1
-
-
0027870652
-
Effect of solid lubricants on low speed sliding behavior of silicon nitride at temperatures to 800°C
-
Murray S.F., Calabrese S.J. Effect of solid lubricants on low speed sliding behavior of silicon nitride at temperatures to 800°C. Lubr. Eng. 49:1993;955-964.
-
(1993)
Lubr. Eng.
, vol.49
, pp. 955-964
-
-
Murray, S.F.1
Calabrese, S.J.2
-
2
-
-
0003142818
-
Decomposition kinetics of some solid lubricants determined by elevated temperature X-ray diffraction techniques
-
H.E. Sliney, Decomposition kinetics of some solid lubricants determined by elevated temperature X-ray diffraction techniques, Proc. of the US Air Force Aerospace Fluids Lubr. Conf., 1963, pp. 350-367.
-
(1963)
Proc. of the US Air Force Aerospace Fluids Lubr. Conf.
, pp. 350-367
-
-
Sliney, H.E.1
-
3
-
-
49949147297
-
Molybdenum disulfide as a lubricant: A review of the fundamental knowledge
-
Winer W.O. Molybdenum disulfide as a lubricant: a review of the fundamental knowledge. Wear. 10:1967;422-452.
-
(1967)
Wear
, vol.10
, pp. 422-452
-
-
Winer, W.O.1
-
5
-
-
0025014176
-
A review of the influence of environmental humidity and water on friction, lubrication and wear
-
Lancaster J.K. A review of the influence of environmental humidity and water on friction, lubrication and wear. Tribology International. 23:1990;371-389.
-
(1990)
Tribology International
, vol.23
, pp. 371-389
-
-
Lancaster, J.K.1
-
6
-
-
0002116466
-
The effect of humidity on the friction and life of unbonded molybdenum disulfide
-
Pritchard C., Midgley J.W. The effect of humidity on the friction and life of unbonded molybdenum disulfide. Wear. 13:1969;39-50.
-
(1969)
Wear
, vol.13
, pp. 39-50
-
-
Pritchard, C.1
Midgley, J.W.2
-
7
-
-
0028992231
-
Friction behavior of pulsed laser deposited tungsten disulfide films
-
Prasad S.V., Zabinski J.S., McDevitt N.T. Friction behavior of pulsed laser deposited tungsten disulfide films. Tribology Transactions. 38:1995;57-62.
-
(1995)
Tribology Transactions
, vol.38
, pp. 57-62
-
-
Prasad, S.V.1
Zabinski, J.S.2
McDevitt, N.T.3
-
8
-
-
0027663473
-
Tribology of tungsten disulfide: Characterization of wear-induced transfer films
-
Prasad S.V., Zabinski J.S. Tribology of tungsten disulfide: characterization of wear-induced transfer films. J. Mater. Sci. Lett. 12:1993;1413-1415.
-
(1993)
J. Mater. Sci. Lett.
, vol.12
, pp. 1413-1415
-
-
Prasad, S.V.1
Zabinski, J.S.2
-
9
-
-
0000510587
-
The influence of substrate hardness on the formation and endurance of molybdenum disulfide films
-
Lancaster J.K. The influence of substrate hardness on the formation and endurance of molybdenum disulfide films. Wear. 10:1967;103-107.
-
(1967)
Wear
, vol.10
, pp. 103-107
-
-
Lancaster, J.K.1
-
10
-
-
0020116354
-
Effect of substrate finish on the lubrication and failure mechanisms of molybdenum disulfide films
-
Fusaro R.L. Effect of substrate finish on the lubrication and failure mechanisms of molybdenum disulfide films. ASLE Trans. 25:1982;141-156.
-
(1982)
ASLE Trans.
, vol.25
, pp. 141-156
-
-
Fusaro, R.L.1
-
11
-
-
0031167099
-
Effect of discontinuous hard under-coating on the life of solid film lubricant under extreme contact pressure
-
Hiraoka N., Sasaki A. Effect of discontinuous hard under-coating on the life of solid film lubricant under extreme contact pressure. Tribology International. 30:1997;344-429.
-
(1997)
Tribology International
, vol.30
, pp. 344-429
-
-
Hiraoka, N.1
Sasaki, A.2
-
12
-
-
84875817474
-
Tribological properties of Al alloy particle composites
-
Prasad S.V., Rohatgi P.K. Tribological properties of Al alloy particle composites. J. Met. 39:1987;22-26.
-
(1987)
J. Met.
, vol.39
, pp. 22-26
-
-
Prasad, S.V.1
Rohatgi, P.K.2
-
13
-
-
0042336854
-
Pulsed laser deposition of tungsten disulfide on aluminum metal-matrix composites
-
Prasad S.V., Zabinski J.S., Dyhouse V.J. Pulsed laser deposition of tungsten disulfide on aluminum metal-matrix composites. J. Mater. Sci. Lett. 11:1992;1282-1284.
-
(1992)
J. Mater. Sci. Lett.
, vol.11
, pp. 1282-1284
-
-
Prasad, S.V.1
Zabinski, J.S.2
Dyhouse, V.J.3
-
14
-
-
0028499669
-
Synthesis and characterization of tungsten disulfide films grown by pulsed laser deposition
-
Zabinski J.S., Donley M.S., Prasad S.V., McDevitt N.T. Synthesis and characterization of tungsten disulfide films grown by pulsed laser deposition. J. Mater. Sci. 29:1994;4834-4839.
-
(1994)
J. Mater. Sci.
, vol.29
, pp. 4834-4839
-
-
Zabinski, J.S.1
Donley, M.S.2
Prasad, S.V.3
McDevitt, N.T.4
-
15
-
-
0007045008
-
Metallography, structures and phase diagrams
-
Metals Park, OH
-
Metallography, structures and phase diagrams, ASM Metals Hand Book, Vol. 8, Metals Park, OH, 1973, p. 124.
-
(1973)
ASM Metals Hand Book
, vol.8
, pp. 124
-
-
-
18
-
-
0029487177
-
Nanostructure of Au-20% Pd layers in multilayer solid lubricant films
-
Jayaram G., Marks L.D., Hilton M.R. Nanostructure of Au-20% Pd layers in multilayer solid lubricant films. Surface and Coatings Technology. 76/77:1995;393-399.
-
(1995)
Surface and Coatings Technology
, vol.7677
, pp. 393-399
-
-
Jayaram, G.1
Marks, L.D.2
Hilton, M.R.3
-
20
-
-
36449003463
-
Characterization of nanometer scale wear and oxidation of transition metal dichalcogenide lubricants by atomic force microscopy
-
Kim Y., Huang J.L., Leiber C.M. Characterization of nanometer scale wear and oxidation of transition metal dichalcogenide lubricants by atomic force microscopy. Appl. Phys. Lett. 59(26):1991;3404-3406.
-
(1991)
Appl. Phys. Lett.
, vol.59
, Issue.26
, pp. 3404-3406
-
-
Kim, Y.1
Huang, J.L.2
Leiber, C.M.3
-
21
-
-
0003749418
-
-
Chap. 8, Cambridge Univ. Press, Cambridge
-
B.R. Lawn, T.R. Wilshaw, Fracture of Brittle Solids, Chap. 8, Cambridge Univ. Press, Cambridge, 1975.
-
(1975)
Fracture of Brittle Solids
-
-
Lawn, B.R.1
Wilshaw, T.R.2
-
23
-
-
0002884895
-
Friction behavior of ceramic fiber-reinforced aluminum metal-matrix composites against a 440C steel counterface
-
Prasad S.V., Mecklenburg K.R. Friction behavior of ceramic fiber-reinforced aluminum metal-matrix composites against a 440C steel counterface. Wear. 162/164:1993;47-56.
-
(1993)
Wear
, vol.162-164
, pp. 47-56
-
-
Prasad, S.V.1
Mecklenburg, K.R.2
|