    • R.L. Clough, N.C. Billingham, & K.T. Gillen. Polymer durability: Degradation, stabilisation and lifetime prediction, Washington: American Chemical Society
    • Gijsman P., Hennekens J., Janssen K. Comparison of UV degradation of polyethylene in accelerated test and sunlight. Clough R.L., Billingham N.C., Gillen K.T. Polymer durability: degradation, stabilisation and lifetime prediction, Advances in Chemistry Series 249. 1996;621-636 American Chemical Society, Washington.
    • (1996) Advances in Chemistry Series , vol.249 , pp. 621-636
    • Gijsman, P.1    Hennekens, J.2    Janssen, K.3
  • 14
    • 33845197823 scopus 로고    scopus 로고
    • Degradation profiles of thick high density polyethylene samples after outdoor and artificial weathering
    • R.L. Clough, N.C. Billingham, & K.T. Gillen.Polymer durability: Degradation, stabilisation and lifetime prediction, Washington: American Chemical Society
    • Bruijn J.C.M. Degradation profiles of thick high density polyethylene samples after outdoor and artificial weathering. Clough R.L., Billingham N.C., Gillen K.T. Polymer durability: degradation, stabilisation and lifetime prediction, Advances in Chemistry Series 249. 1996;599 American Chemical Society, Washington.
    • (1996) Advances in Chemistry Series , vol.249 , pp. 599
    • Bruijn, J.C.M.1
  • 21
    • 0003000366 scopus 로고    scopus 로고
    • Physical constants of polyethylene
    • J. Brandup, E. Immergut, & E. Grulke. New York: John Wiley
    • Zhu L., Chiu F., Fu Q., Quirk R., Cheng S. Physical constants of polyethylene. Brandup J., Immergut E., Grulke E. Polymer handbook. 1999;John Wiley, New York. p. V-9.
    • (1999) Polymer Handbook , pp. V9
    • Zhu, L.1    Chiu, F.2    Fu, Q.3    Quirk, R.4    Cheng, S.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.