메뉴 건너뛰기




Volumn 85, Issue 10, 2002, Pages 2507-2514

Effect of enameling on the strength and dynamic fatigue of soda-lime-silica float glass

Author keywords

[No Author keywords available]

Indexed keywords

FLOAT GLASS;

EID: 0036806412     PISSN: 00027820     EISSN: None     Source Type: Journal    
DOI: 10.1111/j.1151-2916.2002.tb00488.x     Document Type: Article
Times cited : (19)

References (28)
  • 1
    • 0001084701 scopus 로고
    • Glazes and enamels
    • Engineered Materials Handbook, Edited by S.J. Schneider Jr., S.R. Lampman, M.S. Woods, and T.B. Zorc. ASM International, Materials Park, OH
    • R.A. Eppler and L.D. Gill, "Glazes and Enamels"; pp. 1061-68 in Engineered Materials Handbook, Vol. 4, Ceramics and Glasses. Edited by S.J. Schneider Jr., S.R. Lampman, M.S. Woods, and T.B. Zorc. ASM International, Materials Park, OH, 1991.
    • (1991) Ceramics and Glasses , vol.4 , pp. 1061-1068
    • Eppler, R.A.1    Gill, L.D.2
  • 2
    • 0011182922 scopus 로고    scopus 로고
    • private communication
    • G.E. Sakoske; private communication, 1999.
    • (1999)
    • Sakoske, G.E.1
  • 4
    • 0000803183 scopus 로고    scopus 로고
    • Glass-tin interactions during the float glass forming process
    • Ceramic Transactions, Edited by A.G. Clare and L.E. Jones. American Ceramic Society, Westerville, OH
    • A. Mishra, G.A. Pecoraro, T.E. Paulson, and C.G. Pantano, "Glass-Tin Interactions During the Float Glass Forming Process"; pp. 205-17 in Ceramic Transactions, Vol. 82, Advances in Fusion and Processing of Glass II. Edited by A.G. Clare and L.E. Jones. American Ceramic Society, Westerville, OH, 1998.
    • (1998) Advances in Fusion and Processing of Glass II , vol.82 , pp. 205-217
    • Mishra, A.1    Pecoraro, G.A.2    Paulson, T.E.3    Pantano, C.G.4
  • 6
    • 0016622033 scopus 로고
    • Chemical characteristics of float glass surfaces
    • J.S. Sieger, "Chemical Characteristics of Float Glass Surfaces," J. Non-Cryst. Solids, 19, 213-20 (1975).
    • (1975) J. Non-Cryst. Solids , vol.19 , pp. 213-220
    • Sieger, J.S.1
  • 7
    • 0033170340 scopus 로고    scopus 로고
    • The effects of tin on some physical properties of the bottom surface of float glass and the origin of bloom
    • K.F.E. Williams and M.F. Thomas, "The Effects of Tin on Some Physical Properties of the Bottom Surface of Float Glass and the Origin of Bloom," Glass Technol., 40 [4] 103-107 (1999).
    • (1999) Glass Technol. , vol.40 , Issue.4 , pp. 103-107
    • Williams, K.F.E.1    Thomas, M.F.2
  • 8
    • 0029277408 scopus 로고
    • Surface chemistry of commercial float glass
    • H. Franz, "Surface Chemistry of Commercial Float Glass," Ceram. Eng. Sci. Proc., 16 [2] 251-58 (1995).
    • (1995) Ceram. Eng. Sci. Proc. , vol.16 , Issue.2 , pp. 251-258
    • Franz, H.1
  • 10
    • 0000962577 scopus 로고
    • Tin profiles in the bottom surface of float glass: Manufacturing and heat treatment effects
    • Proceedings of the Second Conference of the European Society of Glass Science and Technology (Venice, Italy, June 21-24). Stazione Sperimentale del Vetro, Venice, Italy, 1993.
    • C.G. Pantano and V.J. Bojan, "Tin Profiles in the Bottom Surface of Float Glass: Manufacturing and Heat Treatment Effects"; in Fundamentals of Glass Science and Technology, 1993, Proceedings of the Second Conference of the European Society of Glass Science and Technology (Venice, Italy, June 21-24, 1993). Stazione Sperimentale del Vetro, Venice, Italy, 1993.
    • (1993) Fundamentals of Glass Science and Technology, 1993
    • Pantano, C.G.1    Bojan, V.J.2
  • 11
    • 0011230427 scopus 로고    scopus 로고
    • Property's difference of upper and lower surface of float glass
    • San Francisco, CA. American Ceramic Society, Westerville, OH
    • L. Fu, Z. Liu, and M. Xie, "Property's Difference of Upper and Lower Surface of Float Glass"; in Proceedings of the XVIII International Congress on Glass (San Francisco, CA). American Ceramic Society, Westerville, OH, 1998.
    • (1998) Proceedings of the XVIII International Congress on Glass
    • Fu, L.1    Liu, Z.2    Xie, M.3
  • 13
    • 0002697756 scopus 로고    scopus 로고
    • Effects of tin on the bottom surface of float glass
    • V.F. Solinov and T.V. Kaplina, "Effects of Tin on the Bottom Surface of Float Glass," Glass Ceram., 54 [3-4] 73-76 (1997).
    • (1997) Glass Ceram. , vol.54 , Issue.3-4 , pp. 73-76
    • Solinov, V.F.1    Kaplina, T.V.2
  • 19
    • 0000970144 scopus 로고
    • A method for determining the strength of sheet glass
    • F.F. Vitman and V.P. Pukh, "A Method for Determining the Strength of Sheet Glass," Zavod. Lab., 29, 863 (1963).
    • (1963) Zavod. Lab. , vol.29 , pp. 863
    • Vitman, F.F.1    Pukh, V.P.2
  • 20
    • 84987266075 scopus 로고
    • A statistical distribution function of wide applicability
    • W. Weibull, "A Statistical Distribution Function of Wide Applicability," J. Appl. Mech., 18, 293 (1951).
    • (1951) J. Appl. Mech. , vol.18 , pp. 293
    • Weibull, W.1
  • 22
    • 36849126545 scopus 로고
    • Dynamic fatigue of glass
    • R.J. Charles, "Dynamic Fatigue of Glass," J. Appl. Phys., 29 [12] 1657-62 (1958).
    • (1958) J. Appl. Phys. , vol.29 , Issue.12 , pp. 1657-1662
    • Charles, R.J.1
  • 23
    • 0016071137 scopus 로고
    • Slow crack growth in brittle materials under dynamic loading conditions
    • A.G. Evans, "Slow Crack Growth in Brittle Materials Under Dynamic Loading Conditions," Int. J. Fract., 10 [2] 251-59 (1974).
    • (1974) Int. J. Fract. , vol.10 , Issue.2 , pp. 251-259
    • Evans, A.G.1
  • 24
    • 0020751114 scopus 로고
    • Theory of fatigue for brittle flaws originating from residual stress concentrations
    • E.R. Fuller, B.R. Lawn, and R.F. Cook, "Theory of Fatigue for Brittle Flaws Originating from Residual Stress Concentrations," J. Am. Ceram. Soc., 66 [5] 314-21 (1983).
    • (1983) J. Am. Ceram. Soc. , vol.66 , Issue.5 , pp. 314-321
    • Fuller, E.R.1    Lawn, B.R.2    Cook, R.F.3
  • 25
    • 0019623492 scopus 로고
    • Fatigue analysis of brittle materials using indentation flaws: Part 1 general theory
    • B.R. Lawn, D.B. Marshall, G.R. Anstis, and T.P. Dabbs, "Fatigue Analysis of Brittle Materials Using Indentation Flaws: Part 1 General Theory," J. Mater. Sci., 16 [10] 2846-54 (1981).
    • (1981) J. Mater. Sci. , vol.16 , Issue.10 , pp. 2846-2854
    • Lawn, B.R.1    Marshall, D.B.2    Anstis, G.R.3    Dabbs, T.P.4
  • 26
    • 0016482865 scopus 로고
    • Strength and dynamic fatigue of float glass surfaces
    • R. Tummala and B. Foster, "Strength and Dynamic Fatigue of Float Glass Surfaces," J. Am. Ceram. Soc., 58 [3-4] 156-57 (1975).
    • (1975) J. Am. Ceram. Soc. , vol.58 , Issue.3-4 , pp. 156-157
    • Tummala, R.1    Foster, B.2
  • 27
    • 0017972058 scopus 로고
    • Dynamic fatigue of float glass
    • H. Chandan, R. Bradt, and G. Rindone, "Dynamic Fatigue of Float Glass," J. Am. Ceram. Soc., 61 [5-6] 207-10 (1978).
    • (1978) J. Am. Ceram. Soc. , vol.61 , Issue.5-6 , pp. 207-210
    • Chandan, H.1    Bradt, R.2    Rindone, G.3
  • 28
    • 0001412634 scopus 로고
    • Determination of subcritical crack growth parameters by in situ observation of indentation cracks
    • P.J. Dwivedi and D.J. Green, "Determination of Subcritical Crack Growth Parameters by In Situ Observation of Indentation Cracks," J. Am. Ceram. Soc., 78 [8] 2122-28 (1983).
    • (1983) J. Am. Ceram. Soc. , vol.78 , Issue.8 , pp. 2122-2128
    • Dwivedi, P.J.1    Green, D.J.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.