Volumn 16, Issue 4, 2000, Pages 280-284

Effect of furnace type and ceramming heat treatment conditions on the biaxial flexural strength of a canasite glass-ceramic

Author keywords

Biaxial flexural strength; Castable glass ceramic; Ceramming cycles; Fluorcanasite; Furnace type

Indexed keywords

BIOMEDICAL AND DENTAL MATERIALS; FLUOROCANASITE; GLASS;

EID: 0034230460     PISSN: 01095641     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0109-5641(00)00018-X     Document Type: Article
Times cited : (21)

References (13)
  • 1
    • 0347251824 scopus 로고    scopus 로고
    • The strength of a canasite glass-ceramic using dental laboratory procedures
    • Abstr. no. 2467
    • Shareef MY, Johnson A, van Noort R. The strength of a canasite glass-ceramic using dental laboratory procedures. J Dent Res 1998;77:940 (Abstr. no. 2467).
    • (1998) J Dent Res , vol.77 , pp. 940
    • Shareef, M.Y.1    Johnson, A.2    Van Noort, R.3
  • 3
    • 0004205930 scopus 로고    scopus 로고
    • Effect of nucleation temperature on toughness and flexure strength of canasite glass-ceramic
    • Abstr. no. 395
    • Anusavice KJ, Khang N-Z. Effect of nucleation temperature on toughness and flexure strength of canasite glass-ceramic. J Dent Res 1996;75:67 (Abstr. no. 395).
    • (1996) J Dent Res , vol.75 , pp. 67
    • Anusavice, K.J.1    Khang, N.-Z.2
  • 5
    • 0032223645 scopus 로고    scopus 로고
    • Chemical durability of Dicor and fluorocanasite-based glass-ceramic
    • Anusavice KJ, Khang N-Z. Chemical durability of Dicor and fluorocanasite-based glass-ceramic. J Dent Res 1998;77:1553-9.
    • (1998) J Dent Res , vol.77 , pp. 1553-1559
    • Anusavice, K.J.1    Khang, N.-Z.2
  • 6
    • 0026412860 scopus 로고
    • Chain silicate glass-ceramics
    • Beal GH. Chain silicate glass-ceramics. J Non-Cryst Solids 1991;129:163.
    • (1991) J Non-Cryst Solids , vol.129 , pp. 163
    • Beal, G.H.1
  • 7
    • 0029517755 scopus 로고
    • Effect of fluorine content on crystallization of canasite glass-ceramics
    • Likitvanichkul S, Lacourse WC. Effect of fluorine content on crystallization of canasite glass-ceramics. J Mater Sci 1995;30:6151-5.
    • (1995) J Mater Sci , vol.30 , pp. 6151-6155
    • Likitvanichkul, S.1    Lacourse, W.C.2
  • 8
    • 0032198383 scopus 로고    scopus 로고
    • The effect of casting conditions on the biaxial flexural strength of glass-ceramic materials
    • Johnson A, Shareef MY, Walsh JM, Hatton PV, Van Noort R, Hill RG. The effect of casting conditions on the biaxial flexural strength of glass-ceramic materials. Dent Mater 1998;14:412-6.
    • (1998) Dent Mater , vol.14 , pp. 412-416
    • Johnson, A.1    Shareef, M.Y.2    Walsh, J.M.3    Hatton, P.V.4    Van Noort, R.5    Hill, R.G.6
  • 9
    • 0345990811 scopus 로고    scopus 로고
    • Effect of cooling rate on the biaxial flexural strength of two experimental castable glass-ceramics
    • Abstr. no. 317
    • Johnson A, Shareef MY, Walsh JM, Hatton PV, Van Noort R. Effect of cooling rate on the biaxial flexural strength of two experimental castable glass-ceramics. J Dent Res 1999;78:1074 (Abstr. no. 317).
    • (1999) J Dent Res , vol.78 , pp. 1074
    • Johnson, A.1    Shareef, M.Y.2    Walsh, J.M.3    Hatton, P.V.4    Van Noort, R.5
  • 10
    • 0345990815 scopus 로고    scopus 로고
    • BS EN ISO 6872. Dental Ceramics, 1999. p. 1-10.
    • (1999) Dental Ceramics , pp. 1-10
  • 11
    • 0022606596 scopus 로고
    • Comparison of the strengths of aluminous porcelain fired onto platinum and palladium foils
    • Piddock V, Marquis PM, Wilson HT. Comparison of the strengths of aluminous porcelain fired onto platinum and palladium foils. J Oral Rehabil 1986;13:31-37.
    • (1986) J Oral Rehabil , vol.13 , pp. 31-37
    • Piddock, V.1    Marquis, P.M.2    Wilson, H.T.3
  • 12
    • 0033087401 scopus 로고    scopus 로고
    • The biaxial flexural strength of two pressable ceramic systems
    • Cattell MJ, Knowles JC, Clarke RL, Lynch E. The biaxial flexural strength of two pressable ceramic systems. J Dent 1999;27:183-96.
    • (1999) J Dent , vol.27 , pp. 183-196
    • Cattell, M.J.1    Knowles, J.C.2    Clarke, R.L.3    Lynch, E.4
  • 13
    • 0004111312 scopus 로고
    • London: Academic Press, chap. 4
    • McMillan PW. Glass-ceramics. London: Academic Press, 1979. (chap. 4, p. 1-12).
    • (1979) Glass-ceramics , pp. 1-12
    • McMillan, P.W.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.