Volumn 43, Issue 1, 1999, Pages 27-32

Strength degradation of a tungsten carbide-cobalt composite at elevated temperatures

Author keywords

[No Author keywords available]

Indexed keywords

ADDITION REACTIONS; BENDING STRENGTH; CARBIDE CUTTING TOOLS; COBALT; CRACK PROPAGATION; DEGRADATION; FRACTURE MECHANICS; FRACTURE TOUGHNESS; HARDNESS; HIGH TEMPERATURE EFFECTS; OXIDATION; STRUCTURAL ANALYSIS;

EID: 0033349209     PISSN: 10445803     EISSN: None     Source Type: Journal    
DOI: 10.1016/S1044-5803(98)00056-4     Document Type: Article
Times cited : (89)

References (14)
  • 1
    • 0011750162 scopus 로고
    • Fracture characteristics of ceramic and cermet cutting tools
    • Dusza J., Parilak L., Slesar M. Fracture characteristics of ceramic and cermet cutting tools. Ceram. Int. 13(3):1987;133-137.
    • (1987) Ceram. Int. , vol.13 , Issue.3 , pp. 133-137
    • Dusza, J.1    Parilak, L.2    Slesar, M.3
  • 2
    • 0024682141 scopus 로고
    • Liquid-phase sintering of carbides using a nickel-molybdenum alloy
    • Barranco J.M., Warenchak R.A. Liquid-phase sintering of carbides using a nickel-molybdenum alloy. Int. J. Refract. Met. Hard. Mater. 6:1989;102-110.
    • (1989) Int. J. Refract. Met. Hard. Mater. , vol.6 , pp. 102-110
    • Barranco, J.M.1    Warenchak, R.A.2
  • 4
    • 0017007806 scopus 로고
    • Fracture toughness and failure of WC-Co composites
    • Chermant J.L., Osterstock F. Fracture toughness and failure of WC-Co composites. J. Mater. Sci. 11:1976;1939-1951.
    • (1976) J. Mater. Sci. , vol.11 , pp. 1939-1951
    • Chermant, J.L.1    Osterstock, F.2
  • 6
  • 7
    • 0342638152 scopus 로고
    • Fracture analysis of cobalt-bonded tungsten carbide composites
    • Han D., Mecholsky J.J. Fracture analysis of cobalt-bonded tungsten carbide composites. J. Mater. Sci. 25:1990;4949-4956.
    • (1990) J. Mater. Sci. , vol.25 , pp. 4949-4956
    • Han, D.1    Mecholsky, J.J.2
  • 8
    • 0006443096 scopus 로고
    • Sintering of submicron tungsten carbide-10wt % cobalt hard metals containing nickel and iron
    • Upadhyaya G.S., Bhaumik S.K. Sintering of submicron tungsten carbide-10wt % cobalt hard metals containing nickel and iron. Mater. Sci. Eng. A105-A106:1988;249-256.
    • (1988) Mater. Sci. Eng. , vol.105-106 , pp. 249-256
    • Upadhyaya, G.S.1    Bhaumik, S.K.2
  • 9
    • 0026155633 scopus 로고
    • SEM study of the fracture behavior of some WC-based cemented carbides
    • Bhaumik S.K., Upadhyaya G.S., Vaidya L.M. SEM study of the fracture behavior of some WC-based cemented carbides. Pract. Met. 28:1991;238-249.
    • (1991) Pract. Met. , vol.28 , pp. 238-249
    • Bhaumik, S.K.1    Upadhyaya, G.S.2    Vaidya, L.M.3
  • 14
    • 0017023263 scopus 로고
    • Thermal-shock resistance and fracture-strength behavior of two tool carbides
    • Mai Y.W. Thermal-shock resistance and fracture-strength behavior of two tool carbides. J. Amer. Ceram. Soc. 59:1976;491-494.
    • (1976) J. Amer. Ceram. Soc. , vol.59 , pp. 491-494
    • Mai, Y.W.1


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.