메뉴 건너뛰기




Volumn 40 B, Issue 3-4, 2001, Pages 507-515

Brittle failure versus structure of HDPE pipe resins

Author keywords

Failure mode; Polyethylene; Structure

Indexed keywords

CHARACTERIZATION; DIFFERENTIAL SCANNING CALORIMETRY; FAILURE (MECHANICAL); HIGH DENSITY POLYETHYLENES; MORPHOLOGY; OPTIMIZATION; PLASTIC PIPE; STRUCTURE (COMPOSITION);

EID: 0035325301     PISSN: 00222348     EISSN: None     Source Type: Journal    
DOI: 10.1081/MB-100106173     Document Type: Article
Times cited : (16)

References (7)
  • 4
    • 0003056319 scopus 로고    scopus 로고
    • Notch tensile test to measure the resistance to slow crack growth of polyethylene materials for pipe and fitting products (PENT)
    • ISO/CD 16241
  • 5
    • 39349113986 scopus 로고    scopus 로고
    • Plastics-Determination of Environmental Stress Cracking (ESC) of Polyethylene (PE)-Full Notch Creep Test (FNCT)
    • ISO/CD 16770
  • 6
    • 44049120740 scopus 로고
    • Evaluation of the heterogeneity in linear low-density polyethylene comonomer unit distribution by differential scanning calorimetry characterisation of thermally treated samples
    • (1992) Polymer , vol.33 , Issue.20 , pp. 4337-4342
    • Adison, E.1    Ribeiro, M.2    Deffieux, A.3    Fontanille, M.4


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.