Volumn 49, Issue 9, 2002, Pages 787-792

Influence of boron addition on the tensile properties of sintered FeAl compacts by powder injection molding

Author keywords

B; FeAl; Powder injection molding; Sintering temperature; Tensile property

Indexed keywords

BORON; INJECTION MOLDING; POWDER METALS; SINTERING; TENSILE STRENGTH; THERMAL EFFECTS;

EID: 0036762788     PISSN: 05328799     EISSN: None     Source Type: Journal    
DOI: 10.2497/jjspm.49.787     Document Type: Article
Times cited : (9)

References (12)
  • 1
    • 0000413782 scopus 로고
    • The effect of temperature and Fe:Al ratio on the flow and fracture of FeAl
    • I. Baker, H. Xiao, O. Klein, C. Neison and J.D. Whittenberger: "The Effect of Temperature and Fe:Al Ratio on The Flow and Fracture of FeAl", Acta matall. mater., 43(1995)1723-1730.
    • (1995) Acta matall. mater. , vol.43 , pp. 1723-1730
    • Baker, I.1    Xiao, H.2    Klein, O.3    Neison, C.4    Whittenberger, J.D.5
  • 2
    • 85036823387 scopus 로고    scopus 로고
    • Japanese source
  • 3
    • 0025461964 scopus 로고
    • Environmental embrittlement in boron-free and boron-doped FeAl (40at%Al) alloys
    • C.T. Liu and E.P. George: "Environmental Embrittlement in Boron-Free and Boron-Doped FeAl (40at%Al) Alloys", Scripta Metall. et Mater., 24(1990)1285-1290.
    • (1990) Scripta Metall. et Mater. , vol.24 , pp. 1285-1290
    • Liu, C.T.1    George, E.P.2
  • 5
    • 0004676661 scopus 로고    scopus 로고
    • Sintering and mechanical properties of a boron-doped austenitic stainless steel
    • R. Tandon and R.M. German: "Sintering and Mechanical properties of A Boron-doped Austenitic stainless Steel", The Intern. J. Powder Met., 34(1) (1998)40-49.
    • (1998) The Intern. J. Powder Met. , vol.34 , Issue.1 , pp. 40-49
    • Tandon, R.1    German, R.M.2
  • 6
    • 85036802415 scopus 로고    scopus 로고
    • Japanese source
  • 7
    • 85036848127 scopus 로고    scopus 로고
    • Japanese source
  • 8
    • 85036806812 scopus 로고    scopus 로고
    • Japanese source
  • 9
    • 0030212853 scopus 로고    scopus 로고
    • Tesile properties of cast and mechanical alloyed FeAl with high boron content
    • M.H. Kim and S.I. Kwun: "Tesile Properties of Cast and Mechanical Alloyed FeAl with High Boron Content", Scripta Mater., 35(1996)317-322.
    • (1996) Scripta Mater. , vol.35 , pp. 317-322
    • Kim, M.H.1    Kwun, S.I.2
  • 11
    • 85036826417 scopus 로고    scopus 로고
    • Japanese source
  • 12
    • 0012028167 scopus 로고
    • Optimization of the boron content in FeAl (40at.%Al) alloys
    • G. Webb, P. Juliet and A. Lefort: "Optimization of The Boron Content in FeAl (40at.%Al) Alloys", Scripta Metall. et Mater., 28(1993)769-772.
    • (1993) Scripta Metall. et Mater. , vol.28 , pp. 769-772
    • Webb, G.1    Juliet, P.2    Lefort, A.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.