메뉴 건너뛰기




Volumn 86, Issue 5, 2001, Pages 526-531

Shear bond strengths of 2 intraoral porcelain repair systems to porcelain or metal substrates

Author keywords

[No Author keywords available]

Indexed keywords

ACRYLIC ACID DERIVATIVE; ACRYLIC ACID RESIN; ADHESIVE AGENT; ALLOY; ALUMINUM SILICATE; BISPHENOL A BIS(2 HYDROXYPROPYL) ETHER DIMETHACRYLATE; BISPHENOL A GLYCIDYL METHACRYLATE; DENTAL ALLOY; ESPE VISIO GEM; ESPE VISIO-GEM; FELDSPAR; GOLD ALLOY; HELIOBOND; METHACRYLIC ACID DERIVATIVE; MONOBOND S; POTASSIUM DERIVATIVE; RESIN; TETRIC CERAM; TOOTH CEMENT; VISIO BOND; VISIO-BOND; WATER;

EID: 0035514702     PISSN: 00223913     EISSN: None     Source Type: Journal    
DOI: 10.1067/mpr.2001.119843     Document Type: Article
Times cited : (75)

References (29)
  • 2
    • 0023967360 scopus 로고
    • Causes of failure following oral rehabilitation: Biological versus technical factors
    • Strub JR, Stiffler S, Schärer P. Causes of failure following oral rehabilitation: biological versus technical factors. Quintessence Int 1988;19:215-22.
    • (1988) Quintessence Int , vol.19 , pp. 215-222
    • Strub, J.R.1    Stiffler, S.2    Schärer, P.3
  • 3
    • 0021403252 scopus 로고
    • Long-term clinical study of porcelain-fused-to-gold restorations
    • Coornaert J, Adriaens P, De Boever J. Long-term clinical study of porcelain-fused-to-gold restorations. J Prosthet Dent 1984;51:338-42.
    • (1984) J Prosthet Dent , vol.51 , pp. 338-342
    • Coornaert, J.1    Adriaens, P.2    De Boever, J.3
  • 5
    • 0027637689 scopus 로고
    • Bond strength of composite resin to porcelain with newer generation of porcelain repair systems
    • Appeldoorn RE, Wilwerding TM, Barkmeier WW. Bond strength of composite resin to porcelain with newer generation of porcelain repair systems. J Prosthet Dent 1993;70:6-11.
    • (1993) J Prosthet Dent , vol.70 , pp. 6-11
    • Appeldoorn, R.E.1    Wilwerding, T.M.2    Barkmeier, W.W.3
  • 7
    • 0026009658 scopus 로고
    • Evaluation of a 4-META porcelain repair system
    • Cooley RL, Tseng EY, Evans JG. Evaluation of a 4-META porcelain repair system. J Esthet Dent 1991;3:11-3.
    • (1991) J Esthet Dent , vol.3 , pp. 11-13
    • Cooley, R.L.1    Tseng, E.Y.2    Evans, J.G.3
  • 8
    • 0025520189 scopus 로고
    • Shear bond strength of composite resin porcelain repair materials bonded to metal and porcelain
    • Beck DA, Janus CE, Douglas HB. Shear bond strength of composite resin porcelain repair materials bonded to metal and porcelain. J Prosthet Dent 1990;64:529-33.
    • (1990) J Prosthet Dent , vol.64 , pp. 529-533
    • Beck, D.A.1    Janus, C.E.2    Douglas, H.B.3
  • 9
    • 0024616164 scopus 로고
    • Porcelain-to-composite bond strengths using four organosilane materials
    • Bailey JH. Porcelain-to-composite bond strengths using four organosilane materials. J Prosthet Dent 1989;61:174-7.
    • (1989) J Prosthet Dent , vol.61 , pp. 174-177
    • Bailey, J.H.1
  • 10
    • 0029684965 scopus 로고    scopus 로고
    • Repairing porcelain restorations intraorally: Techniques and materials
    • passim; quiz 30
    • Zhukovsky L, Godder B, Settembrini L, Scherer W. Repairing porcelain restorations intraorally: techniques and materials. Compend Contin Educ Dent 1996;17:18, 20, 22 passim; quiz 30.
    • (1996) Compend Contin Educ Dent , vol.17 , pp. 18
    • Zhukovsky, L.1    Godder, B.2    Settembrini, L.3    Scherer, W.4
  • 11
    • 0029258548 scopus 로고
    • Shear bond strength of composite resin to microetched metal with five newer-generation bonding agents
    • Czerw RJ, Wakefield CW, Robbins JW, Fulkerson MS. Shear bond strength of composite resin to microetched metal with five newer-generation bonding agents. Oper Dent 1995;20:58-62.
    • (1995) Oper Dent , vol.20 , pp. 58-62
    • Czerw, R.J.1    Wakefield, C.W.2    Robbins, J.W.3    Fulkerson, M.S.4
  • 12
    • 0031228944 scopus 로고    scopus 로고
    • Bonding strengths of porcelain repair systems with various surface treatments
    • Chung KH, Hwang YC. Bonding strengths of porcelain repair systems with various surface treatments. J Prosthet Dent 1997;78:267-74.
    • (1997) J Prosthet Dent , vol.78 , pp. 267-274
    • Chung, K.H.1    Hwang, Y.C.2
  • 13
    • 0027652208 scopus 로고
    • Effects of surface treatment and bonding agents on bond strength of composite resin to porcelain
    • Suliman AH, Swift EJ Jr, Perdigao J. Effects of surface treatment and bonding agents on bond strength of composite resin to porcelain. J Prosthet Dent 1993;70:118-20.
    • (1993) J Prosthet Dent , vol.70 , pp. 118-120
    • Suliman, A.H.1    Swift E.J., Jr.2    Perdigao, J.3
  • 15
    • 0026856210 scopus 로고
    • Bond strength of composite to porcelain treated with new porcelain repair agents
    • Wolf DM, Powers JM, O'Keefe KL. Bond strength of composite to porcelain treated with new porcelain repair agents. Dent Mater 1992;8:158-61.
    • (1992) Dent Mater , vol.8 , pp. 158-161
    • Wolf, D.M.1    Powers, J.M.2    O'Keefe, K.L.3
  • 16
    • 0026893507 scopus 로고
    • The influence of surface conditions and silane agents on the bond of resin to dental porcelain
    • Hayakawa T, Horie K, Aida M, Kanaya H, Kobayashi T, Murata Y. The influence of surface conditions and silane agents on the bond of resin to dental porcelain. Dent Mater 1992;8:238-40.
    • (1992) Dent Mater , vol.8 , pp. 238-240
    • Hayakawa, T.1    Horie, K.2    Aida, M.3    Kanaya, H.4    Kobayashi, T.5    Murata, Y.6
  • 17
    • 0030207640 scopus 로고    scopus 로고
    • Evaluation of porcelain surface treatments and agents for composite-to-porcelain repair
    • Kupiec KA, Wuertz KM, Barkmeier WW, Wilwerding TM. Evaluation of porcelain surface treatments and agents for composite-to-porcelain repair. J Prosthet Dent 1996;76:119-24.
    • (1996) J Prosthet Dent , vol.76 , pp. 119-124
    • Kupiec, K.A.1    Wuertz, K.M.2    Barkmeier, W.W.3    Wilwerding, T.M.4
  • 18
    • 0023413139 scopus 로고
    • Shear strength of the composite bond to etched porcelain
    • Stangel I, Nathanson D, Hsu CS. Shear strength of the composite bond to etched porcelain. J Dent Res 1987;66:1460-5.
    • (1987) J Dent Res , vol.66 , pp. 1460-1465
    • Stangel, I.1    Nathanson, D.2    Hsu, C.S.3
  • 19
    • 0027596321 scopus 로고
    • Sandblasting and silica-coating of dental alloys: Volume loss, morphology and changes in the surface composition
    • Kern M, Thompson VP. Sandblasting and silica-coating of dental alloys: volume loss, morphology and changes in the surface composition. Dent Mater 1993;9:151-61.
    • (1993) Dent Mater , vol.9 , pp. 151-161
    • Kern, M.1    Thompson, V.P.2
  • 20
    • 0029242652 scopus 로고
    • Durability of resin bonds to a cobalt-chromium alloy
    • Kern M, Thompson VP. Durability of resin bonds to a cobalt-chromium alloy. J Dent 1995;23:47-54.
    • (1995) J Dent , vol.23 , pp. 47-54
    • Kern, M.1    Thompson, V.P.2
  • 22
    • 0024722777 scopus 로고
    • An evaluation of the bond strengths of four organosilane materials in response to thermal stress
    • Diaz-Arnold AM, Aquilino SA. An evaluation of the bond strengths of four organosilane materials in response to thermal stress. J Prosthet Dent 1989;62:257-60.
    • (1989) J Prosthet Dent , vol.62 , pp. 257-260
    • Diaz-Arnold, A.M.1    Aquilino, S.A.2
  • 25
    • 0034134024 scopus 로고    scopus 로고
    • Biocompatibility of dental casting alloys: A review
    • Wataha JC. Biocompatibility of dental casting alloys: a review. J Prosthet Dent 2000;83:223-34.
    • (2000) J Prosthet Dent , vol.83 , pp. 223-234
    • Wataha, J.C.1
  • 26
    • 0030641633 scopus 로고    scopus 로고
    • An evaluation of casting alloys used for restorative procedures
    • Leinfelder KF. An evaluation of casting alloys used for restorative procedures. J Am Dent Assoc 1997;128:37-45.
    • (1997) J Am Dent Assoc , vol.128 , pp. 37-45
    • Leinfelder, K.F.1
  • 27
    • 0033072233 scopus 로고    scopus 로고
    • In vitro study of the effect of thermo-and load-cycling on the bond strength of porcelain repair systems
    • Leibrock A, Degenhart M, Behr M, Rosentritt M, Handel G. In vitro study of the effect of thermo-and load-cycling on the bond strength of porcelain repair systems. J Oral Rehabil 1999;26:130-7.
    • (1999) J Oral Rehabil , vol.26 , pp. 130-137
    • Leibrock, A.1    Degenhart, M.2    Behr, M.3    Rosentritt, M.4    Handel, G.5
  • 28
    • 0033071448 scopus 로고    scopus 로고
    • Thermal cycling procedures for laboratory testing of dental restorations
    • Gale MS, Darvell BW. Thermal cycling procedures for laboratory testing of dental restorations. J Dent 1999;27:89-99.
    • (1999) J Dent , vol.27 , pp. 89-99
    • Gale, M.S.1    Darvell, B.W.2
  • 29
    • 0022731613 scopus 로고
    • Effects of 15 vs 60 second enamel acid conditioning on adhesion and morphology
    • Barkmeier WW, Shaffer SE, Gwinnett AJ. Effects of 15 vs 60 second enamel acid conditioning on adhesion and morphology. Oper Dent 1986;11:111-6.
    • (1986) Oper Dent , vol.11 , pp. 111-116
    • Barkmeier, W.W.1    Shaffer, S.E.2    Gwinnett, A.J.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.