메뉴 건너뛰기




Volumn 83, Issue 11, 2000, Pages 2788-2792

Crack healing behavior of silicon carbide ceramics

Author keywords

[No Author keywords available]

Indexed keywords

BENDING STRENGTH; CERAMIC MATERIALS; CRACKS; FATIGUE TESTING; HEAT TREATMENT;

EID: 0034323009     PISSN: 00027820     EISSN: None     Source Type: Journal    
DOI: 10.1111/j.1151-2916.2000.tb01632.x     Document Type: Article
Times cited : (84)

References (17)
  • 1
    • 0016873264 scopus 로고
    • Controlled surface flaws in hot-pressed SiC
    • J. J. Petrovic and L. A Jacobson "Controlled Surface Flaws in Hot-Pressed SiC," J. Am. Ceram. Soc. 59 [1-2] 34-37 (1976).
    • (1976) J. Am. Ceram. Soc. , vol.59 , Issue.1-2 , pp. 34-37
    • Petrovic, J.J.1    Jacobson, L.A.2
  • 2
    • 0016951229 scopus 로고
    • Crack healing and strengthening of thermally shocked alumina
    • T. K. Gupta, "Crack Healing and Strengthening of Thermally Shocked Alumina," J. Am. Ceram. Soc. 59 [5-6] 259-62 (1976).
    • (1976) J. Am. Ceram. Soc. , vol.59 , Issue.5-6 , pp. 259-262
    • Gupta, T.K.1
  • 3
    • 0026840695 scopus 로고
    • Crack healing behaviour of hot pressed silicon nitride due to oxidation
    • S. R. Choi and V. Tikare, "Crack Healing Behaviour of Hot Pressed Silicon Nitride Due to Oxidation" Ser. Metall. Mater., 26, 1263-68 (1992).
    • (1992) Ser. Metall. Mater. , vol.26 , pp. 1263-1268
    • Choi, S.R.1    Tikare, V.2
  • 4
    • 0029779785 scopus 로고    scopus 로고
    • High temperature crack annealing effect on fracture toughness of alumina and alumina-SiC composite
    • J. E. Moffatt, W. J. Plumbridge, and R. Hermann, "High Temperature Crack Annealing Effect on Fracture Toughness of Alumina and Alumina-SiC Composite," Br. Ceram. Trans., 95 [1] 23-29 (1996).
    • (1996) Br. Ceram. Trans. , vol.95 , Issue.1 , pp. 23-29
    • Moffatt, J.E.1    Plumbridge, W.J.2    Hermann, R.3
  • 5
    • 0029371327 scopus 로고
    • Damage healing and strengthening behaviour in intelligent mullite/SiC ceramics
    • M. C. Chu, S. Sato, Y. Kobayashi, and K. Ando, "Damage Healing and Strengthening Behaviour in Intelligent Mullite/SiC Ceramics," Fatigue Fract. Eng. Mater. Struct., 18 [9] 1019-29 (1995).
    • (1995) Fatigue Fract. Eng. Mater. Struct. , vol.18 , Issue.9 , pp. 1019-1029
    • Chu, M.C.1    Sato, S.2    Kobayashi, Y.3    Ando, K.4
  • 6
    • 85004287822 scopus 로고
    • Study on strengthening of mullite by dispersion of carbide ceramics particles
    • M. C. Chu, S. Sato, Y. Kobayashi, and K. Ando, "Study on Strengthening of Mullite by Dispersion of Carbide Ceramics Particles" (in Jpn.), Jpn. Soc. Mech. Eng., 60 [580] 2829-34 (1994).
    • (1994) Jpn. Soc. Mech. Eng. , vol.60 , Issue.580 , pp. 2829-2834
    • Chu, M.C.1    Sato, S.2    Kobayashi, Y.3    Ando, K.4
  • 9
    • 0003157862 scopus 로고    scopus 로고
    • 4 ceramics and its application to structural integrity
    • Edited by M. W. Brown, E. R de los Rios, and K. J. Miller. Engineering Materials Advisory Services, Sheffield, U.K.
    • 4 Ceramics and Its Application to Structural Integrity"; pp. 497-502 in Fracture from Defects, EFC-12. Edited by M. W. Brown, E. R de los Rios, and K. J. Miller. Engineering Materials Advisory Services, Sheffield, U.K., 1998.
    • (1998) Fracture from Defects, EFC-12 , pp. 497-502
    • Ando, K.1    Sato, S.2    Kobayashi, Y.3    Chu, M.C.4
  • 10
    • 0033208064 scopus 로고    scopus 로고
    • Fatigue properties of crack healed mullite/SiC composite ceramics
    • K. Ando, K. Tsuji, M. Ariga, and S. Sato, "Fatigue Properties of Crack Healed Mullite/SiC Composite Ceramics" (in Jpn.), J. Soc. Mater. Sci., Jpn., 48 [10] 1151-56 (1999).
    • (1999) J. Soc. Mater. Sci., Jpn. , vol.48 , Issue.10 , pp. 1151-1156
    • Ando, K.1    Tsuji, K.2    Ariga, M.3    Sato, S.4
  • 11
    • 84875873679 scopus 로고    scopus 로고
    • The study on crack healing behavior of silicon nitride ceramics
    • K. Ando, M. C. Chu, S. Sato, F. Yao, and Y. Kobayashi, "The Study on Crack Healing Behavior of Silicon Nitride Ceramics" (in Jpn.), Jpn. Soc. Mech. Eng., 64 [623] 1936-42 (1998).
    • (1998) Jpn. Soc. Mech. Eng. , vol.64 , Issue.623 , pp. 1936-1942
    • Ando, K.1    Chu, M.C.2    Sato, S.3    Yao, F.4    Kobayashi, Y.5
  • 12
    • 0002251556 scopus 로고    scopus 로고
    • Crack healing behaviour of silicon nitride ceramics (effect of chemical composition on crack healing ability)
    • M. C. Chu, K. Ando, T. Hirasawa, S. Sato, and Y. Kobayashi, "Crack Healing Behaviour of Silicon Nitride Ceramics (Effect of Chemical Composition on Crack Healing Ability)" (in Jpn.), J. High Pressure Inst. Jpn., 36 [2] 82-89 (1998).
    • (1998) J. High Pressure Inst. Jpn. , vol.36 , Issue.2 , pp. 82-89
    • Chu, M.C.1    Ando, K.2    Hirasawa, T.3    Sato, S.4    Kobayashi, Y.5
  • 13
    • 0001195536 scopus 로고    scopus 로고
    • Crack healing behaviour and high temperature strength of silicon nitride ceramics
    • K. Ando, M. C. Chu, S. Sato, F. Yao, and Y. Kobayashi, "Crack Healing Behaviour and High Temperature Strength of Silicon Nitride Ceramics" (in Jpn.), Jpn. Soc. Mech. Eng., 65 [633] 1132-39 (1999).
    • (1999) Jpn. Soc. Mech. Eng. , vol.65 , Issue.633 , pp. 1132-1139
    • Ando, K.1    Chu, M.C.2    Sato, S.3    Yao, F.4    Kobayashi, Y.5
  • 16
    • 0006838368 scopus 로고    scopus 로고
    • Japan Industrial Standard R1601. Testing Method for Flexural Strength of High Performance Ceramics, Japan Standards Association, 1993
    • Japan Industrial Standard R1601. Testing Method for Flexural Strength of High Performance Ceramics, Japan Standards Association, 1993.
  • 17
    • 0006831185 scopus 로고    scopus 로고
    • Japan Industrial Standard R1607, Testing Method for Fracture Toughness of High Performance Ceramics, Japan Standards Association, 1993
    • Japan Industrial Standard R1607, Testing Method for Fracture Toughness of High Performance Ceramics, Japan Standards Association, 1993.


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.