Volumn 6, Issue 5, 1999, Pages 620-631

Review of aging and recovery of silicone rubber insulation for outdoor use

Author keywords

[No Author keywords available]

Indexed keywords

AGING OF MATERIALS; ELECTRIC CORONA; HYDROPHOBICITY; RUBBER; SILICONES;

EID: 0033336962     PISSN: 10709878     EISSN: None     Source Type: Journal    
DOI: 10.1109/94.798119     Document Type: Article
Times cited : (176)

References (78)
  • 1
    • 0010116794 scopus 로고
    • Field experience and testing of new insulator types in South Africa
    • Paris, August paper 22-03
    • H. Weihe, J. P. Reynders, R. E. Macey, "Field experience and testing of new insulator types in South Africa", Cigré Session, Paris, August 1980, paper 22-03.
    • (1980) Cigré Session
    • Weihe, H.1    Reynders, J.P.2    Macey, R.E.3
  • 2
    • 33749906732 scopus 로고    scopus 로고
    • The design of Silicone Rubber insulation to minimize surface aging influences
    • Zagreb, September paper P39
    • J. P. Reynders, S. M. Reynders, "The design of Silicone Rubber insulation to minimize surface aging influences", Cigré International Symposium, Zagreb, September 1998, paper P39.
    • (1998) Cigré International Symposium
    • Reynders, J.P.1    Reynders, S.M.2
  • 4
    • 6244255085 scopus 로고
    • Evaluation of the condition of non-ceramic insulators after long-term operation under service conditions
    • J. Kindersberger, M. Kuhl, R. Barsch, "Evaluation of the condition of non-ceramic insulators after long-term operation under service conditions", 9th ISH Graz 1995, pp. 3193-1 to 3193-4.
    • (1995) 9th ISH Graz , pp. 31931-31934
    • Kindersberger, J.1    Kuhl, M.2    Barsch, R.3
  • 5
    • 33749914339 scopus 로고
    • Review of Cigré and IEEE Research into Pollution Performance of Non-ceramic Insulators: Field Aging Effects and Laboratory Test Techniques
    • Paris, paper 33-103
    • G. G. Karady, H. M. Schneider, F. A. M. Rizk, "Review of Cigré and IEEE Research into Pollution Performance of Non-ceramic Insulators: Field Aging Effects and Laboratory Test Techniques", Cigré Technical Session 1994, Paris, paper 33-103.
    • (1994) Cigré Technical Session
    • Karady, G.G.1    Schneider, H.M.2    Rizk, F.A.M.3
  • 8
    • 0028593201 scopus 로고
    • Laboratory Analysis of Naturally Aged Silicone Rubber Polymer Insulators from Contaminated Environments, 138 to 765 kV
    • April
    • R. J. Hill, "Laboratory Analysis of Naturally Aged Silicone Rubber Polymer Insulators from Contaminated Environments, 138 to 765 kV". Presented at IEEE Power Engineering Society Transmission and Distribution Conference April 1994.
    • (1994) IEEE Power Engineering Society Transmission and Distribution Conference
    • Hill, R.J.1
  • 10
    • 0026880858 scopus 로고
    • Hydrophobic Behavior of Insulators coated with RTV Silicone Rubber
    • June
    • S. H. Kim, E. A. Cherney, R. Hackman, "Hydrophobic Behavior of Insulators coated with RTV Silicone Rubber", IEEE Transactions on Electrical Insulation Vol.27 No. 3, June 1992, pp. 610-622.
    • (1992) IEEE Transactions on Electrical Insulation , vol.27 , Issue.3 , pp. 610-622
    • Kim, S.H.1    Cherney, E.A.2    Hackman, R.3
  • 11
    • 33749940863 scopus 로고    scopus 로고
    • fax communication (05-11-1997), Wacker Chemie GmbH, Hans-Seidel-Platz 4, D-81737 M'unchen
    • H. J. Winter, fax communication (05-11-1997), Wacker Chemie GmbH, Hans-Seidel-Platz 4, D-81737 M'unchen.
    • Winter, H.J.1
  • 12
    • 0028426016 scopus 로고
    • Oxidative Damage and Recovery of Silicone Rubber Surfaces. I. X-ray Photoelectron Spectroscopic Study
    • John Wiley and Sons Inc
    • A. Toth, I. Bertoti, M. Blazso, G. Banhegyi, A. Bognar, P. Szaplonczay, "Oxidative Damage and Recovery of Silicone Rubber Surfaces. I. X-ray Photoelectron Spectroscopic Study", Journal of Applied Polymer Science, Vol 52, John Wiley and Sons Inc, 1994, pp. 1293-1307.
    • (1994) Journal of Applied Polymer Science , vol.52 , pp. 1293-1307
    • Toth, A.1    Bertoti, I.2    Blazso, M.3    Banhegyi, G.4    Bognar, A.5    Szaplonczay, P.6
  • 13
    • 0003604096 scopus 로고    scopus 로고
    • Service Performance, Material Design and Applications of Composite Insulators with Silicone Rubber Housings
    • paper 33-303
    • J. Kindersberger, A. Schultz, H. C. Kärner, R. van de Huir, "Service Performance, Material Design and Applications of Composite Insulators with Silicone Rubber Housings", Cigré Session 1996, paper 33-303.
    • (1996) Cigré Session
    • Kindersberger, J.1    Schultz, A.2    Kärner, H.C.3    Van De Huir, R.4
  • 18
    • 33749950746 scopus 로고    scopus 로고
    • Tracking Degradation of Silicon Rubber
    • Montréal
    • N. Fujioka, S. Ohgaki, "Tracking Degradation of Silicon Rubber", ISH'97, Montréal, 1997, pp. 69-72.
    • (1997) ISH'97 , pp. 69-72
    • Fujioka, N.1    Ohgaki, S.2
  • 19
    • 33747438222 scopus 로고
    • The Loss and Recovery of Hydrophobicity of RTV Silicone Rubber Insulator Coatings
    • July
    • S. H. Kim, E. A. Cherney, R. Hackman, "The Loss and Recovery of Hydrophobicity of RTV Silicone Rubber Insulator Coatings", IEEE Transactions on Power Delivery, Vol 5, No. 3, July 1990, pp. 1491-1499.
    • (1990) IEEE Transactions on Power Delivery , vol.5 , Issue.3 , pp. 1491-1499
    • Kim, S.H.1    Cherney, E.A.2    Hackman, R.3
  • 20
    • 0026238254 scopus 로고
    • Contamination performance of Silicone Rubber Cable Terminations
    • October
    • R. S. Gorur, L. A. Johnson, H. C. Hervig, "Contamination performance of Silicone Rubber Cable Terminations", IEEE Transactions on Power Delivery, Vol. 6, No. 4, October 1991, pp. 1366-1370.
    • (1991) IEEE Transactions on Power Delivery , vol.6 , Issue.4 , pp. 1366-1370
    • Gorur, R.S.1    Johnson, L.A.2    Hervig, H.C.3
  • 22
    • 0002918137 scopus 로고    scopus 로고
    • The Loss and Recovery of Hydrophobicity on Silicone Rubber Surfaces
    • H. Janssen, A. Herden, H. C. Kärner," The Loss and Recovery of Hydrophobicity on Silicone Rubber Surfaces", ISH'97 Montréal, pp. 145-148.
    • ISH'97 Montréal , pp. 145-148
    • Janssen, H.1    Herden, A.2    Kärner, H.C.3
  • 23
    • 0141932243 scopus 로고    scopus 로고
    • Laboratory wet Tests on Artificially contaminated Non-ceramic and Ceramic Insulators
    • A. de la O, R. S. Gorur, J. T. Burham, "Laboratory wet Tests on Artificially contaminated Non-ceramic and Ceramic Insulators", ISH'97 Montréal, pp. 61-63.
    • ISH'97 Montréal , pp. 61-63
    • De La O, A.1    Gorur, R.S.2    Burham, J.T.3
  • 25
    • 33749958569 scopus 로고
    • Natural and Artificial Aging of Non Ceramic Insulators, Evaluation of Techniques
    • G. Riquel, J. M. Fourmigue, M. Noel, D. de Decker, R. Parraud, "Natural and Artificial Aging of Non Ceramic Insulators, Evaluation Of Techniques", 9th ISH Graz 1995, pp. 3188-1 to 3188-4.
    • (1995) 9th ISH Graz , pp. 31881-31884
    • Riquel, G.1    Fourmigue, J.M.2    Noel, M.3    De Decker, D.4    Parraud, R.5
  • 26
  • 29
    • 33749923200 scopus 로고
    • Laboratory Comparative Tests on Composite Insulators
    • V. Sklenička, J. Vokálek, "Laboratory Comparative Tests on Composite Insulators", 9th ISH Graz 1995, pp. 3182-1 to 3182-4.
    • (1995) 9th ISH Graz , pp. 31821-31824
    • Sklenička, V.1    Vokálek, J.2
  • 30
    • 33749897201 scopus 로고    scopus 로고
    • Contamination Withstand Voltage Characteristics of Polymer Insulators
    • R. Matsuoka, S. Ito, K. Tanaka, K. Kondo, "Contamination Withstand Voltage Characteristics of Polymer Insulators", ISH'97 Montréal, pp. 81-84.
    • ISH'97 Montréal , pp. 81-84
    • Matsuoka, R.1    Ito, S.2    Tanaka, K.3    Kondo, K.4
  • 31
    • 33749877467 scopus 로고
    • Koeberg Insulator Pollution Test Station (KIPTS)
    • W. L. Vosloo, J. P. Holtzhausen, "Koeberg Insulator Pollution Test Station (KIPTS)", 9th ISH Graz 1995, pp. 3228-1 to 3228.
    • (1995) 9th ISH Graz
    • Vosloo, W.L.1    Holtzhausen, J.P.2
  • 32
    • 84883002756 scopus 로고
    • On the Valuation of the Early Aging Period of Polymer Insulator Surfaces during Accelerated Aging Tests
    • R. Barsch, J. Lambrecht, H. J. Winter, "On the Valuation of the Early Aging Period of Polymer Insulator Surfaces During Accelerated Aging Tests", 9th ISH Graz, 1995, pp. 3023-1 to 3023-4.
    • (1995) 9th ISH Graz , pp. 30231-30234
    • Barsch, R.1    Lambrecht, J.2    Winter, H.J.3
  • 33
    • 33749953684 scopus 로고    scopus 로고
    • Salt Fog Aging Evaluation of EPDM and EPDM/Silicone Alloy Non-ceramic Insulators
    • T. Zhao, J. D. Sakich, R. K. Niedermier, "Salt Fog Aging Evaluation of EPDM and EPDM/Silicone Alloy Non-ceramic Insulators", ISH'97 Montréal, pp. 215-218.
    • ISH'97 Montréal , pp. 215-218
    • Zhao, T.1    Sakich, J.D.2    Niedermier, R.K.3
  • 35
    • 25044467797 scopus 로고
    • Surface Aging and its Impact on the Performance of Polymeric Insulators
    • T. Sorqvist, T. Karlsson, A. E. Vlastos, "Surface Aging and its Impact on the Performance of Polymeric Insulators", 9th ISH Graz 1995, pp. 3234-1 to 3234-4.
    • (1995) 9th ISH Graz , pp. 32341-32344
    • Sorqvist, T.1    Karlsson, T.2    Vlastos, A.E.3
  • 36
    • 33749954686 scopus 로고
    • Clean Fog Flashover Testing of Non-Ceramic Insulating Materials
    • Graz
    • A. Lavalle de La O, R. S. Gorur, "Clean Fog Flashover Testing of Non-Ceramic Insulating Materials", 9th ISH, Graz, 1995, pp. 3566-1 to 3566-4.
    • (1995) 9th ISH , pp. 35661-35664
    • Lavalle De La O, A.1    Gorur, R.S.2
  • 37
    • 84863352423 scopus 로고    scopus 로고
    • Performance of Composite Insulators under Polluted Conditions
    • Paris, paper 33-301
    • K. Naito, K. Izumi, K. Takusu, R. Matsuoka, "Performance of Composite Insulators under Polluted Conditions", Cigré Session, Paris, 1996, paper 33-301.
    • (1996) Cigré Session
    • Naito, K.1    Izumi, K.2    Takusu, K.3    Matsuoka, R.4
  • 38
    • 0030315896 scopus 로고    scopus 로고
    • Surface Conductivity as an Indication of the surface condition of Non-Ceramic Insulators
    • Stellenbosch 24-27 September
    • L. Van Wyk, J. P. Holtzhausen, W. L. Vosloo, "Surface Conductivity as an Indication of the surface condition of Non-Ceramic Insulators", IEEE Africon'96 Stellenbosch 24-27 September 1997 pp485-488.
    • (1997) IEEE Africon'96 , pp. 485-488
    • Van Wyk, L.1    Holtzhausen, J.P.2    Vosloo, W.L.3
  • 39
    • 33749894867 scopus 로고
    • Effects of Electrohydrodynamic Processes in Droplet Layers to Partial Discharges and Leakage Current and their use for a sensitive Diagnostic on Polymeric Insulating Surfaces
    • Graz
    • J. Hofman, R. Barsch, "Effects of Electrohydrodynamic Processes in Droplet Layers to Partial Discharges and Leakage Current and their use for a sensitive Diagnostic on Polymeric Insulating Surfaces", 9 th ISH, Graz, 1995, pp. 5605-1 to 5605-4.
    • (1995) 9 Th ISH , pp. 56051-56054
    • Hofman, J.1    Barsch, R.2
  • 41
    • 67649495111 scopus 로고    scopus 로고
    • Studies of the Long-Term Performance of Composite Insulators and of the Representativity of Aging Tests
    • Paris
    • G. Riquel, J. M. Fourmigue, D. de Decker, R. Joulie, R. Parraud, "Studies of the Long-Term Performance of Composite Insulators and of the Representativity of Aging Tests", Cigré Session, Paris, 1996, 33-304.
    • (1996) Cigré Session , pp. 33-304
    • Riquel, G.1    Fourmigue, J.M.2    De Decker, D.3    Joulie, R.4    Parraud, R.5
  • 42
    • 0026140347 scopus 로고
    • Surface Structural Changes of Naturally Aged Silicone and EPDM Composite Insulators
    • April
    • A. E. Vlastos, S. M. Gubanski, "Surface Structural Changes of Naturally Aged Silicone and EPDM Composite Insulators", IEEE Transactions on Power Delivery, Vol. 6, No. 2, April 1991, pp. 888-900.
    • (1991) IEEE Transactions on Power Delivery , vol.6 , Issue.2 , pp. 888-900
    • Vlastos, A.E.1    Gubanski, S.M.2
  • 43
    • 85047159270 scopus 로고
    • Aging of Polymer Insulator Surface under the Influence of Sand Storms
    • Graz
    • B. A. Arafa, M. Hamed, A. Sedeek, O. A. ElGendy, M. M. Awad, A. Nosseir, "Aging of Polymer Insulator Surface Under the Influence of Sand Storms", 9th ISH, Graz, 1995, pp. 3185-1 to 3185-4.
    • (1995) 9th ISH , pp. 31851-31854
    • Arafa, B.A.1    Hamed, M.2    Sedeek, A.3    Elgendy, O.A.4    Awad, M.M.5    Nosseir, A.6
  • 44
    • 33749958568 scopus 로고    scopus 로고
    • Thermally Accelerated Corona Aging of Silicone Rubber Surface Insulation
    • S. M. Reynders, P. Hendey, J. P. Reynders, "Thermally Accelerated Corona Aging of Silicone Rubber Surface Insulation", ISH'97 Montréal, pp121-124.
    • ISH'97 Montréal , pp. 121-124
    • Reynders, S.M.1    Hendey, P.2    Reynders, J.P.3
  • 45
    • 33749893393 scopus 로고    scopus 로고
    • Effects of Artificial Environmental Aging on Polymer Insulator Flashover
    • G. Xu, N. E. Frost, P. B. McGrath, C. W. Burns, "Effects of Artificial Environmental Aging on Polymer Insulator Flashover", ISH'97 Montréal, pp. 181-184.
    • ISH'97 Montréal , pp. 181-184
    • Xu, G.1    Frost, N.E.2    McGrath, P.B.3    Burns, C.W.4
  • 46
    • 33749950745 scopus 로고
    • Effect of ultra-violet radiation and high temperature on polymer insulating materials
    • Dresden, paper 24-01
    • R. S. Gorur, R. S. Thallam, "Effect of ultra-violet radiation and high temperature on polymer insulating materials", 7th ISH, Dresden, 1991, paper 24-01.
    • (1991) 7th ISH
    • Gorur, R.S.1    Thallam, R.S.2
  • 47
    • 84889782410 scopus 로고    scopus 로고
    • Contact Angle Measurement on Clean and Polluted HV Polymer Insulators
    • H. Janssen, U. Steitzel, "Contact Angle Measurement on Clean and Polluted HV Polymer Insulators", ISH'97 Montréal, pp. 149-152.
    • ISH'97 Montréal , pp. 149-152
    • Janssen, H.1    Steitzel, U.2
  • 50
    • 0030312322 scopus 로고    scopus 로고
    • Leakage Current Performance of Naturally Aged Non-Ceramic Insulators under a Severe Marine Environment
    • Stellenbosch, September
    • W. L. Vosloo, J. P. Holtzhausen, A. H. A. Roediger, "Leakage Current Performance of Naturally Aged Non-Ceramic Insulators under a Severe Marine Environment", IEEE Africon'96, Stellenbosch, September 1997, pp. 439-495.
    • (1997) IEEE Africon'96 , pp. 439-495
    • Vosloo, W.L.1    Holtzhausen, J.P.2    Roediger, A.H.A.3
  • 52
    • 33749903410 scopus 로고    scopus 로고
    • On the Evaluation of Influences on the Hydrophobicity of Silicone Rubber Surfaces
    • R. Barsch, J. Lambrecht, H-J. Winter, "On the Evaluation of Influences on the Hydrophobicity of Silicone Rubber Surfaces", ISH'97 Montréal, pp. 13-16.
    • ISH'97 Montréal , pp. 13-16
    • Barsch, R.1    Lambrecht, J.2    Winter, H.-J.3
  • 53
    • 0007934664 scopus 로고
    • Hydrophobicity of composite insulators: Measurement and influence on flashover performance
    • June
    • R. Hartings, "Hydrophobicity of composite insulators: measurement and influence on flashover performance", Stockholm International Symposium on Electric Power Engineering, June 1995, pp. 18-22.
    • (1995) Stockholm International Symposium on Electric Power Engineering , pp. 18-22
    • Hartings, R.1
  • 55
    • 33749974081 scopus 로고    scopus 로고
    • Effect of Dessert Environment on the Electrical Performance of Silicone Rubber Insulators
    • M. S. Rizk, A. Nosseir, B. A. Arafa, O. Elgendy, M. Awad, "Effect of Dessert Environment on the Electrical Performance of Silicone Rubber Insulators", ISH'97 Montréal, pp. 133-136.
    • ISH'97 Montréal , pp. 133-136
    • Rizk, M.S.1    Nosseir, A.2    Arafa, B.A.3    Elgendy, O.4    Awad, M.5
  • 56
    • 0028754486 scopus 로고
    • Surface Recovery of Silicone Rubber Used for HV Outdoor Insulation
    • December
    • J. W. Chang, R. S. Gorur, "Surface Recovery of Silicone Rubber Used for HV Outdoor Insulation", IEEE Transactions on Dielectrics and Electrical Insulation, Vol. 1, No. 6, December 1994, pp. 1039-1045.
    • (1994) IEEE Transactions on Dielectrics and Electrical Insulation , vol.1 , Issue.6 , pp. 1039-1045
    • Chang, J.W.1    Gorur, R.S.2
  • 59
    • 0030314407 scopus 로고    scopus 로고
    • Pollution Severity Instrument for Relevance to HV Insulators: Hardware Development Employing Peltier Junctions
    • Stellenbosch, September
    • D. R. H. Orbin, D. A. Swift, "Pollution Severity Instrument for Relevance to HV Insulators: Hardware Development Employing Peltier Junctions", IEEE Africon'96, Stellenbosch, September 1997, pp. 235-240.
    • (1997) IEEE Africon'96 , pp. 235-240
    • Orbin, D.R.H.1    Swift, D.A.2
  • 60
    • 33747706636 scopus 로고
    • The effects of Corona on the surface properties and Chemical Composition of Silicon Rubber Insulators
    • Graz
    • A. E. Dickson, J. P. Reynders, "The effects of Corona on the surface properties and Chemical Composition of Silicon Rubber Insulators", 9th ISH, Graz, 1995, pp. 3231-1 to 3231-4.
    • (1995) 9th ISH , pp. 32311-32314
    • Dickson, A.E.1    Reynders, J.P.2
  • 61
    • 33749902876 scopus 로고    scopus 로고
    • personal communication, Mattek CSIR, Meiring Naude Road, Vrummeria, Pretoria East, South Africa
    • W. Louw, personal communication, Mattek CSIR, Meiring Naude Road, Vrummeria, Pretoria East, South Africa.
    • Louw, W.1
  • 62
    • 33749931773 scopus 로고    scopus 로고
    • personal communication, Polymer research group - Mattek CSIR, Meiring Naude Road, Vrummeria, Pretoria East, South Africa
    • M. Jones, personal communication, Polymer research group - Mattek CSIR, Meiring Naude Road, Vrummeria, Pretoria East, South Africa.
    • Jones, M.1
  • 63
    • 33749932927 scopus 로고
    • Negative dc Discharge Triggered by Water Drops on Hydrophobic Surface of Insulation Materials
    • Graz
    • N. Sugawara, K. Sakaguchi, I. Nakajima, K. Kondo, "Negative dc Discharge Triggered by Water Drops on Hydrophobic Surface of Insulation Materials", 9th ISH, Graz, 1995, pp. 3216-1 to 3216-4.
    • (1995) 9th ISH , pp. 32161-32164
    • Sugawara, N.1    Sakaguchi, K.2    Nakajima, I.3    Kondo, K.4
  • 67
    • 33749925170 scopus 로고
    • Ac Flashover Mechanism for Water Droplets on an Hydrophobic Insulator
    • Yokohama, August paper 44.09
    • D. A. Swift, "ac Flashover Mechanism for Water Droplets on an Hydrophobic Insulator", 8th ISH, Yokohama, August 1993, paper 44.09
    • (1993) 8th ISH
    • Swift, D.A.1
  • 68
    • 0003204902 scopus 로고
    • Mathematical model of dry-band arcing on self supporting, all dielectric optical cables, strung on overhead power lines
    • May
    • C. N. Carter, M. A. Waldron, "Mathematical model of dry-band arcing on self supporting, all dielectric optical cables, strung on overhead power lines", IEE Proc C, Vol. 139, (3), May 1992, pp. 185-196.
    • (1992) IEE Proc C , vol.139 , Issue.3 , pp. 185-196
    • Carter, C.N.1    Waldron, M.A.2
  • 69
    • 33749910634 scopus 로고
    • Surface Dielectric Behavior of Polymeric Insulation
    • October
    • R. S. Gorur, T. Orbeck, "Surface Dielectric Behavior of Polymeric Insulation", IEEE Transactions on Electric Insulation, Vol. 26, No. 5, October 1991, pp. 1068-1069.
    • (1991) IEEE Transactions on Electric Insulation , vol.26 , Issue.5 , pp. 1068-1069
    • Gorur, R.S.1    Orbeck, T.2
  • 72
    • 33749912960 scopus 로고
    • The Effect of Changes in Volume and Air Density on the Corona Onset potential of water drops
    • Graz
    • A. J. Phillips, I. R. Jandrell, J. P. Reynders, "The Effect of Changes in Volume and Air Density on the Corona Onset potential of water drops", 9th ISH, Graz, 1995, pp. 2160-4 2166-4.
    • (1995) 9th ISH
    • Phillips, A.J.1    Jandrell, I.R.2    Reynders, J.P.3
  • 74
    • 33749974080 scopus 로고    scopus 로고
    • Formation of Dry bands on Polluted HV Insulators having Hydrophilic Surfaces; the Influence of Air Density for Natural Convective Cooling
    • D. A. Hoch, D. A. Swift, "Formation of Dry bands on Polluted HV Insulators having Hydrophilic Surfaces; The Influence of Air Density for Natural Convective Cooling", ISH'97 Montreal, pp. 337-340.
    • ISH'97 Montreal , pp. 337-340
    • Hoch, D.A.1    Swift, D.A.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.