메뉴 건너뛰기




Volumn 4639, Issue , 2002, Pages 30-39

Bending strength and fractographic analysis of zinc tellurite glass modified optical fibres

Author keywords

Bending strength; Fracture toughness; Microhardness; Mirror constant; Tellurite fibres

Indexed keywords

BARIUM COMPOUNDS; BENDING STRENGTH; CLADDING (COATING); ELASTIC MODULI; FRACTALS; FRACTOGRAPHY; FRACTURE TOUGHNESS; GLASS FIBERS; INDENTATION; MICROHARDNESS; MIRRORS; MULTIMODE FIBERS; SCANNING ELECTRON MICROSCOPY; ZINC COMPOUNDS;

EID: 0036381277     PISSN: 0277786X     EISSN: None     Source Type: Journal    
DOI: 10.1117/12.481341     Document Type: Article
Times cited : (5)

References (38)
  • 1
    • 0028479992 scopus 로고
    • Tellurite glass: A new candidate for fiber devices
    • J.S. Wang, E.M. Vogel, and E. Snitzer, "Tellurite glass: a new candidate for fiber devices, " Opt. Mater. 3, pp. 187-203, 1994.
    • (1994) Opt. Mater. , vol.3 , pp. 187-203
    • Wang, J.S.1    Vogel, E.M.2    Snitzer, E.3
  • 4
    • 0000694012 scopus 로고    scopus 로고
    • 3+-doped tellurite glass for a broadband amplifier at 1.47 μm
    • 3+-doped tellurite glass for a broadband amplifier at 1.47 μm, " Appl. Opt. 39, pp. 4979-4984, 2000.
    • (2000) Appl. Opt. , vol.39 , pp. 4979-4984
    • Naftaly, M.1    Shen, S.2    Jha, A.3
  • 5
    • 0034932212 scopus 로고    scopus 로고
    • 3+-doped tellurite glasses for 1.4 μm amplifier
    • 3+-doped tellurite glasses for 1.4 μm amplifier, " Proc. SPIE 4282, pp. 85-92, 2001.
    • (2001) Proc. SPIE , vol.4282 , pp. 85-92
    • Tanabe, S.1
  • 8
    • 0035337766 scopus 로고    scopus 로고
    • NMR studies of aluminum speciation in tellurite glasses
    • R.E. Youngman and B.G. Aitken, "NMR studies of aluminum speciation in tellurite glasses, " J. Non-Cryst. Solids 284, pp. 9-15, 2001.
    • (2001) J. Non-Cryst. Solids , vol.284 , pp. 9-15
    • Youngman, R.E.1    Aitken, B.G.2
  • 10
    • 0344671561 scopus 로고    scopus 로고
    • Studies on telluilte glasses using differential thermal analysis
    • E.B. Araújo, J.A. Eiras, and A.C. Hernandes, "Studies on telluilte glasses using differential thermal analysis, " J. Mater. Sci. Lett. 18, pp. 793-795, 1999.
    • (1999) J. Mater. Sci. Lett. , vol.18 , pp. 793-795
    • Araújo, E.B.1    Eiras, J.A.2    Hernandes, A.C.3
  • 11
    • 0031373191 scopus 로고    scopus 로고
    • Broadband amplification characteristics of tellurite-based EDFAs
    • A. Mori, Y. Ohishi, M. Yamada, H. Ono, and S. Sudo, "Broadband amplification characteristics of tellurite-based EDFAs, " Proc. ECOC' 97, pp. 135-138, 1997.
    • (1997) Proc. ECOC' 97 , pp. 135-138
    • Mori, A.1    Ohishi, Y.2    Yamada, M.3    Ono, H.4    Sudo, S.5
  • 13
    • 0000253191 scopus 로고    scopus 로고
    • A 50 nm broadband tellurite-based EDFA with 0.6 dB gain excursion and a 25.3 dB gain for 1.58 μm-band WDM signals
    • A. Mori, T. Sakamoto, K. Kobayashi, K. Shikano, K. Oikawa, K. Hoshino, T. Kanamori, and M. Shimizu, "A 50 nm broadband tellurite-based EDFA with 0.6 dB gain excursion and a 25.3 dB gain for 1.58 μm-band WDM signals, " Proc. ECOC '99, pp. 268-269, 1999.
    • (1999) Proc. ECOC '99 , pp. 268-269
    • Mori, A.1    Sakamoto, T.2    Kobayashi, K.3    Shikano, K.4    Oikawa, K.5    Hoshino, K.6    Kanamori, T.7    Shimizu, M.8
  • 15
    • 0035336215 scopus 로고    scopus 로고
    • Thermoplastic polyetherimide - A helpful aid for the drawing of fluoride fibres
    • J. Kraus, C. Bruschi, and E. Billi, "Thermoplastic polyetherimide - a helpful aid for the drawing of fluoride fibres, " J. Non-Cryst. Solids 284, pp. 139-145, 2001.
    • (2001) J. Non-Cryst. Solids , vol.284 , pp. 139-145
    • Kraus, J.1    Bruschi, C.2    Billi, E.3
  • 18
    • 0002196482 scopus 로고
    • Direct calculation of Young's modulus of glass
    • A. Makishima and J.D. Mackenzie, "Direct calculation of Young's modulus of glass, " J. Non-Cryst. Solids 12, pp. 35-45, 1973.
    • (1973) J. Non-Cryst. Solids , vol.12 , pp. 35-45
    • Makishima, A.1    Mackenzie, J.D.2
  • 19
    • 0033314509 scopus 로고    scopus 로고
    • Young's modulus and compositional parameters of oxide glasses
    • S. Inaba, S. Fujino, and K. Morinaga, "Young's modulus and compositional parameters of oxide glasses, " J. Am. Ceram. Soc. 82, pp. 3501-3507, 1999.
    • (1999) J. Am. Ceram. Soc. , vol.82 , pp. 3501-3507
    • Inaba, S.1    Fujino, S.2    Morinaga, K.3
  • 21
  • 23
    • 0026140999 scopus 로고
    • Fractographic analysis of fused silica optical fibres with sub-threshold indentation flaws
    • S.R. Choi and J.E. Ritter, "Fractographic analysis of fused silica optical fibres with sub-threshold indentation flaws, " Phys. Chem. Glasses 32, pp. 79-80, 1991.
    • (1991) Phys. Chem. Glasses , vol.32 , pp. 79-80
    • Choi, S.R.1    Ritter, J.E.2
  • 24
    • 0020813623 scopus 로고
    • Strength and fatigue of fluoride glass optical fibres
    • S. Sakaguchi and S. Mitachi, "Strength and fatigue of fluoride glass optical fibres, " J. Am. Ceram. Soc. 66, pp. C151-C152, 1983.
    • (1983) J. Am. Ceram. Soc. , vol.66 , pp. C151-C152
    • Sakaguchi, S.1    Mitachi, S.2
  • 25
    • 0027797875 scopus 로고
    • Fractographic analysis of hydrothermally treated silica glass
    • W.T. Han and M. Tomozawa, "Fractographic analysis of hydrothermally treated silica glass, " J. Non-Cryst. Solids 163, pp. 309-314, 1993.
    • (1993) J. Non-Cryst. Solids , vol.163 , pp. 309-314
    • Han, W.T.1    Tomozawa, M.2
  • 26
    • 84987335986 scopus 로고
    • A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements
    • G.R. Anstis, P. Chantikul, B.R. Lawn, and D.B. Marshall, "A critical evaluation of indentation techniques for measuring fracture toughness: I, direct crack measurements, " J. Am. Ceram. Soc. 64, pp. 533-538, 1981.
    • (1981) J. Am. Ceram. Soc. , vol.64 , pp. 533-538
    • Anstis, G.R.1    Chantikul, P.2    Lawn, B.R.3    Marshall, D.B.4
  • 27
    • 0035311129 scopus 로고    scopus 로고
    • Effect of load-dependence of hardness on indentation toughness determination for soda-lime glass
    • J. Gong, W. Si, and Z. Guan, "Effect of load-dependence of hardness on indentation toughness determination for soda-lime glass, " J. Non-Cryst. Solids 282, pp. 325-328, 2001.
    • (2001) J. Non-Cryst. Solids , vol.282 , pp. 325-328
    • Gong, J.1    Si, W.2    Guan, Z.3
  • 28
    • 0031207278 scopus 로고    scopus 로고
    • Indentation brittleness of ceramics: A fresh approach
    • J.B. Quinn and G.D. Quinn, "Indentation brittleness of ceramics: a fresh approach, " J. Mater. Sci. 32, pp. 4331-4346, 1997.
    • (1997) J. Mater. Sci. , vol.32 , pp. 4331-4346
    • Quinn, J.B.1    Quinn, G.D.2
  • 31
    • 0035155713 scopus 로고    scopus 로고
    • Crack growth behavior of zinc tellurite glass with or without sodium oxide
    • S. Yoshida, J. Matsuoka, and N. Soga, "Crack growth behavior of zinc tellurite glass with or without sodium oxide, " J. Non-Cryst. Solids 279, pp. 44-50, 2001.
    • (2001) J. Non-Cryst. Solids , vol.279 , pp. 44-50
    • Yoshida, S.1    Matsuoka, J.2    Soga, N.3
  • 32
    • 0000633967 scopus 로고
    • Relationship between fractal geometry and fractography
    • J.J. Mecholsky and S.W. Freiman, "Relationship between fractal geometry and fractography, " J. Am. Ceram. Soc. 74, pp. 3136-3138, 1991.
    • (1991) J. Am. Ceram. Soc. , vol.74 , pp. 3136-3138
    • Mecholsky, J.J.1    Freiman, S.W.2
  • 33
    • 0026927508 scopus 로고
    • Fractal analysis on fracture surfaces of glass using replication techniques
    • J.J. Mecholsky and J.R. Plaia, "Fractal analysis on fracture surfaces of glass using replication techniques, " J. Non-Cryst. Solids 146, pp. 249-255, 1992.
    • (1992) J. Non-Cryst. Solids , vol.146 , pp. 249-255
    • Mecholsky, J.J.1    Plaia, J.R.2
  • 35
    • 0033324228 scopus 로고    scopus 로고
    • The application of fractal and quantum geometry to brittle fracture
    • J.K. West, J.J. Mecholsky, and L.L. Hench, "The application of fractal and quantum geometry to brittle fracture, " J. Non-Cryst. Solids 260, pp. 99-108, 1999.
    • (1999) J. Non-Cryst. Solids , vol.260 , pp. 99-108
    • West, J.K.1    Mecholsky, J.J.2    Hench, L.L.3
  • 36
    • 0026170699 scopus 로고
    • Fractal fracture in single-crystal silicon
    • Y.L. Tsai and J.J. Mecholsky, "Fractal fracture in single-crystal silicon, " J. Mater. Res. 6, pp. 1248-1263, 1991.
    • (1991) J. Mater. Res. , vol.6 , pp. 1248-1263
    • Tsai, Y.L.1    Mecholsky, J.J.2
  • 37
    • 0023998162 scopus 로고
    • Effects of composition and environment on the fracture of fluoride glass
    • S.W. Freiman and T.L. Baker, "Effects of composition and environment on the fracture of fluoride glass, " J. Am. Ceram. Soc. 71, pp. C214-C216, 1988.
    • (1988) J. Am. Ceram. Soc. , vol.71 , pp. C214-C216
    • Freiman, S.W.1    Baker, T.L.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.