Fabrication of high valence Sr(Fe0.65Co0.35)O3 film by a pulsed laser ablation technique

Author keywords

Film formation diagram; Laser ablation; Oxidation equilibrium; Perovskite oxide; Sr(Fe,Co)O3 film

Indexed keywords

COBALT COMPOUNDS; FILM GROWTH; IRON OXIDES; LASER ABLATION; PEROVSKITE; PHASE EQUILIBRIA; PULSED LASER APPLICATIONS; STRONTIUM COMPOUNDS;

EID: 0032482822     PISSN: 00406090     EISSN: None     Source Type: Journal    
DOI: 10.1016/S0040-6090(98)00600-2     Document Type: Article
Times cited : (6)