Remanence enhancement and coercivity in two-phase CoPt bulk magnets
|
Author keywords
[No Author keywords available]
|
Indexed keywords
ANNEALING TEMPERATURES;
BULK MAGNETS;
DEGREE OF EXCHANGE;
DISORDER-ORDER;
FACE CENTERED CUBIC PHASE;
FCC PHASE;
HARD PHASIS;
HIGH TEMPERATURE;
LOW TEMPERATURES;
MEAN-GRAIN SIZE;
REMANENCE ENHANCEMENT;
COERCIVE FORCE;
ISOTHERMAL ANNEALING;
METAL CASTINGS;
X RAY DIFFRACTION;
REMANENCE;
|