The study on characteristics of heat treatment of the direct squeeze cast 7075 wrought Al alloy

Author keywords

7075 wrought Al alloy; Direct squeeze casting; Non pressurized(gravity) die cast; Rapid cooling rate; Solidification time; Wear loss amount

Indexed keywords

AGING OF MATERIALS; BILLETS (METAL BARS); EUTECTICS; GRAIN BOUNDARIES; HARDNESS; HEAT TREATMENT; METAL CASTING; METALLOGRAPHIC MICROSTRUCTURE; NUCLEATION; PRECIPITATION (CHEMICAL); PRESSURE EFFECTS; SOLIDIFICATION;