Effects of gasoline absorption on the tensile impact response of HDPE/Selar™ laminar microlayer composites
|
Author keywords
Barrier resin; Gasoline absorption; HDPE; Microlayer composites; Plastification; Selar ; Strain stress behavior; Tensile impact
|
Indexed keywords
ABSORPTION;
BLOW MOLDING;
DIFFUSION IN SOLIDS;
FRACTOGRAPHY;
GASOLINE;
HIGH DENSITY POLYETHYLENES;
MECHANICAL PERMEABILITY;
POLYAMIDES;
POLYMER BLENDS;
STRAIN;
STRESS ANALYSIS;
TENSILE PROPERTIES;
FICKIAN LAW OF DIFFUSION;
MICROLAYER COMPOSITES;
PLASTIFICATION;
SELAR BARRIER RESIN;
LAMINATED COMPOSITES;
|