메뉴 건너뛰기




Volumn 29, Issue 1, 2003, Pages 19-25

Properties and microstructure of machinable Al2O3/LaPO4 ceramic composites

Author keywords

B. Microstructure; C. Hardness; D. Al2O3

Indexed keywords

ALUMINA; INTERFACES (MATERIALS); LANTHANUM COMPOUNDS; METALLOGRAPHIC MICROSTRUCTURE; X RAY DIFFRACTION ANALYSIS;

EID: 0037230221     PISSN: 02728842     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0272-8842(02)00083-4     Document Type: Article
Times cited : (58)

References (11)
  • 1
    • 84979340076 scopus 로고
    • Machinable glass-ceramics based on tetrasilicic mica
    • Grossman D.G. Machinable glass-ceramics based on tetrasilicic mica. J. Am. Ceram. Soc. 55(9):1972;446-449.
    • (1972) J. Am. Ceram. Soc. , vol.55 , Issue.9 , pp. 446-449
    • Grossman, D.G.1
  • 3
    • 0029172160 scopus 로고
    • Enhanced machinability of silicon carbide via microstructural design
    • Padture N.P., Evans C.J., Xu H.H.K.et al. Enhanced machinability of silicon carbide via microstructural design. J. Am. Ceram. Soc. 78(1):1995;215-217.
    • (1995) J. Am. Ceram. Soc. , vol.78 , Issue.1 , pp. 215-217
    • Padture, N.P.1    Evans, C.J.2    Xu, H.H.K.3
  • 4
    • 0032208691 scopus 로고    scopus 로고
    • Machinability of high-strength porous silicon nitride ceramic
    • Chihiro Kawai AkiraYamakawa Machinability of high-strength porous silicon nitride ceramic. J. Ceram. Soc. Jap. 106(11):1998;1135-1137.
    • (1998) J. Ceram. Soc. Jap. , vol.106 , Issue.11 , pp. 1135-1137
    • Kawai, A.Y.C.1
  • 5
    • 0029254292 scopus 로고
    • Scratching and grinding of a machinable glass-ceramic with weak interfaces and rising T-curve
    • Xu Hockin H.K., Said J. Scratching and grinding of a machinable glass-ceramic with weak interfaces and rising T-curve. J. Am. Ceram. Soc. 78(2):1995;497-500.
    • (1995) J. Am. Ceram. Soc. , vol.78 , Issue.2 , pp. 497-500
    • Xu Hockin, H.K.1    Said, J.2
  • 6
    • 24044460227 scopus 로고    scopus 로고
    • Machinable ceramics and its graded design
    • Pan W., Wang R.G. Machinable ceramics and its graded design. Rare Metal Mater. Eng. 29(Suppl.):2000;84-88.
    • (2000) Rare Metal Mater. Eng. , vol.29 , Issue.SUPPL. , pp. 84-88
    • Pan, W.1    Wang, R.G.2
  • 7
    • 0031926334 scopus 로고    scopus 로고
    • 4 monazite and beta-alumina on alumina fibers for ceramic matrix composites
    • 4 monazite and beta-alumina on alumina fibers for ceramic matrix composites. Mater. Sci. Eng. A. 244(1):1998;91-96.
    • (1998) Mater. Sci. Eng. A , vol.244 , Issue.1 , pp. 91-96
    • Hwang, T.J.1    Hendrick, M.R.2
  • 8
    • 0032139481 scopus 로고    scopus 로고
    • Machinable ceramics containing rare-earth phosphates
    • Davis J.B., Marshall D.B. Machinable ceramics containing rare-earth phosphates. J. Am. Ceram. Soc. 81(8):1998;2169-2175.
    • (1998) J. Am. Ceram. Soc. , vol.81 , Issue.8 , pp. 2169-2175
    • Davis, J.B.1    Marshall, D.B.2
  • 10
    • 0031084105 scopus 로고    scopus 로고
    • Layered machinable ceramics for high temperature applications
    • Barsoum M.W. Layered machinable ceramics for high temperature applications. Scripta Mater. 36(5):1997;535-541.
    • (1997) Scripta Mater. , vol.36 , Issue.5 , pp. 535-541
    • Barsoum, M.W.1
  • 11
    • 0001359652 scopus 로고    scopus 로고
    • Indentation fatigue in random and textured alumina composites
    • Linan An Indentation fatigue in random and textured alumina composites. J. Am. Ceram. Soc. 82(1):1999;78-82.
    • (1999) J. Am. Ceram. Soc. , vol.82 , Issue.1 , pp. 78-82
    • Linan, A.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.