The effect of luting media on the fracture resistance of a flame sprayed all-ceramic crown

Author keywords

All ceramic crown; Failure; Fracture resistance; Luting agent

Indexed keywords

GLASS IONOMER; RESIN; RESIN CEMENT; TOOTH CEMENT; ZINC PHOSPHATE;

EID: 0035514021     PISSN: 03005712     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0300-5712(01)00040-9     Document Type: Article
Times cited : (31)

References (32)
  • 2
    • 0005188752 scopus 로고
    • Porcelain baked to gold - A new medium in prosthetics
    • Brecker CS. Porcelain baked to gold - a new medium in prosthetics. Journal of Prosthetic Dentistry 1956;6:801-10.
    • (1956) Journal of Prosthetic Dentistry , vol.6 , pp. 801-810
    • Brecker, C.S.1
  • 3
    • 0023321067 scopus 로고
    • Compressive strengths of a new foil and porcelain-fused-to-metal crowns
    • Brukl CE, Ocampo OO. Compressive strengths of a new foil and porcelain-fused-to-metal crowns. Journal of Prosthetic Dentistry 1987;57:404-10.
    • (1987) Journal of Prosthetic Dentistry , vol.57 , pp. 404-410
    • Brukl, C.E.1    Ocampo, O.O.2
  • 5
    • 0028390711 scopus 로고
    • Ceramic vs porcelain-fused-to-metal crowns: Give your patients a choice
    • Christensen GJ. Ceramic vs porcelain-fused-to-metal crowns: give your patients a choice. Journal of the American Dental Association 1994;125:311-4.
    • (1994) Journal of the American Dental Association , vol.125 , pp. 311-314
    • Christensen, G.J.1
  • 7
    • 0000653434 scopus 로고
    • The reinforcement of dental porcelain with ceramic oxides
    • McLean JW, Hughes TH. The reinforcement of dental porcelain with ceramic oxides. British Dental Journal 1965;119:251-67.
    • (1965) British Dental Journal , vol.119 , pp. 251-267
    • McLean, J.W.1    Hughes, T.H.2
  • 8
    • 0031226791 scopus 로고    scopus 로고
    • Preliminary Investigation of a novel retentive system for In-Ceram and In-Ceram Spinell dental ceramics
    • Wood DJ, Bubb NL, Millar BJ, et al. Preliminary Investigation of a novel retentive system for In-Ceram and In-Ceram Spinell dental ceramics. Journal of Prosthetic Dentistry 1997;78:275-80.
    • (1997) Journal of Prosthetic Dentistry , vol.78 , pp. 275-280
    • Wood, D.J.1    Bubb, N.L.2    Millar, B.J.3
  • 9
    • 0346332876 scopus 로고    scopus 로고
    • Techceram strength in advanced technology
    • Qualtrough AJE. Techceram strength in advanced technology. Dental Practice 1996;34:8.
    • (1996) Dental Practice , vol.34 , pp. 8
    • Qualtrough, A.J.E.1
  • 10
    • 0026955496 scopus 로고
    • The effect of crown length on the fracture resistance of posterior porcelain and glass-ceramic crowns
    • Scherrer SS, de Rijk WG. The effect of crown length on the fracture resistance of posterior porcelain and glass-ceramic crowns. International Journal of Prosthodontics 1992;5:550-7.
    • (1992) International Journal of Prosthodontics , vol.5 , pp. 550-557
    • Scherrer, S.S.1    De Rijk, W.G.2
  • 13
    • 0027546050 scopus 로고
    • In vitro comparison of conventional crowns and a new all-ceramic system
    • Grey NJA, Piddock V, Wilson MA. In vitro comparison of conventional crowns and a new all-ceramic system. Journal of Dentistry 1993;21:47-51.
    • (1993) Journal of Dentistry , vol.21 , pp. 47-51
    • Grey, N.J.A.1    Piddock, V.2    Wilson, M.A.3
  • 14
    • 0031082841 scopus 로고    scopus 로고
    • The effect of different ceramic materials on the fracture resistance of dentine-bonded crowns
    • Mak M, Qualtrough AJE, Burke FJT. The effect of different ceramic materials on the fracture resistance of dentine-bonded crowns. Quintessence International 1997;28:197-203.
    • (1997) Quintessence International , vol.28 , pp. 197-203
    • Mak, M.1    Qualtrough, A.J.E.2    Burke, F.J.T.3
  • 15
    • 0024528428 scopus 로고
    • Marginal seal of injection moulded ceramic crowns cemented with three adhesive systems
    • Shortall AC, Fayyad MA, Williams JD. Marginal seal of injection moulded ceramic crowns cemented with three adhesive systems. Journal of Prosthetic Dentistry 1989;61:24-7.
    • (1989) Journal of Prosthetic Dentistry , vol.61 , pp. 24-27
    • Shortall, A.C.1    Fayyad, M.A.2    Williams, J.D.3
  • 16
    • 0027620663 scopus 로고
    • Effect of luting media on the compressive strengths of two types of all-ceramic crown
    • McCormick JT, Rowland W, Shillingburg HT, et al. Effect of luting media on the compressive strengths of two types of all-ceramic crown. Quintessence International 1993;24:405-8.
    • (1993) Quintessence International , vol.24 , pp. 405-408
    • McCormick, J.T.1    Rowland, W.2    Shillingburg, H.T.3
  • 17
    • 0442303888 scopus 로고    scopus 로고
    • Effect of cement on fracture resistance of all-ceramic crowns
    • Dwan A, Yaman P, Razzooog ME, et al. Effect of cement on fracture resistance of all-ceramic crowns. Journal of Dental Research 1996; 75:2136.
    • (1996) Journal of Dental Research , vol.75 , pp. 2136
    • Dwan, A.1    Yaman, P.2    Razzooog, M.E.3
  • 18
    • 0024067098 scopus 로고
    • Effect of different types of smear layers on dentin and enamel shear bond strengths
    • Tao L, Pashley DH, Boyd L. Effect of different types of smear layers on dentin and enamel shear bond strengths. Dental Materials 1988;4:208-16.
    • (1988) Dental Materials , vol.4 , pp. 208-216
    • Tao, L.1    Pashley, D.H.2    Boyd, L.3
  • 19
    • 0028437167 scopus 로고
    • Fracture resistance of teeth restored with dentine-bonded crowns
    • Burke FJT, Watts DC. Fracture resistance of teeth restored with dentine-bonded crowns. Quintessence International 1994;25:335-40.
    • (1994) Quintessence International , vol.25 , pp. 335-340
    • Burke, F.J.T.1    Watts, D.C.2
  • 20
    • 0026922592 scopus 로고
    • Compressive strength of two modern all-ceramic crowns
    • Pröbster L. Compressive strength of two modern all-ceramic crowns. International Journal of Prosthodontics 1992;5:409-14.
    • (1992) International Journal of Prosthodontics , vol.5 , pp. 409-414
    • Pröbster, L.1
  • 21
    • 0033146116 scopus 로고    scopus 로고
    • Clinically relevant approach to failure testing of all-ceramic restorations
    • Kelly JR. Clinically relevant approach to failure testing of all-ceramic restorations. Journal of Prosthetic Dentistry 1999;81:652-61.
    • (1999) Journal of Prosthetic Dentistry , vol.81 , pp. 652-661
    • Kelly, J.R.1
  • 22
    • 0030154926 scopus 로고    scopus 로고
    • Contact damage as a failure mode during in vitro testing
    • Harvey CK, Kelly JR. Contact damage as a failure mode during in vitro testing. Journal of Prosthodontics 1996;5:95-100.
    • (1996) Journal of Prosthodontics , vol.5 , pp. 95-100
    • Harvey, C.K.1    Kelly, J.R.2
  • 23
    • 0028249215 scopus 로고
    • Long term clinical evaluation of three luting materials
    • Pameijer CH, Nilner K. Long term clinical evaluation of three luting materials. Swedish Dental Journal 1994;18:59-67.
    • (1994) Swedish Dental Journal , vol.18 , pp. 59-67
    • Pameijer, C.H.1    Nilner, K.2
  • 24
    • 0029283875 scopus 로고
    • The effect of variations in bonding procedures on fracture resistance of dentine-bonded all-ceramic crowns
    • Burke FJT. The effect of variations in bonding procedures on fracture resistance of dentine-bonded all-ceramic crowns. Quintessence International 1995;26:293-300.
    • (1995) Quintessence International , vol.26 , pp. 293-300
    • Burke, F.J.T.1
  • 25
    • 0026873580 scopus 로고
    • Tooth fracture in vivo and in vitro
    • Burke FJT. Tooth fracture in vivo and in vitro. Journal of Dentistry 1992;20:131-9.
    • (1992) Journal of Dentistry , vol.20 , pp. 131-139
    • Burke, F.J.T.1
  • 26
    • 0028709614 scopus 로고
    • Fracture surface characterization of clinically failed all-ceramic crowns
    • Thompson JY, Anusavice KJ, Naman A, et al. Fracture surface characterization of clinically failed all-ceramic crowns. Journal of Dental Research 1994;73:1824-32.
    • (1994) Journal of Dental Research , vol.73 , pp. 1824-1832
    • Thompson, J.Y.1    Anusavice, K.J.2    Naman, A.3
  • 27
    • 0026878328 scopus 로고
    • Crown behaviour during cementation
    • Wilson PR. Crown behaviour during cementation. Journal of Dentistry 1992;20:156-62.
    • (1992) Journal of Dentistry , vol.20 , pp. 156-162
    • Wilson, P.R.1
  • 28
    • 0026886739 scopus 로고
    • The effect of adhesive luting agent-dentinal surface interaction on film thickness
    • White SN, Zhaokun YU. The effect of adhesive luting agent-dentinal surface interaction on film thickness. Journal of prosthetic Dentistry 1992;68:49-52.
    • (1992) Journal of Prosthetic Dentistry , vol.68 , pp. 49-52
    • White, S.N.1    Zhaokun, Y.U.2
  • 29
    • 0028399185 scopus 로고
    • Comparison of patient perceived post cementation sensitivity with glass ionomer and zinc phosphate cements
    • Bebermeyer RD, Berg JH. Comparison of patient perceived post cementation sensitivity with glass ionomer and zinc phosphate cements. Quintessence International 1994;25:209-14.
    • (1994) Quintessence International , vol.25 , pp. 209-214
    • Bebermeyer, R.D.1    Berg, J.H.2
  • 30
    • 0028545354 scopus 로고
    • An investigation into the pressure transmitted to the pulp chamber on crown cementation: A laboratory study
    • Wylie SG, Wilson PR. An investigation into the pressure transmitted to the pulp chamber on crown cementation: a laboratory study. Journal of Dental Research 1994;73:1684-9.
    • (1994) Journal of Dental Research , vol.73 , pp. 1684-1689
    • Wylie, S.G.1    Wilson, P.R.2
  • 31
  • 32
    • 0031614740 scopus 로고    scopus 로고
    • Effect of differing resin luting systems on fracture resistance of teeth restored with dentin-bonded crowns
    • Burke FJT, Watts DC. Effect of differing resin luting systems on fracture resistance of teeth restored with dentin-bonded crowns. Quintessence International 1998;29:21-7.
    • (1998) Quintessence International , vol.29 , pp. 21-27
    • Burke, F.J.T.1    Watts, D.C.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.