Volumn 189, Issue 1-4, 2002, Pages 350-357
|
Use of PIXE-PIGE under variable incident angle for ancient glass corrosion measurements
|
Author keywords
Archaeometry; Corrosion; Glass artifact; PIXE
|
Indexed keywords
ABSORPTION;
CORROSION PREVENTION;
DEGRADATION;
GLASS;
ION BEAMS;
NONDESTRUCTIVE EXAMINATION;
X RAY ANALYSIS;
ARCHAEOMETRY;
GLASS CORROSION MEASUREMENTS;
NUCLEAR PHYSICS;
|
EID: 0036534543
PISSN: 0168583X
EISSN: None
Source Type: Journal
DOI: 10.1016/S0168-583X(01)01085-0 Document Type: Conference Paper |
Times cited : (31)
|
References (10)
|