메뉴 건너뛰기




Volumn 84, Issue 8, 2001, Pages 1767-1776

Wet Erosive Wear of Alumina Densified with Magnesium Silicate Additions

Author keywords

[No Author keywords available]

Indexed keywords

ADDITION REACTIONS; DENSIFICATION; FRACTURE MECHANICS; GRAIN BOUNDARIES; GRAIN SIZE AND SHAPE; MAGNESIUM COMPOUNDS; PHOTOLUMINESCENCE; POLYCRYSTALLINE MATERIALS; SINTERING; THERMAL EXPANSION; WEAR OF MATERIALS;

EID: 0035437656     PISSN: 00027820     EISSN: None     Source Type: Journal    
DOI: 10.1111/j.1151-2916.2001.tb00913.x     Document Type: Article
Times cited : (22)

References (34)
  • 1
    • 0345941375 scopus 로고
    • "Data Review," Section 1, "High-Alumina Ceramics,"
    • Her Majesty's Stationery Office, London, U.K.
    • R. Morrell, Handbook of Properties of Technical and Engineering Ceramics, Part 2, "Data Review," Section 1, "High-Alumina Ceramics," Her Majesty's Stationery Office, London, U.K., 1987.
    • (1987) Handbook of Properties of Technical and Engineering Ceramics , Issue.2 PART
    • Morrell, R.1
  • 2
    • 0016972484 scopus 로고
    • Effect of Microstructure on Rate of Machining of Ceramics
    • R. W. Rice and B. K. Speronello, "Effect of Microstructure on Rate of Machining of Ceramics," J. Am. Ceram. Soc., 59, 330-33 (1976).
    • (1976) J. Am. Ceram. Soc. , vol.59 , pp. 330-333
    • Rice, R.W.1    Speronello, B.K.2
  • 3
    • 0020718748 scopus 로고
    • Effect of Material Parameters on the Erosion Resistance of Brittle Materials
    • S. M. Wiederhorn and B. J. Hockey, "Effect of Material Parameters on the Erosion Resistance of Brittle Materials," J. Mater. Sci., 18, 766-80 (1983).
    • (1983) J. Mater. Sci. , vol.18 , pp. 766-780
    • Wiederhorn, S.M.1    Hockey, B.J.2
  • 4
    • 0023362875 scopus 로고
    • Microstructural Effects on Grinding of Alumina and Glass-Ceramics
    • D. B. Marshall, B. R. Lawn, and R. F. Cook, "Microstructural Effects on Grinding of Alumina and Glass-Ceramics," J. Am. Ceram. Soc., 70, C-139-C-140 (1987).
    • (1987) J. Am. Ceram. Soc. , vol.70
    • Marshall, D.B.1    Lawn, B.R.2    Cook, R.F.3
  • 5
    • 0025205356 scopus 로고
    • Effect of Surface Finish on the Sliding Wear of Alumina
    • M. G. Gee and E. A. Almond, "Effect of Surface Finish on the Sliding Wear of Alumina," J. Mater. Sci., 25, 296-310 (1990).
    • (1990) J. Mater. Sci. , vol.25 , pp. 296-310
    • Gee, M.G.1    Almond, E.A.2
  • 6
    • 0028381561 scopus 로고
    • Grain Size Effects on the Wet Erosive Wear of High-Purity Polycrystalline Alumina
    • M. Miranda-Martinez, R. W. Davidge, and F. L. Riley, "Grain Size Effects on the Wet Erosive Wear of High-Purity Polycrystalline Alumina," Wear, 172, 41-48 (1994).
    • (1994) Wear , vol.172 , pp. 41-48
    • Miranda-Martinez, M.1    Davidge, R.W.2    Riley, F.L.3
  • 7
    • 0030647683 scopus 로고    scopus 로고
    • Factors Affecting the Wet Erosive Wear of Liquid-Phase-Sintered Aluminas
    • Key Engineering Materials, Edited by J. Baxter et al. TransTech, Aedermannsdorf, Switzerland
    • P. C. Twigg, R. W. Davidge, S. G. Roberts, and F. L. Riley, "Factors Affecting the Wet Erosive Wear of Liquid-Phase-Sintered Aluminas": pp. 1524-27 in Key Engineering Materials, Vols. 132-136, Part 3, European Ceramics, V. Edited by J. Baxter et al. TransTech, Aedermannsdorf, Switzerland, 1997.
    • (1997) European Ceramics, V , vol.132-136 , Issue.3 PART , pp. 1524-1527
    • Twigg, P.C.1    Davidge, R.W.2    Roberts, S.G.3    Riley, F.L.4
  • 8
    • 0031997931 scopus 로고    scopus 로고
    • Microstructure and Chemistry of Intergranular Glassy Films in Liquid-Phase-Sintered Alumina
    • R. Brydson, P. C. Twigg, S. C. Chen, F. L. Riley, X. Pan, and M. Rühle, " Microstructure and Chemistry of Intergranular Glassy Films in Liquid-Phase-Sintered Alumina," J. Am. Ceram. Soc., 81, 369-79 (1998).
    • (1998) J. Am. Ceram. Soc. , vol.81 , pp. 369-379
    • Brydson, R.1    Twigg, P.C.2    Chen, S.C.3    Riley, F.L.4    Pan, X.5    Rühle, M.6
  • 9
    • 0035295263 scopus 로고    scopus 로고
    • 2 Ratio on the Chemistry of Intergranular Films in Liquid Phase Sintered Alumina and Implications for Rate of Erosive Wear
    • in press
    • 2 Ratio on the Chemistry of Intergranular Films in Liquid Phase Sintered Alumina and Implications for Rate of Erosive Wear," J. Mater. Res., (2001), in press.
    • (2001) J. Mater. Res.
    • Brydson, R.1    Twigg, P.C.2    Riley, F.L.3
  • 11
    • 0013247382 scopus 로고    scopus 로고
    • Mapping Residual Stresses Using Optical Microprobe in Alumina Films Formed by Thermal Oxidation of NiAl
    • A. Atkinson, D. R Clarke, and S. J. Webb, "Mapping Residual Stresses Using Optical Microprobe in Alumina Films Formed by Thermal Oxidation of NiAl," Mater. Sci. Technol., 14, 531-34 (1998).
    • (1998) Mater. Sci. Technol. , vol.14 , pp. 531-534
    • Atkinson, A.1    Clarke, D.R.2    Webb, S.J.3
  • 12
    • 40549125271 scopus 로고
    • Determination of the Piezospectroscopic Coefficients for Chromium-Doped Sapphire
    • J. He and D. R. Clarke, "Determination of the Piezospectroscopic Coefficients for Chromium-Doped Sapphire," J. Am. Ceram. Soc., 78, 1347-53 (1995).
    • (1995) J. Am. Ceram. Soc. , vol.78 , pp. 1347-1353
    • He, J.1    Clarke, D.R.2
  • 13
    • 0028382718 scopus 로고
    • Piezospectroscopic Determination of Residual Stresses in Polycrystalline Alumina
    • Q. Ma and D. R. Clarke, "Piezospectroscopic Determination of Residual Stresses in Polycrystalline Alumina," J. Am. Ceram. Soc., 77, 298-302 (1994).
    • (1994) J. Am. Ceram. Soc. , vol.77 , pp. 298-302
    • Ma, Q.1    Clarke, D.R.2
  • 15
    • 84987359727 scopus 로고
    • Grain-Size Dependence of Fracture Energy in Ceramics: II, A Model for Noncubic Materials
    • R. W. Rice and S. W. Freiman, "Grain-Size Dependence of Fracture Energy in Ceramics: II, A Model for Noncubic Materials," J. Am. Ceram. Soc., 64, 350-54 (1981).
    • (1981) J. Am. Ceram. Soc. , vol.64 , pp. 350-354
    • Rice, R.W.1    Freiman, S.W.2
  • 16
    • 0017982146 scopus 로고
    • Impact Damage in Brittle Materials in the Elastic-Plastic Regime
    • A. G. Evans, M. E. Gulden, and M. Rosenblatt, "Impact Damage in Brittle Materials in the Elastic-Plastic Regime," Proc. R. Soc. London A, 361, 343-65 (1978).
    • (1978) Proc. R. Soc. London A , vol.361 , pp. 343-365
    • Evans, A.G.1    Gulden, M.E.2    Rosenblatt, M.3
  • 17
    • 0002699323 scopus 로고
    • Abrasive Wear in Ceramics: An Assessment
    • Edited by B. J. Hockley and R. W. Rice. National Bureau of Standards Special Publication 562, U.S. Government Printing Office. Washington, DC
    • A. G. Evans, "Abrasive Wear in Ceramics: An Assessment"; pp.1-14 in The Science at Ceramic Machining and Surface Finishing II. Edited by B. J. Hockley and R. W. Rice. National Bureau of Standards Special Publication 562, U.S. Government Printing Office. Washington, DC, 1979.
    • (1979) The Science at Ceramic Machining and Surface Finishing II , pp. 1-14
    • Evans, A.G.1
  • 18
    • 0018305252 scopus 로고
    • Strength Degradation of Glass Impacted with Sharp Particles: I, Annealed Surface
    • S. M. Wiederhorn and B. R. Lawn, "Strength Degradation of Glass Impacted with Sharp Particles: I, Annealed Surface," J. Am. Ceram. Soc., 62, 66-70 (1979).
    • (1979) J. Am. Ceram. Soc. , vol.62 , pp. 66-70
    • Wiederhorn, S.M.1    Lawn, B.R.2
  • 19
    • 0025478077 scopus 로고
    • Structure of Alumina Grain Boundaries Prepared with and without a Thin Amorphous Intergranular Film
    • D. W. Susnitzky and C. B. Carter, "Structure of Alumina Grain Boundaries Prepared with and without a Thin Amorphous Intergranular Film," J. Am. Ceram. Soc., 73, 2485-93 (1990).
    • (1990) J. Am. Ceram. Soc. , vol.73 , pp. 2485-2493
    • Susnitzky, D.W.1    Carter, C.B.2
  • 21
    • 0025474796 scopus 로고
    • Faceting Behavior of Alumina in the Presence of a Glass
    • Y. K. Simpson and C. B. Carter, "Faceting Behavior of Alumina in the Presence of a Glass," J. Am. Ceram. Soc., 73, 2391-98 (1990).
    • (1990) J. Am. Ceram. Soc. , vol.73 , pp. 2391-2398
    • Simpson, Y.K.1    Carter, C.B.2
  • 22
    • 0007676814 scopus 로고
    • Microstructure of a 96% Alumina Ceramic: II. Crystallization of High-Magnesia Boundary Glasses
    • C. A. Powell-Dogan and A. H. Heuer, "Microstructure of a 96% Alumina Ceramic: II. Crystallization of High-Magnesia Boundary Glasses," J. Am. Ceram. Soc., 73, 3677-83 (1990).
    • (1990) J. Am. Ceram. Soc. , vol.73 , pp. 3677-3683
    • Powell-Dogan, C.A.1    Heuer, A.H.2
  • 24
    • 33846351913 scopus 로고
    • Grain-Size and R-Curve Effects in the Abrasive Wear of Alumina
    • S.-J. Cho, B. J. Hockey, B. R. Lawn, and S. J. Bennison, "Grain-Size and R-Curve Effects in the Abrasive Wear of Alumina," J. Am. Ceram. Soc., 72, 1249-52 (1989).
    • (1989) J. Am. Ceram. Soc. , vol.72 , pp. 1249-1252
    • Cho, S.-J.1    Hockey, B.J.2    Lawn, B.R.3    Bennison, S.J.4
  • 25
    • 0023126048 scopus 로고
    • On the Equilibrium Thickness of Intergranular Glass Phases in Ceramic Materials
    • D. R. Clarke, "On the Equilibrium Thickness of Intergranular Glass Phases in Ceramic Materials," J. Am. Ceram. Soc., 70, 15-22 (1987).
    • (1987) J. Am. Ceram. Soc. , vol.70 , pp. 15-22
    • Clarke, D.R.1
  • 26
    • 0031199954 scopus 로고    scopus 로고
    • Atomistic Structure of Calcium Silicate Intergranular Films in Alumina Studied by Molecular Dynamics Simulation
    • S. Blonski and S. H. Garofalini, "Atomistic Structure of Calcium Silicate Intergranular Films in Alumina Studied by Molecular Dynamics Simulation," J. Am. Ceram. Soc., 80, 1997-2004 (1997).
    • (1997) J. Am. Ceram. Soc. , vol.80 , pp. 1997-2004
    • Blonski, S.1    Garofalini, S.H.2
  • 28
    • 84985123247 scopus 로고
    • Improved Flaw Tolerance in Alumina Containing 1 vol% Anorthite via Crystallization of the Intergranular Glass
    • N. P. Padture and H. M. Chan, "Improved Flaw Tolerance in Alumina Containing 1 vol% Anorthite via Crystallization of the Intergranular Glass," J. Am. Ceram. Soc., 75, 1870-75 (1992).
    • (1992) J. Am. Ceram. Soc. , vol.75 , pp. 1870-1875
    • Padture, N.P.1    Chan, H.M.2
  • 29
    • 84979186757 scopus 로고
    • Relationship between Chemical Composition and Thermal Expansion of Glasses
    • S. English and W. E. S. Turner, "Relationship between Chemical Composition and Thermal Expansion of Glasses," J. Am. Ceram. Soc., 10, 551-70 (1929).
    • (1929) J. Am. Ceram. Soc. , vol.10 , pp. 551-570
    • English, S.1    Turner, W.E.S.2
  • 30
    • 0029329002 scopus 로고
    • The Grain Size Dependence of the Wear of Alumina
    • R. W. Davidge and F. L. Riley, "The Grain Size Dependence of the Wear of Alumina," Wear, 186-187, 45-49 (1995).
    • (1995) Wear , vol.186-187 , pp. 45-49
    • Davidge, R.W.1    Riley, F.L.2
  • 31
    • 0023327964 scopus 로고
    • Crack-Interface Grain Bridging as a Fracture Resistance Mechanism in Ceramics: I, Experimental Study on Alumina
    • P. L. Swanson, C. J. Fairbanks, B. R. Lawn, Y.-W. Mai, and B. J. Hockey, "Crack-Interface Grain Bridging as a Fracture Resistance Mechanism in Ceramics: I, Experimental Study on Alumina," J. Am. Ceram. Soc., 70, 279-89 (1987).
    • (1987) J. Am. Ceram. Soc. , vol.70 , pp. 279-289
    • Swanson, P.L.1    Fairbanks, C.J.2    Lawn, B.R.3    Mai, Y.-W.4    Hockey, B.J.5
  • 33
    • 11544334425 scopus 로고
    • The Strength of Two-Phase Ceramic Materials
    • R. W. Davidge and T. J. Green, "The Strength of Two-Phase Ceramic Materials," J. Mater. Sci., 3, 629-34 (1968).
    • (1968) J. Mater. Sci. , vol.3 , pp. 629-634
    • Davidge, R.W.1    Green, T.J.2
  • 34
    • 0030482147 scopus 로고    scopus 로고
    • The Effects of Silicon Carbide Nano-Phase on the Wet Erosive Wear of Polycrystalline Alumina
    • P. C. Twigg, R. W. Davidge, and F. L. Riley, "The Effects of Silicon Carbide Nano-Phase on the Wet Erosive Wear of Polycrystalline Alumina," J. Eur. Ceram. Soc., 16, 799-802 (1996).
    • (1996) J. Eur. Ceram. Soc. , vol.16 , pp. 799-802
    • Twigg, P.C.1    Davidge, R.W.2    Riley, F.L.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.