메뉴 건너뛰기




Volumn 233-235, Issue , 1999, Pages 293-305

The damage mechanisms of several plasma-sprayed ceramic coatings in controlled scratching

Author keywords

Fracture; Plasma sprayed ceramic coatings; Scratching; Wear mechanism

Indexed keywords

ALUMINA; CRACKS; FRACTURE; MICROSTRUCTURE; MORPHOLOGY; PLASMA SPRAYING; POLISHING; PORE SIZE;

EID: 0033380465     PISSN: 00431648     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0043-1648(99)00211-2     Document Type: Conference Paper
Times cited : (64)

References (22)
  • 1
    • 0343024453 scopus 로고
    • Plasma-sprayed ceramic coatings
    • in: K.N. Strafford et al. (Eds.), Technomic Publishing, Lancaster
    • R. McPherson, Plasma-sprayed ceramic coatings, in: K.N. Strafford et al. (Eds.), Surface Engineering: Processes and Applications, Technomic Publishing, Lancaster, 1995, pp. 3-20.
    • (1995) Surface Engineering: Processes and Applications , pp. 3-20
    • McPherson, R.1
  • 2
    • 0026864342 scopus 로고
    • The effect of microstructure on wear modes of ceramic materials
    • Ajayi O.O., Ludema K.C. The effect of microstructure on wear modes of ceramic materials. Wear. 154:1992;371-385.
    • (1992) Wear , vol.154 , pp. 371-385
    • Ajayi, O.O.1    Ludema, K.C.2
  • 3
    • 0029378554 scopus 로고
    • Characterization of microstructural defects in plasma-sprayed thermal barrier coatings
    • Bengtsson P., Johannesson T. Characterization of microstructural defects in plasma-sprayed thermal barrier coatings. Journal of Thermal Spray Technology. 4(3):1995;245-251.
    • (1995) Journal of Thermal Spray Technology , vol.4 , Issue.3 , pp. 245-251
    • Bengtsson, P.1    Johannesson, T.2
  • 4
    • 17744404643 scopus 로고    scopus 로고
    • The microstructural dependence of wear and indentation behaviour of some plasma-sprayed alumina coatings
    • Hawthorne H.M., Erickson L.C., Ross D., Tai H., Troczynski T. The microstructural dependence of wear and indentation behaviour of some plasma-sprayed alumina coatings. Wear. 203-204:1997;709-714.
    • (1997) Wear , vol.203-204 , pp. 709-714
    • Hawthorne, H.M.1    Erickson, L.C.2    Ross, D.3    Tai, H.4    Troczynski, T.5
  • 6
    • 0343895853 scopus 로고    scopus 로고
    • Processing-dependent microstructure and wear-related surface properties of plasma-sprayed alumina coatings
    • 8-12 September London, Abstracts of Papers, MEP, London, in press
    • L.C. Erickson, T. Troczynski, D. Ross, H. Tai, H.M. Hawthorne, Processing-dependent microstructure and wear-related surface properties of plasma-sprayed alumina coatings, Presented to the World Tribology Congress, 8-12 September 1997, London, Abstracts of Papers, MEP, London, p. 146, in press.
    • (1997) Presented to the World Tribology Congress , pp. 146
    • Erickson, L.C.1    Troczynski, T.2    Ross, D.3    Tai, H.4    Hawthorne, H.M.5
  • 7
    • 0042168889 scopus 로고
    • Relationship between wear and microstructures of ceramic spray coatings
    • ASM, Metals Park, OH
    • K. Furukuba, S. Oki, S. Gohda, Relationship between wear and microstructures of ceramic spray coatings, Advances in Coatings Technology, ASM, Metals Park, OH, 1992, pp. 705-709.
    • (1992) Advances in Coatings Technology , pp. 705-709
    • Furukuba, K.1    Oki, S.2    Gohda, S.3
  • 8
    • 0342590221 scopus 로고
    • Abrasive and erosive wear of thermally sprayed ceramic and cermet coatings
    • in: H.M. Hawthorne, T. Troczynski (Eds.), CIM, Montreal
    • T.A. Mantyla, K. Niemi, P. Vuoristo, Abrasive and erosive wear of thermally sprayed ceramic and cermet coatings, in: H.M. Hawthorne, T. Troczynski (Eds.), Advanced Ceramics for Structural and Tribological Applications, CIM, Montreal, 1995, pp. 483-494.
    • (1995) Advanced Ceramics for Structural and Tribological Applications , pp. 483-494
    • Mantyla, T.A.1    Niemi, K.2    Vuoristo, P.3
  • 9
    • 0024082428 scopus 로고
    • Study of the surface cracking of alumina scratched by single-point diamonds
    • Bi Z., Tokura H., Yoshikawa M. Study of the surface cracking of alumina scratched by single-point diamonds. Journal of Materials Science. 23:1988;3214-3224.
    • (1988) Journal of Materials Science , vol.23 , pp. 3214-3224
    • Bi, Z.1    Tokura, H.2    Yoshikawa, M.3
  • 10
    • 0029290824 scopus 로고
    • Effect of grain size on scratch interactions and material removal in alumina
    • Xu H.H.K., Jahanmir S., Wang Y. Effect of grain size on scratch interactions and material removal in alumina. Journal of The American Ceramic Society. 78(4):1995;881-891.
    • (1995) Journal of the American Ceramic Society , vol.78 , Issue.4 , pp. 881-891
    • Xu, H.H.K.1    Jahanmir, S.2    Wang, Y.3
  • 11
    • 0031187556 scopus 로고    scopus 로고
    • Correlations between tangential force and damage mechanisms in the scratch testing of ceramics
    • Axen N., Kahlman L., Hutchings I.M. Correlations between tangential force and damage mechanisms in the scratch testing of ceramics. Tribology International. 30(7):1997;467-474.
    • (1997) Tribology International , vol.30 , Issue.7 , pp. 467-474
    • Axen, N.1    Kahlman, L.2    Hutchings, I.M.3
  • 14
    • 0030549334 scopus 로고    scopus 로고
    • Analytical models of scratch hardness
    • Williams J.A. Analytical models of scratch hardness. Tribology International. 29(8):1996;675-694.
    • (1996) Tribology International , vol.29 , Issue.8 , pp. 675-694
    • Williams, J.A.1
  • 15
  • 17
    • 0029336352 scopus 로고
    • Measurement of plastic strain below an indentation and piling-up between two adjacent indentations
    • Oka Y.I., Matsumura M., Funaki H. Measurement of plastic strain below an indentation and piling-up between two adjacent indentations. Wear. 186-187:1995;50-55.
    • (1995) Wear , vol.186-187 , pp. 50-55
    • Oka, Y.I.1    Matsumura, M.2    Funaki, H.3
  • 19
    • 34249753644 scopus 로고
    • Microstructure and material removal in scratching of alumina
    • Xu H.H.K., Jahanmir S. Microstructure and material removal in scratching of alumina. Journal of Material Science. 30:1995;2235-2247.
    • (1995) Journal of Material Science , vol.30 , pp. 2235-2247
    • Xu, H.H.K.1    Jahanmir, S.2
  • 21
    • 4244025922 scopus 로고    scopus 로고
    • Wear mechanism of plasma-sprayed alumina coating in sliding contacts with harder asperities
    • Submitted for Presentation to the Atlanta, USA, 25-29 April submitted for publication
    • Y. Xie, H.M. Hawthorne, Wear mechanism of plasma-sprayed alumina coating in sliding contacts with harder asperities, Submitted for Presentation to the 12th International Conference on Wear of Materials, Atlanta, USA, 25-29 April 1999, Wear, submitted for publication.
    • (1999) 12th International Conference on Wear of Materials
    • Xie, Y.1    Hawthorne, H.M.2
  • 22
    • 0023541001 scopus 로고
    • Indentation toughness testing of plasma-sprayed coatings
    • Ostojic P., McPherson R. Indentation toughness testing of plasma-sprayed coatings. Materials Forum. 10(4):1987;247-255.
    • (1987) Materials Forum , vol.10 , Issue.4 , pp. 247-255
    • Ostojic, P.1    McPherson, R.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.