메뉴 건너뛰기




Volumn 82, Issue 8, 1999, Pages 2269-2272

Sandwiched-beam procedure for precracking brittle materials

Author keywords

[No Author keywords available]

Indexed keywords

BENDING MOMENTS; CRACK INITIATION; CRACK PROPAGATION; ELASTIC MODULI; FRACTURE TOUGHNESS; LOADS (FORCES); MATERIALS TESTING; MATERIALS TESTING APPARATUS; STRESS INTENSITY FACTORS;

EID: 0033355952     PISSN: 00027820     EISSN: None     Source Type: Journal    
DOI: 10.1111/j.1151-2916.1999.tb02077.x     Document Type: Article
Times cited : (19)

References (42)
  • 1
    • 0024048393 scopus 로고
    • Comparison of the fracture toughness of alumina measured by three different methods
    • P. Lamaitre and R. Piller, "Comparison of the Fracture Toughness of Alumina Measured by Three Different Methods," J. Mater. Sci. Lett., 7, 772-74 (1988).
    • (1988) J. Mater. Sci. Lett. , vol.7 , pp. 772-774
    • Lamaitre, P.1    Piller, R.2
  • 2
    • 0028498251 scopus 로고
    • The fracture toughness of a high-strength alumina: Compact tension versus indentation fracture techniques
    • B. R. Murphy, W. W. Predebon, and B. J. Pletka, "The Fracture Toughness of a High-Strength Alumina: Compact Tension versus Indentation Fracture Techniques," J. Mater. Sci. Lett., 13, 1346-48 (1994).
    • (1994) J. Mater. Sci. Lett. , vol.13 , pp. 1346-1348
    • Murphy, B.R.1    Predebon, W.W.2    Pletka, B.J.3
  • 3
    • 0028382852 scopus 로고
    • Flat R-curve from stable propagation of indentation cracks in coarse-grained alumina
    • D. Bleise and R. W. Steinbrech, "Flat R-Curve from Stable Propagation of Indentation Cracks in Coarse-Grained Alumina," J. Am. Ceram. Soc., 77 [2] 315-22 (1994).
    • (1994) J. Am. Ceram. Soc. , vol.77 , Issue.2 , pp. 315-322
    • Bleise, D.1    Steinbrech, R.W.2
  • 4
    • 0028422032 scopus 로고
    • Crack-growth resistance of in situ-toughened silicon nitride
    • S. R. Choi and J. A. Salem, "Crack-Growth Resistance of in Situ-Toughened Silicon Nitride," J. Am. Ceram. Soc., 77 [4] 1042-46 (1994).
    • (1994) J. Am. Ceram. Soc. , vol.77 , Issue.4 , pp. 1042-1046
    • Choi, S.R.1    Salem, J.A.2
  • 5
    • 0003068736 scopus 로고    scopus 로고
    • R-curve measurement of alumina using straight notched or indented bending bars
    • Edited by R. C. Bradt, D. P. H. Hasselman, D. Munz, M. Sakai, and V. Ya. Schevchenko. Plenum Press, New York
    • S. Sakaguci, "R-Curve Measurement of Alumina Using Straight Notched or Indented Bending Bars"; pp. 39-51 in Fracture Mechanics of Ceramics, Vol. 11. Edited by R. C. Bradt, D. P. H. Hasselman, D. Munz, M. Sakai, and V. Ya. Schevchenko. Plenum Press, New York, 1996.
    • (1996) Fracture Mechanics of Ceramics , vol.11 , pp. 39-51
    • Sakaguci, S.1
  • 8
    • 0029778616 scopus 로고    scopus 로고
    • Determination of short-crack toughness curves
    • S. M. Smith and R. O. Scattergood, "Determination of Short-Crack Toughness Curves," J. Am. Ceram. Soc., 79 [1] 129-36 (1996).
    • (1996) J. Am. Ceram. Soc. , vol.79 , Issue.1 , pp. 129-136
    • Smith, S.M.1    Scattergood, R.O.2
  • 9
    • 0012974958 scopus 로고    scopus 로고
    • Standard test method for plane-strain fracture toughness of metallic materials
    • Vol. 03.01, American Society for Testing and Materials, Philadelphia, PA
    • "Standard Test Method for Plane-Strain Fracture Toughness of Metallic Materials," ASTM Designation E 399-90, 1991 Annual Book of ASTM Standards, Vol. 03.01, pp. 412-42. American Society for Testing and Materials, Philadelphia, PA.
    • ASTM Designation E 399-90, 1991 Annual Book of ASTM Standards , pp. 412-442
  • 11
    • 0343325401 scopus 로고    scopus 로고
    • VAMAS round robin on fracture toughness measurement of ceramic matrix composite
    • Japan Fine Ceramics Center, Nagoya, Japan
    • "VAMAS Round Robin on Fracture Toughness Measurement of Ceramic Matrix Composite," Final Report, Japan Fine Ceramics Center, Nagoya, Japan, 1997.
    • (1997) Final Report
  • 12
  • 13
    • 0000327659 scopus 로고
    • Objective evaluation of short crack toughness curves using indentation flaws: Case study on alumina-based ceramics
    • L. M. Braun, S. J. Bennison, and B. R. Lawn, "Objective Evaluation of Short Crack Toughness Curves using Indentation Flaws: Case Study on Alumina-Based Ceramics," J. Am. Ceram. Soc., 75 [11] 3049-57 (1992).
    • (1992) J. Am. Ceram. Soc. , vol.75 , Issue.11 , pp. 3049-3057
    • Braun, L.M.1    Bennison, S.J.2    Lawn, B.R.3
  • 14
    • 0030084086 scopus 로고    scopus 로고
    • Method for measuring short-crack R-curves without calibration parameters: Case studies on alumina and alumina/aluminum composites
    • M. Stech and J. Rödel, "Method for Measuring Short-Crack R-Curves without Calibration Parameters: Case Studies on Alumina and Alumina/Aluminum Composites," J. Am. Ceram. Soc., 79 [2] 291-97 (1996).
    • (1996) J. Am. Ceram. Soc. , vol.79 , Issue.2 , pp. 291-297
    • Stech, M.1    Rödel, J.2
  • 15
    • 0031339892 scopus 로고    scopus 로고
    • Crack decorating technique for fracture-toughness measurement in alumina
    • V. M. Sglavo and P. Pancheri, "Crack Decorating Technique for Fracture-Toughness Measurement in Alumina," J. Eur. Ceram. Soc., 17 [14] 1697-706 (1997).
    • (1997) J. Eur. Ceram. Soc. , vol.17 , Issue.14 , pp. 1697-1706
    • Sglavo, V.M.1    Pancheri, P.2
  • 16
    • 0024016154 scopus 로고
    • Evaluation of fracture toughness for ceramic materials by a single-edge-precracked-beam method
    • T. Nose and T. Fujii, "Evaluation of Fracture Toughness for Ceramic Materials by a Single-Edge-Precracked-Beam Method," J. Am. Ceram. Soc., 71 [5] 328-33 (1988).
    • (1988) J. Am. Ceram. Soc. , vol.71 , Issue.5 , pp. 328-333
    • Nose, T.1    Fujii, T.2
  • 18
    • 0019632938 scopus 로고
    • Crack stability in the work-of-fracture test: Refractory applications
    • J. Nakayama, H. Abe, and R. C. Bradt, "Crack Stability in the Work-of-Fracture Test: Refractory Applications," J. Am. Ceram. Soc., 64 [11] 671-75 (1981).
    • (1981) J. Am. Ceram. Soc. , vol.64 , Issue.11 , pp. 671-675
    • Nakayama, J.1    Abe, H.2    Bradt, R.C.3
  • 19
    • 0024619714 scopus 로고
    • Dimensionless load-displacement relation and its application to crack propagation problems
    • M. Sakai and M. Inagaki, "Dimensionless Load-Displacement Relation and Its Application to Crack Propagation Problems," J. Am. Ceram. Soc., 72 [3] 388-94 (1989).
    • (1989) J. Am. Ceram. Soc. , vol.72 , Issue.3 , pp. 388-394
    • Sakai, M.1    Inagaki, M.2
  • 20
    • 0030242990 scopus 로고    scopus 로고
    • Crack stability and its effect on fracture toughness of hot-pressed silicon nitride beam specimens
    • I. Bar-On, F. I. Baratta, and K. Cho, "Crack Stability and Its Effect on Fracture Toughness of Hot-Pressed Silicon Nitride Beam Specimens," J. Am. Ceram. Soc., 79 [9] 2300-308 (1996).
    • (1996) J. Am. Ceram. Soc. , vol.79 , Issue.9 , pp. 2300-2308
    • Bar-On, I.1    Baratta, F.I.2    Cho, K.3
  • 23
    • 0032010589 scopus 로고    scopus 로고
    • Production of sharp cracks in ceramic materials by three-point bending of sandwiched specimens
    • P. Pancheri, P. Bosetti, R. Dal. Maschio, and V. M. Sglavo, "Production of Sharp Cracks in Ceramic Materials by Three-Point Bending of Sandwiched Specimens," Eng. Fract. Mech., 59 [4] 447-56 (1998).
    • (1998) Eng. Fract. Mech. , vol.59 , Issue.4 , pp. 447-456
    • Pancheri, P.1    Bosetti, P.2    Dal Maschio, R.3    Sglavo, V.M.4
  • 24
    • 11544372348 scopus 로고
    • Wide range stress intensity factor expression for ASTM E399 standard fracture toughness specimens
    • J. E. Srawley, "Wide Range Stress Intensity Factor Expression for ASTM E399 Standard Fracture Toughness Specimens," Int. J. Fract., 12, 475-76 (1976).
    • (1976) Int. J. Fract. , vol.12 , pp. 475-476
    • Srawley, J.E.1
  • 26
    • 0039540337 scopus 로고    scopus 로고
    • Standard test method for dynamic young's modulus, shear modulus and poisson's ratio for advanced ceramics by sonic resonance
    • Vol. 15.01, American Society for Testing and Materials, Philadelphia, PA
    • "Standard Test Method for Dynamic Young's Modulus, Shear Modulus and Poisson's Ratio for Advanced Ceramics by Sonic Resonance," ASTM Designation Cl198-91, 199 Annual Book of ASTM Standards, Vol. 15.01, pp. 332-38. American Society for Testing and Materials, Philadelphia, PA.
    • ASTM Designation Cl198-91, 199 Annual Book of ASTM Standards , pp. 332-338
  • 27
    • 0029270958 scopus 로고
    • Strength and fatigue of silicate glass
    • V. M. Sglavo and D. J. Green, "Strength and Fatigue of Silicate Glass," Acta Metall. Mater., 43 [3] 965-72 (1995).
    • (1995) Acta Metall. Mater. , vol.43 , Issue.3 , pp. 965-972
    • Sglavo, V.M.1    Green, D.J.2
  • 28
    • 84977250775 scopus 로고
    • Fracture surface energy of glass
    • S. M. Wiederhorn, "Fracture Surface Energy of Glass," J. Am. Ceram. Soc., 52 [2] 99-105 (1969).
    • (1969) J. Am. Ceram. Soc. , vol.52 , Issue.2 , pp. 99-105
    • Wiederhorn, S.M.1
  • 29
    • 84959610090 scopus 로고
    • Crack resistance by interfacial bridgings: Its role in determining strength characteristics
    • R. F. Cook, C. J. Fairbanks, B. R. Lawn, and Y.-W. Mai, "Crack Resistance by Interfacial Bridgings: Its Role in Determining Strength Characteristics," J. Mater. Res., 2 [3] 345-56 (1987).
    • (1987) J. Mater. Res. , vol.2 , Issue.3 , pp. 345-356
    • Cook, R.F.1    Fairbanks, C.J.2    Lawn, B.R.3    Mai, Y.-W.4
  • 30
    • 0024063867 scopus 로고
    • R-curve behavior of a polycrystalline graphite: Microcracking and grain bridging in the wake region
    • M. Sakai, J.-I. Yoshimura, Y. Goto, and M. Inagaki, "R-Curve Behavior of a Polycrystalline Graphite: Microcracking and Grain Bridging in the Wake Region," J. Am. Ceram. Soc., 71 [8] 609-16 (1988).
    • (1988) J. Am. Ceram. Soc. , vol.71 , Issue.8 , pp. 609-616
    • Sakai, M.1    Yoshimura, J.-I.2    Goto, Y.3    Inagaki, M.4
  • 31
    • 0024014520 scopus 로고
    • Crack-resistance curves of surface cracks in alumina
    • R. W. Steinbrech and O. Schmenkel, "Crack-Resistance Curves of Surface Cracks in Alumina," J. Am. Ceram. Soc., 71 [5] C-271-C-273 (1988).
    • (1988) J. Am. Ceram. Soc. , vol.71 , Issue.5
    • Steinbrech, R.W.1    Schmenkel, O.2
  • 33
    • 0025477859 scopus 로고
    • Role of grain size in the strength and R-curve properties of alumina
    • P. Chantikul, S. J. Bennison, and B. R. Lawn, "Role of Grain Size in the Strength and R-Curve Properties of Alumina," J. Am. Ceram. Soc., 73 [8] 2419-27 (1990).
    • (1990) J. Am. Ceram. Soc. , vol.73 , Issue.8 , pp. 2419-2427
    • Chantikul, P.1    Bennison, S.J.2    Lawn, B.R.3
  • 35
    • 0027801798 scopus 로고
    • Fracture behavior of chemically-vapor-deposited SiC-coated graphite: I, experimental results
    • T. R. Watkins and D. J. Green, "Fracture Behavior of Chemically-Vapor-Deposited SiC-Coated Graphite: I, Experimental Results," J. Am. Ceram. Soc., 76 [12] 3066-72 (1993).
    • (1993) J. Am. Ceram. Soc. , vol.76 , Issue.12 , pp. 3066-3072
    • Watkins, T.R.1    Green, D.J.2
  • 37
    • 0030401342 scopus 로고    scopus 로고
    • Short-crack toughness and abrasive machining of silicon nitride
    • H. H. K. Xu, S. Jahanmir, L. K. Ives, L. S. Job, and K. T. Ritchie, "Short-Crack Toughness and Abrasive Machining of Silicon Nitride," J. Am. Ceram. Soc., 79 [12] 3055-64 (1996).
    • (1996) J. Am. Ceram. Soc. , vol.79 , Issue.12 , pp. 3055-3064
    • Xu, H.H.K.1    Jahanmir, S.2    Ives, L.K.3    Job, L.S.4    Ritchie, K.T.5
  • 38
    • 0029713117 scopus 로고    scopus 로고
    • Tensile properties and fracture toughness of TiAl alloys with controlled microstructures
    • C. T. Liu, J. H. Schneibel, P. J. Mazias, J. L. Wright, and D. S. Easton, "Tensile Properties and Fracture Toughness of TiAl Alloys with Controlled Microstructures," Intermetallics, 4 [6] 429-40 (1996).
    • (1996) Intermetallics , vol.4 , Issue.6 , pp. 429-440
    • Liu, C.T.1    Schneibel, J.H.2    Mazias, P.J.3    Wright, J.L.4    Easton, D.S.5
  • 39
    • 0028383043 scopus 로고
    • Effect of notch-root radius on the fracture toughness of a fine-grained alumina
    • T. Nishida, Y. Hanaki, and G. Pezzotti, "Effect of Notch-Root Radius on the Fracture Toughness of a Fine-Grained Alumina," J. Am. Ceram. Soc., 77 [2] 606-608 (1994).
    • (1994) J. Am. Ceram. Soc. , vol.77 , Issue.2 , pp. 606-608
    • Nishida, T.1    Hanaki, Y.2    Pezzotti, G.3
  • 40
    • 0031333746 scopus 로고    scopus 로고
    • Polished notch modification of SENB-S fracture toughness testing
    • R. J. Damani, C. Schuster, and R. Danzer, "Polished Notch Modification of SENB-S Fracture Toughness Testing," J. Eur. Ceram. Soc., 17 [14] 1685-89 (1997).
    • (1997) J. Eur. Ceram. Soc. , vol.17 , Issue.14 , pp. 1685-1689
    • Damani, R.J.1    Schuster, C.2    Danzer, R.3
  • 41
    • 0032678726 scopus 로고    scopus 로고
    • Fracture toughness of high purity alumina at room and elevated temperature
    • in press
    • V. M. Sglavo, E. Trentini, and M. Boniecki, "Fracture Toughness of High Purity Alumina at Room and Elevated Temperature," J. Mater. Sci. Lett., in press.
    • J. Mater. Sci. Lett.
    • Sglavo, V.M.1    Trentini, E.2    Boniecki, M.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.