A study of the global kinetics of thermal degradation of a fibre-intumescent mixture

Author keywords

Cellulosic fibre; Char formation; Intumescent; Kinetics; Mathematical modelling; Pyrolysis; Thermal decomposition

Indexed keywords

COMPOSITE MATERIALS; HEATING; HIGH TEMPERATURE EFFECTS; IMPREGNATION; MATHEMATICAL MODELS; MELAMINE; PYROLYSIS; REACTION KINETICS; SYNTHETIC FIBERS; THERMOGRAVIMETRIC ANALYSIS;

EID: 0036064587     PISSN: 01413910     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0141-3910(02)00033-2     Document Type: Article
Times cited : (14)

References (15)
  • 1
    • 0032842721 scopus 로고    scopus 로고
    • Complex char formation in flame-retarded fibre-intumescent combinations: Physical and chemical nature of char
    • (1999) Text Res. J. , vol.69 , Issue.5 , pp. 374-381
    • Kandola, B.K.1    Horrocks, A.R.2
  • 2
    • 0034314231 scopus 로고    scopus 로고
    • Complex char formation in flame-retarded fibre-intumescent combinations - IV. Mass loss and thermal barrier properties
    • (2000) Fire Mater. , vol.24 , pp. 265-275
    • Kandola, B.K.1    Horrocks, A.R.2
  • 3
    • 0030283415 scopus 로고    scopus 로고
    • Developments in flame retardants for heat and fire resistant textiles - The role of char formation and intumescence
    • (1996) Polym Degrad Stab , vol.54 , pp. 143-154
    • Horrocks, A.R.1
  • 11
    • 0027592828 scopus 로고
    • Non-isothermal thermogravimetry of polymers II. Analysis of TG records of several superimposed temperature-dependent waves
    • (1993) J Thermal Analysis , vol.39 , pp. 569-574
    • Rychly, J.1    Rychla, L.2
  • 15
    • 0033080274 scopus 로고    scopus 로고
    • Modelling thermal degradation of polymers using single-step first-order kinetics
    • (1999) Fire Safety J. , vol.32 , pp. 17-34
    • Staggs, J.E.J.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.