Volumn 40, Issue 23, 1999, Pages 6465-6473

In vitro study of poly(lactic acid) pin degradation

Author keywords

Biodegradation; Pins; Poly(lactic acid)

Indexed keywords

BIOCOMPATIBILITY; BIODEGRADATION; CRYSTAL STRUCTURE; IMPLANTS (SURGICAL);

EID: 0032818105     PISSN: 00323861     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0032-3861(98)00846-5     Document Type: Article
Times cited : (141)

References (27)
  • 1
    • 0026576011 scopus 로고
    • Resorbable polymers for internal fixation
    • Gogolewski S. Resorbable polymers for internal fixation. Clin Mater. 10:1992;13-20.
    • (1992) Clin Mater , vol.10 , pp. 13-20
    • Gogolewski, S.1
  • 3
    • 0026059172 scopus 로고
    • Physico-mechanical properties of degradable polymers used in medical applications: A comparative study
    • Engelberg I., Kohn J. Physico-mechanical properties of degradable polymers used in medical applications: a comparative study. Biomaterials. 12:1991;292-304.
    • (1991) Biomaterials , vol.12 , pp. 292-304
    • Engelberg, I.1    Kohn, J.2
  • 4
    • 0026587974 scopus 로고
    • Resorbable polyesters: Composition properties applications
    • Amecke B., Bendix D., Entenmann G. Resorbable polyesters: composition properties applications. Clin Mater. 10:1992;47-50.
    • (1992) Clin Mater , vol.10 , pp. 47-50
    • Amecke, B.1    Bendix, D.2    Entenmann, G.3
  • 5
    • 0027572376 scopus 로고
    • Poly(L-Lactide): A long-term degradation study in vivo. Part III. Analytical characterization
    • Pistner H., Bendix D.R., Muhling J., Reuther J.F. Poly(L-Lactide): a long-term degradation study in vivo. Part III. Analytical characterization. Biomaterials. 14:1993;291-298.
    • (1993) Biomaterials , vol.14 , pp. 291-298
    • Pistner, H.1    Bendix, D.R.2    Muhling, J.3    Reuther, J.F.4
  • 6
    • 0024321951 scopus 로고
    • Transphyseal fracture fixation using biodegradable pins in children
    • Bostman ., Makela E.A., Tormala P., Rokkanen P. Transphyseal fracture fixation using biodegradable pins in children. J Bone Joint Surg. 17-B:1989;706-707.
    • (1989) J Bone Joint Surg , vol.17 , pp. 706-707
    • Bostman1    Makela, E.A.2    Tormala, P.3    Rokkanen, P.4
  • 7
    • 0023133637 scopus 로고
    • Resorbable materials of poly(L-lactide). VI. Plates and screws for internal fracture fixation
    • Leeslag J.W., Pennings A.J., Bos R.R.M., Rozema F.R., Boering G. Resorbable materials of poly(L-lactide). VI. Plates and screws for internal fracture fixation. Biomaterials. 8:1987;70-73.
    • (1987) Biomaterials , vol.8 , pp. 70-73
    • Leeslag, J.W.1    Pennings, A.J.2    Bos, R.R.M.3    Rozema, F.R.4    Boering, G.5
  • 10
    • 0027577987 scopus 로고
    • Biocompatibility and resorbability of a polylactic acid membrane for periodontal guided tissue regeneration
    • Robert P., Mauduit J., Frank R.M., Vert M. Biocompatibility and resorbability of a polylactic acid membrane for periodontal guided tissue regeneration. Biomaterials. 14:1993;353-358.
    • (1993) Biomaterials , vol.14 , pp. 353-358
    • Robert, P.1    Mauduit, J.2    Frank, R.M.3    Vert, M.4
  • 13
    • 0028335230 scopus 로고
    • Poly(L-lactide): A long-term degradation study in vivo. Part II: Physico-mechanical behaviour of implants
    • Pistner H., Stallforth H., Gutwald R., Muhling J., Reuther J., Michael C. Poly(L-lactide): a long-term degradation study in vivo. Part II: physico-mechanical behaviour of implants. Biomaterials. 15:1995;439-450.
    • (1995) Biomaterials , vol.15 , pp. 439-450
    • Pistner, H.1    Stallforth, H.2    Gutwald, R.3    Muhling, J.4    Reuther, J.5    Michael, C.6
  • 14
    • 0025784686 scopus 로고
    • Osteolytic changes accompanying degradation of absorbable fracture fixation implants
    • Bostman O. Osteolytic changes accompanying degradation of absorbable fracture fixation implants. J Bone Joint Surg. 73:1991;679-682.
    • (1991) J Bone Joint Surg , vol.73 , pp. 679-682
    • Bostman, O.1
  • 15
    • 0031081408 scopus 로고    scopus 로고
    • Long-term in vivo degradation and bone reaction to various polylactides. 1. One year results
    • Mainil-Varlet P., Rahn B., Gogolewiski S. Long-term in vivo degradation and bone reaction to various polylactides. 1. One year results. Biomaterials. 18:1997;257-266.
    • (1997) Biomaterials , vol.18 , pp. 257-266
    • Mainil-Varlet, P.1    Rahn, B.2    Gogolewiski, S.3
  • 16
    • 0024859916 scopus 로고
    • The injection molding of resorbable implants
    • Offegeld H., Michaeli W., Menges G. The injection molding of resorbable implants. Antec. 35:1989;1282-1286.
    • (1989) Antec , vol.35 , pp. 1282-1286
    • Offegeld, H.1    Michaeli, W.2    Menges, G.3
  • 18
    • 0027897736 scopus 로고
    • The effect of phagocytosis of poly(L-lactic acid) fragments on cellular morphology and viability
    • Lam K.H., Schakenraad J.M., Esselbrugge H., Feijen J., Nieuwenhuis P. The effect of phagocytosis of poly(L-lactic acid) fragments on cellular morphology and viability. J Biomed Mater Res. 27:1993;1569-1577.
    • (1993) J Biomed Mater Res , vol.27 , pp. 1569-1577
    • Lam, K.H.1    Schakenraad, J.M.2    Esselbrugge, H.3    Feijen, J.4    Nieuwenhuis, P.5
  • 19
    • 0029347560 scopus 로고
    • The influence of surface morphology and wettability on inflammatory response against poly(L-lactic acid): A semi-quantitative study with monoclonal antibodies
    • Lam K.H., Schakenraad J.M., Groen H., Esselbrugge H., Dijkstra P.J., Feijen J., Nieuwenhuis P. The influence of surface morphology and wettability on inflammatory response against poly(L-lactic acid): a semi-quantitative study with monoclonal antibodies. J Biomed Mater Res. 29:1995;929-942.
    • (1995) J Biomed Mater Res , vol.29 , pp. 929-942
    • Lam, K.H.1    Schakenraad, J.M.2    Groen, H.3    Esselbrugge, H.4    Dijkstra, P.J.5    Feijen, J.6    Nieuwenhuis, P.7
  • 21
    • 0011786536 scopus 로고
    • Investigation of the structure of solution grown crystals of lactide copolymers by means of chemical reactions
    • Fisher E.W., Sterzel H.J., Wegner G. Investigation of the structure of solution grown crystals of lactide copolymers by means of chemical reactions. Kolloid-Z Z Polymere. 251:1973;980-990.
    • (1973) Kolloid-Z Z Polymere , vol.251 , pp. 980-990
    • Fisher, E.W.1    Sterzel, H.J.2    Wegner, G.3
  • 22
    • 25144457882 scopus 로고
    • Structure-property relationships in the case of the degradation of massive aliphatic poly(α-hydroxy acids) in aqueous media, Part 2: Degradation of lactide-glicolide copolymers: PLa37.5Ga25 and PLA75Ga25
    • Li S.M., Garreau H., Vert M. Structure-property relationships in the case of the degradation of massive aliphatic poly(α-hydroxy acids) in aqueous media, Part 2: degradation of lactide-glicolide copolymers: PLa37.5Ga25 and PLA75Ga25. J Mater Sci: Mater in Med. 1:1990;131-139.
    • (1990) J Mater Sci: Mater in Med , vol.1 , pp. 131-139
    • Li, S.M.1    Garreau, H.2    Vert, M.3
  • 23
    • 0023237597 scopus 로고
    • Resorbable materials of poly(L-lactide) VIII. in vivo and in vitro degradation
    • Leenslag J.W., Pennings A.J., Bos R.R.M., Rozema F.R., Boering G. Resorbable materials of poly(L-lactide) VIII. in vivo and in vitro degradation. Biomaterials. 8:1987;311-314.
    • (1987) Biomaterials , vol.8 , pp. 311-314
    • Leenslag, J.W.1    Pennings, A.J.2    Bos, R.R.M.3    Rozema, F.R.4    Boering, G.5
  • 25
    • 0025510186 scopus 로고
    • Structure-property relationships in the case of the degradation of massive aliphatic poly((-hydroxy acids) in aqueous media, Part 3: Influence of the morphology of poly(L-lactic acid)
    • Li S.M., Garreau H., e Vert M. Structure-property relationships in the case of the degradation of massive aliphatic poly((-hydroxy acids) in aqueous media, Part 3: Influence of the morphology of poly(L-lactic acid). J Mater Sci: Mater in Med. 1:1990;198-206.
    • (1990) J Mater Sci: Mater in Med , vol.1 , pp. 198-206
    • Li, S.M.1    Garreau, H.2    E. Vert, M.3
  • 26
    • 0030561484 scopus 로고    scopus 로고
    • Long-Term soft tissue reaction to various polylactides and their in vivo degradation
    • Mainil-Varlet P., Gogolewski S., Nieuwenhuis P. Long-Term soft tissue reaction to various polylactides and their in vivo degradation. J Mater Sci Mater in Med. 7:1996;713-721.
    • (1996) J Mater Sci Mater in Med , vol.7 , pp. 713-721
    • Mainil-Varlet, P.1    Gogolewski, S.2    Nieuwenhuis, P.3
  • 27
    • 0026646773 scopus 로고
    • In vivo degradation of massive poly(α-hydroxy acids): Validation of in vitro findings
    • Therin M., Cristel P., Li S., Garreau H., Vert M. In vivo degradation of massive poly(α-hydroxy acids): validation of in vitro findings. Biomaterials. 13:1992;594.
    • (1992) Biomaterials , vol.13 , pp. 594
    • Therin, M.1    Cristel, P.2    Li, S.3    Garreau, H.4    Vert, M.5


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.