Composed phases and microhardness of aluminium-rich aluminium-iron alloys obtained by rapid quenching, mechanical alloying and high pressure torsion deformation
a a a a a a a a |
Author keywords
Aluminium iron alloys; High pressure torsion; Mechanical alloying; Microhardness; Rapid quenching; Solid solution
|