메뉴 건너뛰기




Volumn 22, Issue 9, 1999, Pages 753-760

Effects of post-drawing treatments on the fatigue strength of eutectoid steel wires

Author keywords

[No Author keywords available]

Indexed keywords

CRACK INITIATION; HARDNESS; RESIDUAL STRESSES; SHOT PEENING; STRAIN; WIRE;

EID: 0033187890     PISSN: 8756758X     EISSN: None     Source Type: Journal    
DOI: 10.1046/j.1460-2695.1999.t01-1-00212.x     Document Type: Article
Times cited : (18)

References (22)
  • 1
    • 0020208475 scopus 로고
    • Cyclic deformation of pearlitic eutectoid rail steel
    • H. Sunwoo, M. E. Fine, M. Meshii and D. H. Stone (1982) Cyclic deformation of pearlitic eutectoid rail steel. Met. Trans. A 13A, 2035-2046.
    • (1982) Met. Trans. A , vol.13 A , pp. 2035-2046
    • Sunwoo, H.1    Fine, M.E.2    Meshii, M.3    Stone, D.H.4
  • 2
    • 0023961017 scopus 로고
    • Influence of deformation substructure on flow and fracture of fully pearlitic steel
    • M. Dollar, I. M. Bernstein and A. W. Thompson (1988) Influence of deformation substructure on flow and fracture of fully pearlitic steel. Acta Metall. 36, 311-320.
    • (1988) Acta Metall. , vol.36 , pp. 311-320
    • Dollar, M.1    Bernstein, I.M.2    Thompson, A.W.3
  • 3
    • 0029306035 scopus 로고
    • Fatigue properties of very thin steel wire under fluctuating tension
    • in Japanese
    • Y. Kuroshima, S. Harada, K. Ogawa and M. Isaji (1995) Fatigue properties of very thin steel wire under fluctuating tension. J. Soc. Mat. Sci., Japan 44, 551-556 (in Japanese).
    • (1995) J. Soc. Mat. Sci., Japan , vol.44 , pp. 551-556
    • Kuroshima, Y.1    Harada, S.2    Ogawa, K.3    Isaji, M.4
  • 5
    • 0022059595 scopus 로고
    • Influence of microstructure on fatigue crack initiation in fully pearliric steels
    • G. T. Gray III, A. W. Thompson and J. C. Williams (1985) Influence of microstructure on fatigue crack initiation in fully pearliric steels. Met. Trans. A 16A, 753-760.
    • (1985) Met. Trans. A , vol.16 A , pp. 753-760
    • Gray G.T. III1    Thompson, A.W.2    Williams, J.C.3
  • 6
    • 0022900533 scopus 로고
    • Microstructural effects on short cracks in eutectoid steels
    • Proc International Workshop on Small Fatigue Cracks. (Edited by R. O. Richie and J. Lankford). The Metallurgical Society of AIME, Warrendale, Pa
    • M. A. Deaubler and A. W. Thompson (1986) Microstructural effects on short cracks in eutectoid steels. In: Small Fatigue Cracks. Proc International Workshop on Small Fatigue Cracks. (Edited by R. O. Richie and J. Lankford). The Metallurgical Society of AIME, Warrendale, Pa, pp. 157-164.
    • (1986) Small Fatigue Cracks , pp. 157-164
    • Deaubler, M.A.1    Thompson, A.W.2
  • 7
    • 0025414033 scopus 로고
    • Influence of microstructure on fatigue behavior and surface fatigue crack growth of fully pearlitic steels
    • M. A. Deaubler, A. W. Thompson and I. M. Bernstein (1990) Influence of microstructure on fatigue behavior and surface fatigue crack growth of fully pearlitic steels. Met. Trans. A 21A, 925-933.
    • (1990) Met. Trans. A , vol.21 A , pp. 925-933
    • Deaubler, M.A.1    Thompson, A.W.2    Bernstein, I.M.3
  • 8
    • 0020128080 scopus 로고
    • Fatigue initiation study of TMT eutectoid steel
    • P. W. Kao and J. G. Byrne (1982) Fatigue initiation study of TMT eutectoid steel. Met. Trans. A 13A, 855-864.
    • (1982) Met. Trans. A , vol.13 A , pp. 855-864
    • Kao, P.W.1    Byrne, J.G.2
  • 9
    • 0024775840 scopus 로고
    • Fatigue limit and fatigue life prediction in high strength cold drawn eutectoid steel wires
    • J. L. Lorca and V. Sanchez-Galvez (1989) Fatigue limit and fatigue life prediction in high strength cold drawn eutectoid steel wires. Fatigue Fract. Engng Mater. Struct. 12, 31-45.
    • (1989) Fatigue Fract. Engng Mater. Struct. , vol.12 , pp. 31-45
    • Lorca, J.L.1    Sanchez-Galvez, V.2
  • 11
    • 0343163161 scopus 로고
    • Investigation on the fatigue properties of steel wire; (part 1) effect of the reduction by drawing and the low-temperature annealing upon the fatigue strength of high carbon steel wire
    • in Japanese
    • T. Ueda and K. Asakura (1957) Investigation on the fatigue properties of steel wire; (part 1) effect of the reduction by drawing and the low-temperature annealing upon the fatigue strength of high carbon steel wire. Mater. Testing 6, 386-391 (in Japanese).
    • (1957) Mater. Testing , vol.6 , pp. 386-391
    • Ueda, T.1    Asakura, K.2
  • 12
    • 0022865988 scopus 로고
    • Barriers to short fatigue crack propagation at low stress amplitude in a banded ferrite-pearlite structure
    • Proc. International Workshop on Small Fatigue Cracks. (Edited by R. O. Richie and J. Lankford). The Metallurgical Society of AIMIE, Warrendale, Pa
    • K. J. Miller, H. J. Mohamed, M. W. Brown and E. R. De Los Rios (1986) Barriers to short fatigue crack propagation at low stress amplitude in a banded ferrite-pearlite structure. In: Small Fatigue Cracks. Proc. International Workshop on Small Fatigue Cracks. (Edited by R. O. Richie and J. Lankford). The Metallurgical Society of AIMIE, Warrendale, Pa, pp. 639-656.
    • (1986) Small Fatigue Cracks , pp. 639-656
    • Miller, K.J.1    Mohamed, H.J.2    Brown, M.W.3    De Los Rios, E.R.4
  • 13
    • 0017503363 scopus 로고
    • Deformation of pearlite
    • G. Langford (1977) Deformation of pearlite. Met. Trans. A 8A, 861-875.
    • (1977) Met. Trans. A , vol.8 A , pp. 861-875
    • Langford, G.1
  • 14
    • 0342728528 scopus 로고
    • Some aspect of the fatigue properties of patented steel wires. II - Note on the effect of lowtemperature heat treatment
    • E. T. Gill and R. Goodacre (1935) Some aspect of the fatigue properties of patented steel wires. II - Note on the effect of lowtemperature heat treatment. J. Iron Steel hist. 130 (II), 143-165.
    • (1935) J. Iron Steel Hist. , vol.130 , Issue.2 , pp. 143-165
    • Gill, E.T.1    Goodacre, R.2
  • 15
    • 0342293508 scopus 로고
    • Investigation on the fatigue properties of steel wire; (part 2) on the effect of the total reduction by drawing and the low temperature annealing upon the longitudinal residual stress of cold drawn steel wire
    • in Japanese
    • T. Ueda, K. Asakura and K. Kurane (1960) Investigation on the fatigue properties of steel wire; (part 2) on the effect of the total reduction by drawing and the low temperature annealing upon the longitudinal residual stress of cold drawn steel wire. Mater: Testing 9, 31-39 (in Japanese).
    • (1960) Mater: Testing , vol.9 , pp. 31-39
    • Ueda, T.1    Asakura, K.2    Kurane, K.3
  • 16
    • 0030189835 scopus 로고    scopus 로고
    • Influence of shot peening on short crack behavior in medium carbon steel
    • D. N. Kocanda, S. Kocanda and K. J. Miller (1996) Influence of shot peening on short crack behavior in medium carbon steel. Fatigue Fract. Engng Mater. Struct. 19, 911-917.
    • (1996) Fatigue Fract. Engng Mater. Struct. , vol.19 , pp. 911-917
    • Kocanda, D.N.1    Kocanda, S.2    Miller, K.J.3
  • 17
    • 0029255928 scopus 로고
    • Effect of shot peening on residual stress and fatigue life of a spring steel
    • G. H. Farrahi, J. L. Lebrun and D. Couratin (1995) Effect of shot peening on residual stress and fatigue life of a spring steel. Fatigue Fract. Engng Mater. Struct. 18, 211-220.
    • (1995) Fatigue Fract. Engng Mater. Struct. , vol.18 , pp. 211-220
    • Farrahi, G.H.1    Lebrun, J.L.2    Couratin, D.3
  • 18
    • 0342293505 scopus 로고
    • Residual stresses in drawn steel
    • in Japanese
    • T. Nishioka (1956) Residual stresses in drawn steel. J. Japan Inst. Metals 20, 424-427 (in Japanese).
    • (1956) J. Japan Inst. Metals , vol.20 , pp. 424-427
    • Nishioka, T.1
  • 20
    • 0041487182 scopus 로고
    • Factors responsible for the sharp fatigue limit in iron and steel
    • A. Yoshikawa and T. Sugeno (1965) Factors responsible for the sharp fatigue limit in iron and steel. Trans. Met. Soc. AIME 233, 1314-1317.
    • (1965) Trans. Met. Soc. AIME , vol.233 , pp. 1314-1317
    • Yoshikawa, A.1    Sugeno, T.2
  • 21
    • 85009578756 scopus 로고
    • Effects of nonmetallic inclusions, small defects and small cracks on fatigue strength of metals
    • in Japanese
    • Y. Murakami and M. Shimizu (1988) Effects of nonmetallic inclusions, small defects and small cracks on fatigue strength of metals. Trans. Jpn. Soc. Mech. Engng A 54, 413-425 (in Japanese).
    • (1988) Trans. Jpn. Soc. Mech. Engng A , vol.54 , pp. 413-425
    • Murakami, Y.1    Shimizu, M.2
  • 22
    • 0343598511 scopus 로고
    • Tips on designing with residual stresses
    • Sept.
    • G. M. Sinclair, J. D. Morrow and A. S. Ross (1959) Tips on designing with residual stresses. SAE J. Sept., 76-77.
    • (1959) SAE J. , pp. 76-77
    • Sinclair, G.M.1    Morrow, J.D.2    Ross, A.S.3


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.