메뉴 건너뛰기




Volumn 24, Issue 7, 2001, Pages 695-707

Multiple surface cracking in glass-fiber-reinforced plastics due to a thermal shock at a low temperature

Author keywords

[No Author keywords available]

Indexed keywords


EID: 0035592854     PISSN: 01495739     EISSN: None     Source Type: Journal    
DOI: 10.1080/014957301300194841     Document Type: Article
Times cited : (1)

References (21)
  • 1
    • 0000168481 scopus 로고
    • Edge Stresses in Woven Laminates at Low Temperatures
    • R. D. Kriz, Edge Stresses in Woven Laminates at Low Temperatures, Composite Mat.: Fatigue and Fracture, vol. 2, pp. 150-161, 1989.
    • (1989) Composite Mat.: Fatigue and Fracture , vol.2 , pp. 150-161
    • Kriz, R.D.1
  • 2
    • 0001375786 scopus 로고
    • Small Specimens and New Testing Techniques for Fiber Reinforced Plastics in the Crack Opening Mode (Mode I) and in the Shear Mode (Mode II)
    • K. Humer, E. K. Tschegg, and H. W. Weber, Small Specimens and New Testing Techniques for Fiber Reinforced Plastics in the Crack Opening Mode (Mode I) and in the Shear Mode (Mode II), Adv in Cryogenic Engrg., vol. 40, pp. 999-1006, 1994.
    • (1994) Adv in Cryogenic Engrg. , vol.40 , pp. 999-1006
    • Humer, K.1    Tschegg, E.K.2    Weber, H.W.3
  • 3
    • 0000082847 scopus 로고
    • Mechanical, Electrical and Thermal Characterization of G-10CR and G-11CR Glass/Epoxy Laminates between Room Temperature and 4K
    • M. B. Kasen, G. R. MacDonald, D. H. Beekman, and R. E. Schramm, Mechanical, Electrical and Thermal Characterization of G-10CR and G-11CR Glass/Epoxy Laminates Between Room Temperature and 4K, Adv. in Cryogenic Engrg., vol. 26, pp. 235-244, 1980.
    • (1980) Adv. in Cryogenic Engrg. , vol.26 , pp. 235-244
    • Kasen, M.B.1    MacDonald, G.R.2    Beekman, D.H.3    Schramm, R.E.4
  • 4
    • 0000280245 scopus 로고
    • Current Status of Standardized Nonmetallic Cryogenic Laminates
    • M B Kasen and R. E. Schramm, Current Status of Standardized Nonmetallic Cryogenic Laminates. Adv, in Cryogenic Engrg., vol. 28, pp. 271-277, 1982.
    • (1982) Adv, in Cryogenic Engrg. , vol.28 , pp. 271-277
    • Kasen, M.B.1    Schramm, R.E.2
  • 5
    • 0001511043 scopus 로고
    • Compression and Shear Tests of Vacuum-impregnated Composites at Cryogenic Temperatures
    • N. J Simon, E S. Drexler, and R. P. Reed, Compression and Shear Tests of Vacuum-impregnated Composites at Cryogenic Temperatures, Adv in Cryogenic Engrg., vol. 40, pp. 977-983, 1994.
    • (1994) Adv in Cryogenic Engrg. , vol.40 , pp. 977-983
    • Simon, N.J.1    Drexler, E.S.2    Reed, R.P.3
  • 6
    • 0022070773 scopus 로고
    • Influence of Damage on Mechanical Properties of Woven Composites at Low Temperatures
    • R. D. Kriz, Influence of Damage on Mechanical Properties of Woven Composites at Low Temperatures, J. Composites Tech. Res. vol. 7, pp. 55-58, 1985.
    • (1985) J. Composites Tech. Res. , vol.7 , pp. 55-58
    • Kriz, R.D.1
  • 7
    • 0026396498 scopus 로고
    • Thermal Singular Stresses and Mechanical Properties in Cracked Glass-Fiber Reinforced Plastics at Low Temperatures
    • S Ueda and Y. Shindo, Thermal Singular Stresses and Mechanical Properties in Cracked Glass-Fiber Reinforced Plastics at Low Temperatures, Theoret Appl. Mech , vol. 40, pp. 249-257, 1991.
    • (1991) Theoret Appl. Mech , vol.40 , pp. 249-257
    • Ueda, S.1    Shindo, Y.2
  • 8
    • 0027004863 scopus 로고
    • Glassfiber Reinforced Plastics with a T-Shaped Crack under Tension at Low Temperatures
    • S. Ueda and Y. Shindo, Glassfiber Reinforced Plastics with a T-Shaped Crack under Tension at Low Temperatures. Theoret Appl. Mech., vol. 41, pp. 169-179, 1992.
    • (1992) Theoret Appl. Mech. , vol.41 , pp. 169-179
    • Ueda, S.1    Shindo, Y.2
  • 9
    • 0028401463 scopus 로고
    • Singular Stresses of Glassfibre Reinforced Plastics with a Broken Layer at Low Temperatures
    • S. Ueda and Y. Shindo, Singular Stresses of Glassfibre Reinforced Plastics with a Broken Layer at Low Temperatures, Mat. Sci. Engrg , vol A176, pp. 471-482, 1994.
    • (1994) Mat. Sci. Engrg , vol.A176 , pp. 471-482
    • Ueda, S.1    Shindo, Y.2
  • 10
    • 0012914404 scopus 로고    scopus 로고
    • Stress Intensity Factors for Glass-fiber Reinforced Plastics with an Infinite Row of Parallel Cracks at Low Temperatures
    • K. Sanada, Y. Shindo, and S. Ueda, Stress Intensity Factors for Glass-fiber Reinforced Plastics with an Infinite Row of Parallel Cracks at Low Temperatures, Theoret Appl. Fracture Mech., vol. 28, pp 183-196, 1998.
    • (1998) Theoret Appl. Fracture Mech. , vol.28 , pp. 183-196
    • Sanada, K.1    Shindo, Y.2    Ueda, S.3
  • 11
    • 0027680156 scopus 로고
    • Dynamic Singular Stresses in Cracked Glassfiber Reinforced Plastics at Low Temperatures
    • S. Ueda and Y. Shindo, Dynamic Singular Stresses in Cracked Glassfiber Reinforced Plastics at Low Temperatures, JSME Int. J , Ser A, vol. 36, pp. 367-373, 1993.
    • (1993) JSME Int. J , Ser A , vol.36 , pp. 367-373
    • Ueda, S.1    Shindo, Y.2
  • 12
    • 0034319103 scopus 로고    scopus 로고
    • Dynamic Singular Stresses in Glassfiber Reinforced Plastics with a Broken Layer at Low Temperatures
    • S. Ueda, Dynamic Singular Stresses in Glassfiber Reinforced Plastics with a Broken Layer at Low Temperatures, Int. J Fracture, vol. 106, pp. 13-31, 2000.
    • (2000) Int. J Fracture , vol.106 , pp. 13-31
    • Ueda, S.1
  • 13
    • 1842653624 scopus 로고    scopus 로고
    • Thermal Singular Stresses of Glassfiber Reinforced Plastics with Surface Cracks at Cryogenic Temperatures
    • in press
    • S. Ueda, Thermal Singular Stresses of Glassfiber Reinforced Plastics with Surface Cracks at Cryogenic Temperatures, Int. J Fracture (in press)
    • Int. J Fracture
    • Ueda, S.1
  • 14
    • 0020600019 scopus 로고
    • Transient Thermal Stress Problem for a Circumferentially Cracked Hollow Cylinder
    • H. F. Nied and F. Erdogan, Transient Thermal Stress Problem for a Circumferentially Cracked Hollow Cylinder, J. Thermal Stresses, vol. 6, pp. 1-14, 1983.
    • (1983) J. Thermal Stresses , vol.6 , pp. 1-14
    • Nied, H.F.1    Erdogan, F.2
  • 15
    • 0019583530 scopus 로고
    • Cryogenic Properties of Filamentary-reinforced Composites: An Update
    • M. B. Kasen, Cryogenic Properties of Filamentary-reinforced Composites: an Update, Cryogenics, vol. 21, pp. 323-340, 1981.
    • (1981) Cryogenics , vol.21 , pp. 323-340
    • Kasen, M.B.1
  • 16
    • 0021158693 scopus 로고
    • Singularities of the Tip of a Crack Normal to the Interface of an Anisotropic Layered Composite
    • T. C. Ting and P. H. Hoang, Singularities of the Tip of a Crack Normal to the Interface of an Anisotropic Layered Composite, Int. J. Solids Structures, vol. 20, pp. 439-454, 1984.
    • (1984) Int. J. Solids Structures , vol.20 , pp. 439-454
    • Ting, T.C.1    Hoang, P.H.2
  • 17
    • 0035589975 scopus 로고    scopus 로고
    • Thermoelastic Analysis of W-Cu Functionally Graded Materials Subjected to a Thermal Shock by Micromechanical Model
    • S. Ueda, Thermoelastic Analysis of W-Cu Functionally Graded Materials Subjected to a Thermal Shock by Micromechanical Model, J. Thermal Stresses, vol. 24, pp. 19-45, 2001.
    • (2001) J. Thermal Stresses , vol.24 , pp. 19-45
    • Ueda, S.1
  • 18
    • 0024901936 scopus 로고
    • The Mechanics of Multiple Transverse Cracking in Composite Laminates
    • J. R. Yeh, The Mechanics of Multiple Transverse Cracking in Composite Laminates, Int. J. Solids Structures, vol. 25, pp. 1445-1455, 1989.
    • (1989) Int. J. Solids Structures , vol.25 , pp. 1445-1455
    • Yeh, J.R.1
  • 20
    • 0018136227 scopus 로고
    • Low Temperature Properties of Epoxy Resins and Composites
    • G. Hartwig, Low Temperature Properties of Epoxy Resins and Composites, Adv. in Cryogenic Engrg., vol. 24, pp. 17-36, 1978.
    • (1978) Adv. in Cryogenic Engrg. , vol.24 , pp. 17-36
    • Hartwig, G.1
  • 21
    • 0010318280 scopus 로고
    • Mechanical and Thermal Properties of Filamentary-reinforced Structural Composites at Cryogenic Temperatures 1: Glass-reinforced Composites
    • M. B. Kasen, Mechanical and Thermal Properties of Filamentary-reinforced Structural Composites at Cryogenic Temperatures 1: Glass-reinforced Composites, Cryogenics, vol. 15, pp. 327-349, 1975.
    • (1975) Cryogenics , vol.15 , pp. 327-349
    • Kasen, M.B.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.