Volumn 37, Issue 2, 1999, Pages 101-112

Recovery as a Measure of Oriented Crystalline Structure in Poly(ether ester)s Based on Poly(ethylene oxide) and Poly(ethylene terephthalate) Used as Shape Memory Polymers

Author keywords

Crystalline structure; Orientation; Poly(ether ester); Poly(ethylene oxide); Poly(ethylene terephthalate); Shape memory; Shrinkage

Indexed keywords

AMORPHOUS MATERIALS; CRYSTAL ORIENTATION; DEFORMATION; DIFFERENTIAL SCANNING CALORIMETRY; ENTROPY; MICROSCOPIC EXAMINATION; MOLECULAR STRUCTURE; MORPHOLOGY; POLYETHYLENE OXIDES; POLYETHYLENE TEREPHTHALATES; SHAPE MEMORY EFFECT; X RAY CRYSTALLOGRAPHY;

EID: 0032762439     PISSN: 08876266     EISSN: None     Source Type: Journal    
DOI: 10.1002/(SICI)1099-0488(19990115)37:2<101::AID-POLB1>3.0.CO;2-X     Document Type: Article
Times cited : (87)

References (39)
  • 1
    • 36749053928 scopus 로고
    • CEER 1984, 16, 34.
    • (1984) CEER , vol.16 , pp. 34
  • 3
    • 85034126992 scopus 로고    scopus 로고
    • (Jpn.) Kokai Tokkyo Koho JP 04,309,583
    • Nakai, Y. (Jpn.) Kokai Tokkyo Koho JP 04,309,583.
    • Nakai, Y.1
  • 31
  • 34
    • 85034125641 scopus 로고    scopus 로고
    • Ph.D. Dissertation, University of Science and Technology of China
    • Wang, M., Ph.D. Dissertation, University of Science and Technology of China, 1997.
    • (1997)
    • Wang, M.1
  • 37
    • 24044455101 scopus 로고
    • Kim, Y. J.; Sung , Y. K.; Piao, A. Z. et al. J Appl Polym Sci 1994, 54, 1863; Clarson, S. J.; Dodgson, K.; Semlyer, J. A. Polymer 1985, 26, 930.
    • (1994) J Appl Polym Sci , vol.54 , pp. 1863
    • Kim, Y.J.1    Sung, Y.K.2    Piao, A.Z.3
  • 38
    • 0022072659 scopus 로고
    • Kim, Y. J.; Sung , Y. K.; Piao, A. Z. et al. J Appl Polym Sci 1994, 54, 1863; Clarson, S. J.; Dodgson, K.; Semlyer, J. A. Polymer 1985, 26, 930.
    • (1985) Polymer , vol.26 , pp. 930
    • Clarson, S.J.1    Dodgson, K.2    Semlyer, J.A.3
  • 39
    • 85034139894 scopus 로고    scopus 로고
    • Melting peaks for PET segments were not observed on DSC curve when PET content in the copolymer was not more than 30% in weight; the reason may be the low crystallizability and content of PET
    • Melting peaks for PET segments were not observed on DSC curve when PET content in the copolymer was not more than 30% in weight; the reason may be the low crystallizability and content of PET.


* 이 정보는 Elsevier사의 SCOPUS DB에서 KISTI가 분석하여 추출한 것입니다.