Volumn 82, Issue 10, 1999, Pages 2833-2840

Microscopic mechanisms of oxidation in SiC-whisker-reinforced mullite/ZrO2 matrix composites

Author keywords

[No Author keywords available]

Indexed keywords

AMORPHOUS MATERIALS; CERAMIC MATRIX COMPOSITES; COMPOSITION EFFECTS; CRYSTAL WHISKERS; DISSOLUTION; HIGH TEMPERATURE EFFECTS; INTERDIFFUSION (SOLIDS); OXIDATION; QUARTZ; SILICON CARBIDE; ZIRCON; ZIRCONIA;

EID: 0033204122     PISSN: 00027820     EISSN: None     Source Type: Journal    
DOI: 10.1111/j.1151-2916.1999.tb02164.x     Document Type: Article
Times cited : (9)

References (31)
  • 1
    • 84985107381 scopus 로고
    • Temperature dependence of strengthening by whisker reinforcement: SiC-whisker-reinforced alumina in air
    • P. F. Becher and T. N. Tiegs, "Temperature Dependence of Strengthening by Whisker Reinforcement: SiC-Whisker-Reinforced Alumina in Air," Adv. Ceram. Mater., 3 [2] 148-53 (1988).
    • (1988) Adv. Ceram. Mater. , vol.3 , Issue.2 , pp. 148-153
    • Becher, P.F.1    Tiegs, T.N.2
  • 2
    • 0343355202 scopus 로고
    • Effect of high temperature oxidation on the microstructure and mechanical properties of whisker-reinforced ceramics
    • Edited by J. A. Pask and A. G. Evans. Plenum Press, New York
    • W. M. Kriven, G. van Tendeloo, T. N. Tiegs, and P. F. Becher, "Effect of High Temperature Oxidation on the Microstructure and Mechanical Properties of Whisker-Reinforced Ceramics"; pp. 939-47 in Ceramic Microstructures '86: Role of Interfaces. Edited by J. A. Pask and A. G. Evans. Plenum Press, New York, 1987.
    • (1987) Ceramic Microstructures '86: Role of Interfaces , pp. 939-947
    • Kriven, W.M.1    Van Tendeloo, G.2    Tiegs, T.N.3    Becher, P.F.4
  • 3
    • 0024683143 scopus 로고
    • Microstructure and mechanical properties of mullite-silicon carbide composites
    • M. I. Osendi, B. A. Bender, and D. Lewis III, "Microstructure and Mechanical Properties of Mullite-Silicon Carbide Composites," J. Am. Ceram. Soc., 72 [2] 1049-54 (1989).
    • (1989) J. Am. Ceram. Soc. , vol.72 , Issue.2 , pp. 1049-1054
    • Osendi, M.I.1    Bender, B.A.2    Lewis D. III3
  • 4
    • 0342919945 scopus 로고
    • Oxygen penetration into silicon carbide ceramics during oxidation
    • J. A. Costello and R. E. Tressler, "Oxygen Penetration into Silicon Carbide Ceramics during Oxidation," Ceram Int., 11 [2] 39-44 (1985).
    • (1985) Ceram Int. , vol.11 , Issue.2 , pp. 39-44
    • Costello, J.A.1    Tressler, R.E.2
  • 5
    • 0019574414 scopus 로고
    • Oxidation kinetics of hot-pressed and sintered α-SiC
    • J. A. Costello and R. E. Tressler, "Oxidation Kinetics of Hot-Pressed and Sintered α-SiC," J. Am. Ceram. Soc., 64 [6] 327-31 (1981).
    • (1981) J. Am. Ceram. Soc. , vol.64 , Issue.6 , pp. 327-331
    • Costello, J.A.1    Tressler, R.E.2
  • 6
    • 84987344259 scopus 로고
    • Oxidation kinetics of silicon carbide crystals and ceramics: I, in dry oxygen
    • J. A. Costello and R. E. Tressler, "Oxidation Kinetics of Silicon Carbide Crystals and Ceramics: I, In Dry Oxygen," J. Am. Ceram. Soc., 69 [9] 674-81 (1986).
    • (1986) J. Am. Ceram. Soc. , vol.69 , Issue.9 , pp. 674-681
    • Costello, J.A.1    Tressler, R.E.2
  • 7
    • 84979184865 scopus 로고
    • Oxidation behavior of silicon carbide
    • G. Ervin, "Oxidation Behavior of Silicon Carbide," J. Am. Ceram. Soc., 41 [9] 347-52 (1958).
    • (1958) J. Am. Ceram. Soc. , vol.41 , Issue.9 , pp. 347-352
    • Ervin, G.1
  • 8
    • 0016428180 scopus 로고
    • Oxidation of 6H-α-silicon carbide platelets
    • R. C. A. Harris, "Oxidation of 6H-α-Silicon Carbide Platelets," J. Am. Ceram. Soc., 58 [1-2] 7-9 (1975).
    • (1975) J. Am. Ceram. Soc. , vol.58 , Issue.1-2 , pp. 7-9
    • Harris, R.C.A.1
  • 9
    • 84985064075 scopus 로고
    • The microstructure of oxide scales on oxidized Si and SiC single crystals
    • A. H. Heuer, L. U. Ogbuji, and T. E. Mitchell, "The Microstructure of Oxide Scales on Oxidized Si and SiC Single Crystals," J. Am. Ceram. Soc., 63 [5-6] 354-55 (1980).
    • (1980) J. Am. Ceram. Soc. , vol.63 , Issue.5-6 , pp. 354-355
    • Heuer, A.H.1    Ogbuji, L.U.2    Mitchell, T.E.3
  • 10
    • 0016179542 scopus 로고
    • The high-temperature oxidation of hot-pressed silicon carbide
    • Edited by A. R. Cooper and A. H. Heuer. Plenum Press, New York
    • J. W. Hinze, W. C. Tripp, and H. C. Graham, "The High-Temperature Oxidation of Hot-Pressed Silicon Carbide"; pp. 409-19 in Materials Science Research, Vol. 9, Mass Transport Phenomena in Ceramics. Edited by A. R. Cooper and A. H. Heuer. Plenum Press, New York, 1975.
    • (1975) Materials Science Research, Vol. 9, Mass Transport Phenomena in Ceramics , vol.9 , pp. 409-419
    • Hinze, J.W.1    Tripp, W.C.2    Graham, H.C.3
  • 12
    • 84978579511 scopus 로고
    • Effects of oxygen partial pressure on the oxidation of silicon carbide
    • P. J. Jorgensen, M. E. Wadsworth, and I. B. Cutler, "Effects of Oxygen Partial Pressure on the Oxidation of Silicon Carbide," J. Am. Ceram. Soc., 43 [4] 209-12 (1960).
    • (1960) J. Am. Ceram. Soc. , vol.43 , Issue.4 , pp. 209-212
    • Jorgensen, P.J.1    Wadsworth, M.E.2    Cutler, I.B.3
  • 13
    • 0026097278 scopus 로고
    • Some new perspectives on oxidation of silicon carbide and silicon nitride
    • K. L. Luthra, "Some New Perspectives on Oxidation of Silicon Carbide and Silicon Nitride," J. Am. Ceram. Soc., 74 [5] 1095-103 (1991).
    • (1991) J. Am. Ceram. Soc. , vol.74 , Issue.5 , pp. 1095-1103
    • Luthra, K.L.1
  • 14
    • 0016557063 scopus 로고
    • Effect of alumina content on the oxidation of hot-pressed silicon carbide
    • S.C. Singhal and F. F. Lange, "Effect of Alumina Content on the Oxidation of Hot-Pressed Silicon Carbide," J. Am. Ceram. Soc., 58 [9-10] 433-35 (1975).
    • (1975) J. Am. Ceram. Soc. , vol.58 , Issue.9-10 , pp. 433-435
    • Singhal, S.C.1    Lange, F.F.2
  • 15
    • 0016971766 scopus 로고
    • Oxidation kinetics of hot-pressed silicon carbide
    • S. C. Singhal, "Oxidation Kinetics of Hot-Pressed Silicon Carbide," J. Mater. Sci., 11 [7] 1246-53 (1976).
    • (1976) J. Mater. Sci. , vol.11 , Issue.7 , pp. 1246-1253
    • Singhal, S.C.1
  • 16
    • 0025434787 scopus 로고
    • Oxidation of mullite-zirconia-alumina-silicon carbide composites
    • C. Baudín and J. S. Moya, "Oxidation of Mullite-Zirconia-Alumina-Silicon Carbide Composites," J. Am. Ceram. Soc., 73 [5] 1417-20 (1990).
    • (1990) J. Am. Ceram. Soc. , vol.73 , Issue.5 , pp. 1417-1420
    • Baudín, C.1    Moya, J.S.2
  • 18
    • 84985092665 scopus 로고
    • Kinetics of oxidation of carbide and silicide dispersed phases in oxide matrices
    • M. P. Borom, M. K. Brun, and L. E. Szala, "Kinetics of Oxidation of Carbide and Silicide Dispersed Phases in Oxide Matrices," Adv. Ceram. Mater., 3 [5] 491-97 (1988).
    • (1988) Adv. Ceram. Mater. , vol.3 , Issue.5 , pp. 491-497
    • Borom, M.P.1    Brun, M.K.2    Szala, L.E.3
  • 19
    • 0024141158 scopus 로고
    • Chemical interreactions in high-temperature ceramic composites
    • K. L. Luthra, "Chemical Interreactions in High-Temperature Ceramic Composites," J. Am. Ceram. Soc., 71 [12] 1114-20 (1988).
    • (1988) J. Am. Ceram. Soc. , vol.71 , Issue.12 , pp. 1114-1120
    • Luthra, K.L.1
  • 20
    • 0025414938 scopus 로고
    • Oxidation of silicon carbide-reinforced oxide-matrix composites at 1375°C to 1575°C
    • K. L. Luthra and H. D. Park, "Oxidation of Silicon Carbide-Reinforced Oxide-Matrix Composites at 1375°C to 1575°C," J. Am. Ceram. Soc., 73 [4] 1014-23 (1990).
    • (1990) J. Am. Ceram. Soc. , vol.73 , Issue.4 , pp. 1014-1023
    • Luthra, K.L.1    Park, H.D.2
  • 21
    • 0025467076 scopus 로고
    • Oxidation behavior of mullite-SiC composites
    • M. I. Osendi, "Oxidation Behavior of Mullite-SiC Composites," J. Mater. Sci., 25, 3561-65 (1990).
    • (1990) J. Mater. Sci. , vol.25 , pp. 3561-3565
    • Osendi, M.I.1
  • 23
    • 0028401190 scopus 로고
    • Oxidation behavior and effects of oxidation on the strength of SiC-whisker-reinforced alumina
    • H. E. Kim and A. J. Moorhead, "Oxidation Behavior and Effects of Oxidation on the Strength of SiC-Whisker-Reinforced Alumina," J. Mater. Sci., 29, 1656-61 (1994).
    • (1994) J. Mater. Sci. , vol.29 , pp. 1656-1661
    • Kim, H.E.1    Moorhead, A.J.2
  • 24
    • 0032653435 scopus 로고    scopus 로고
    • 2 based composites: Oxidation vs depth behavior
    • 2 Based Composites: Oxidation vs Depth Behavior," Acta Mater., 47 [6] 1977-86 (1999).
    • (1999) Acta Mater. , vol.47 , Issue.6 , pp. 1977-1986
    • Lin, C.C.1    Zangvil, A.2    Ruh, R.3
  • 25
    • 0032162957 scopus 로고    scopus 로고
    • Effect of zirconia content on the oxidation behavior of silicon carbide/zironia/mullite composites
    • C. Y. Tsai, C. C. Lin, A. Zangvil, and A. K. Li, "Effect of Zirconia Content on the Oxidation Behavior of Silicon Carbide/Zironia/Mullite Composites," J. Am. Ceram. Soc., 81 [9] 2413-20 (1998).
    • (1998) J. Am. Ceram. Soc. , vol.81 , Issue.9 , pp. 2413-2420
    • Tsai, C.Y.1    Lin, C.C.2    Zangvil, A.3    Li, A.K.4
  • 26
    • 0032289024 scopus 로고    scopus 로고
    • Dependence of oxidation modes on zirconia content in silicon carbide/zirconia/mullite composites
    • C. Y. Tsai and C. C. Lin, "Dependence of Oxidation Modes on Zirconia Content in Silicon Carbide/Zirconia/Mullite Composites," J. Am. Ceram. Soc., 81 [12] 3150-56 (1998).
    • (1998) J. Am. Ceram. Soc. , vol.81 , Issue.12 , pp. 3150-3156
    • Tsai, C.Y.1    Lin, C.C.2
  • 27
    • 84985167273 scopus 로고
    • Microstructural studies in alkoxide-derived mullite-zirconia-SiC whisker composites
    • A. Zangvil, C. C. Lin, and R. Ruh, "Microstructural Studies in Alkoxide-Derived Mullite-Zirconia-SiC Whisker Composites," J. Am. Ceram. Soc., 75 [5] 1254-63 (1992).
    • (1992) J. Am. Ceram. Soc. , vol.75 , Issue.5 , pp. 1254-1263
    • Zangvil, A.1    Lin, C.C.2    Ruh, R.3
  • 28
    • 84986398023 scopus 로고
    • Phase and microstructure evolution in alkoxide-derived mullite/MgO-partially-stabilized zirconia
    • C. C. Lin, A. Zangvil, and R. Ruh, "Phase and Microstructure Evolution in Alkoxide-Derived Mullite/MgO-Partially-Stabilized Zirconia," J. Am. Ceram. Soc., 78 [5] 1361-71 (1995).
    • (1995) J. Am. Ceram. Soc. , vol.78 , Issue.5 , pp. 1361-1371
    • Lin, C.C.1    Zangvil, A.2    Ruh, R.3
  • 29
    • 0017950514 scopus 로고
    • 3 fluxed hot-pressed silicon nitride
    • 3 Fluxed Hot-Pressed Silicon Nitride," J. Am. Ceram. Soc., 61 [3-4] 114-18 (1978).
    • (1978) J. Am. Ceram. Soc. , vol.61 , Issue.3-4 , pp. 114-118
    • Clarke, D.R.1    Thomas, G.2
  • 30
    • 0016027762 scopus 로고
    • The microstructures of silicon nitride ceramics during hot-pressing transformations
    • P. Drew and M. H. Lewis, "The Microstructures of Silicon Nitride Ceramics during Hot-Pressing Transformations," J. Mater. Sci., 9 [2] 261-69 (1974).
    • (1974) J. Mater. Sci. , vol.9 , Issue.2 , pp. 261-269
    • Drew, P.1    Lewis, M.H.2


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.