Performance study of cementitious systems containing zeolite and silica fume: Effects of four metal nitrates on the setting time, strength and leaching characteristics
|
Author keywords
Acid neutralisation capacity; Metal contaminants; Silica fume; Solidification; Zeolite
|
Indexed keywords
CHROMIUM;
IMPURITIES;
LEACHING;
PH EFFECTS;
SILICA;
SOLUBILITY;
STRENGTH OF MATERIALS;
WASTES;
ZEOLITES;
CEMENTITIOUS SYSTEMS;
PORTLAND CEMENT;
CEMENT;
CHROMIUM;
LEAD;
MANGANESE;
NITRATE;
SILICON DIOXIDE;
ZEOLITE;
ZINC;
LEACHING;
METAL;
NITRATE;
SETTLING;
SILICON DIOXIDE;
SOLIDIFICATION;
ZEOLITE;
ARTICLE;
CHEMICAL COMPOSITION;
COMPRESSIVE STRENGTH;
FUME;
HUMIDITY;
LEACHING;
MEASUREMENT;
MONITORING;
PH;
SOLUBILITY;
TEMPERATURE;
COMPRESSIVE STRENGTH;
ENVIRONMENTAL POLLUTANTS;
MANUFACTURED MATERIALS;
METALS, HEAVY;
SILICON DIOXIDE;
SOLUBILITY;
ZEOLITES;
|
EID: 0037158319
PISSN: 03043894
EISSN: None
Source Type: Journal
DOI: 10.1016/S0304-3894(02)00005-5 Document Type: Article |
Times cited : (49)
|
References (27)
|