Creep damage development of a 1.25Cr-0.5Mo steel weldment exposed to long term service
a a a |
Author keywords
1.25Cr 0.5Mo steel; Creep; Creep life assessment; Type IV cracking; Weldment
|
Indexed keywords
BRITTLENESS;
CRACK PROPAGATION;
CREEP TESTING;
DUCTILITY;
FAILURE (MECHANICAL);
GRANULAR MATERIALS;
HIGH TEMPERATURE OPERATIONS;
SERVICE LIFE;
WELDS;
CREEP DAMAGE DEVELOPMENT;
CREEP LIFE;
DUCTILE TRANSGRANULAR RUPTURE;
STEEL WELDMENT;
ULTIMATE FAILURE MODE;